Dental resin composites containing silica-fused whiskers - effects of whisker-to-silica ratio on fracture toughness and indentation properties

被引:73
作者
Xu, HHK
Quinn, JB
Smith, DT
Antonucci, JM
Schumacher, GE
Eichmiller, FC
机构
[1] Natl Inst Stand & Technol, Hlth Fdn, Amer Dent Assoc, Paffenbarger Res Ctr, Gaithersburg, MD 20899 USA
[2] NIST, Div Ceram, Gaithersburg, MD 20899 USA
[3] NIST, Div Polymers, Gaithersburg, MD 20899 USA
关键词
dental resin composite; reinforcement mechanisms; whisker-to-silica ratio; fracture toughness; elastic modulus; brittleness;
D O I
10.1016/S0142-9612(01)00178-8
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Dental resin composites need to be strengthened in order to improve their performance in large stress-bearing applications Such as crowns and multiple-unit restorations. Recently, silica-fused ceramic whiskers were used to reinforce dental composites, and the whisker-to-silica ratio was found to be a key microstructural parameter that determined the composite strength. The aim of this study was to further investigate the effects of whisker-to-silica ratio on the fracture toughness. elastic modulus, hardness and brittleness of the composite. Silica particles and silicon carbide whiskers were mixed at whisker: silica mass ratios of 0:1, 1:5, 1:2, 1:1.2: 1.5:1, and 1:0. Each mixture was thermally fused. silanized and combined with a dental resin at a filler mass percentage of 60%. Fracture toughness was measured with a sin-ale-edge notched beam method. Elastic modulus and hardness were measured with a nano-indentation system. Whisker: silica ratio had significant effects on composite properties. The composite toughness (mean +/- SD; n = 9) at whisker: silica = 2:1 was (2.47 +/-0.28) MPa m(1/2) significantly higher than (1.02 +/-0.23) at whisker: silica = 0:1, (1.13 +/-0.19) of a prosthetic composite control, and (0.95 +/-0.11) of an inlay/onlay composite control (Tukey's at family confidence coefficient=0.95). Elastic modulus increased monotonically and hardness plateaued with increasing the whisker: silica ratio. Increasing the whisker: silica ratio also decreased the composite brittleness, which became about 1/3 of that of the inlay/onlay control. Electron microscopy revealed relatively flat fracture surfaces for the controls, but much rougher ones for the whisker composites. with fracture steps and whisker Pullout contributing to toughness. The whiskers appeared to be well-bonded with the matrix. probably due to the fused silica producing rough whisker surfaces. Reinforcement with silica-fused whiskers resulted in novel dental composites that possessed fracture toughness two times higher than, and brittleness less than half of current dental composites. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:735 / 742
页数:8
相关论文
共 48 条
[1]  
[Anonymous], 1996, T ACAD DENT MAT
[2]  
ASMUSSEN E, 1990, SCAND J DENT RES, V98, P564
[3]  
*ASTM, 1999, C142199 ASTM
[4]   A characterization of first-generation flowable composites [J].
Bayne, SC ;
Thompson, JY ;
Swift, EJ ;
Stamatiades, P ;
Wilkerson, M .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1998, 129 (05) :567-577
[5]  
BAYNE SC, 1996, ACAD DENT MAT T, V9, P238
[7]   INFLUENCE OF FILLER TYPE AND WATER EXPOSURE ON FLEXURAL STRENGTH OF EXPERIMENTAL COMPOSITE RESINS [J].
CALAIS, JG ;
SODERHOLM, KJM .
JOURNAL OF DENTAL RESEARCH, 1988, 67 (05) :836-840
[8]   Porcelain-fused-to-metal vs. nonmetal crowns [J].
Christensen, GJ .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1999, 130 (03) :409-411
[9]   MECHANICAL-PROPERTIES OF HEAT-TREATED COMPOSITE RESIN RESTORATIVE MATERIALS [J].
COVEY, DA ;
TAHANEY, SR ;
DAVENPORT, JM .
JOURNAL OF PROSTHETIC DENTISTRY, 1992, 68 (03) :458-461
[10]  
Donly KJ, 1999, QUINTESSENCE INT, V30, P163