Surface Properties and Corrosion Behavior of Co-Cr Alloy Fabricated with Selective Laser Melting Technique

被引:70
作者
Xin, Xian-zhen [1 ]
Chen, Jie [1 ]
Xiang, Nan [1 ]
Wei, Bin [1 ]
机构
[1] Shanghai Jiao Tong Univ, Peoples Hosp 9, Sch Med,Shanghai Key Lab Stomatol, Stomatol Special Consultat Clin,Dept Prosthodont, Shanghai 200011, Peoples R China
关键词
Cobalt-chromium alloy; SLM; Surface property; Corrosion; Microstructure; NI-CR; COCRMO; XPS;
D O I
10.1007/s12013-013-9593-9
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
We sought to study the corrosion behavior and surface properties of a commercial cobalt-chromium (Co-Cr) alloy which was fabricated with selective laser melting (SLM) technique. For this purpose, specimens were fabricated using different techniques, such as SLM system and casting methods. Surface hardness testing, microstructure observation, surface analysis using X-ray photoelectron spectroscopy (XPS) and electrochemical corrosion test were carried out to evaluate the corrosion properties and surface properties of the specimens. We found that microstructure of SLM specimens was more homogeneous than that of cast specimens. The mean surface hardness values of SLM and cast specimens were 458.3 and 384.8, respectively; SLM specimens showed higher values than cast ones in hardness. Both specimens exhibited no differences in their electrochemical corrosion properties in the artificial saliva through potentiodynamic curves and EIS, and no significant difference via XPS. Therefore, we concluded that within the scope of this study, SLM-fabricated restorations revealed good surface properties, such as proper hardness, homogeneous microstructure, and also showed sufficient corrosion resistance which could meet the needs of dental clinics.
引用
收藏
页码:983 / 990
页数:8
相关论文
共 14 条
[1]   Electrochemical behaviour of recasting Ni-Cr and Co-Cr non-precious dental alloys [J].
Ameer, MA ;
Khamis, E ;
Al-Motlaq, M .
CORROSION SCIENCE, 2004, 46 (11) :2825-2836
[2]   Corrosion behaviour of commercially pure titanium shot blasted with different materials and sizes of shot particles for dental implant applications [J].
Aparicio, C ;
Gil, FJ ;
Fonseca, C ;
Barbosa, M ;
Planell, JA .
BIOMATERIALS, 2003, 24 (02) :263-273
[3]   Clinical performance of chairside CAD/CAM restorations [J].
Fasbinder, Dennis J. .
JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 2006, 137 :22S-31S
[4]   Characterization of the surface oxide film of a Co-Cr-Mo alloy after being located in quasi-biological environments using XPS [J].
Hanawa, T ;
Hiromoto, S ;
Asami, K .
APPLIED SURFACE SCIENCE, 2001, 183 (1-2) :68-75
[5]   Passive and transpassive behaviour of CoCrMo in simulated biological solutions [J].
Hodgson, AWE ;
Kurz, S ;
Virtanen, S ;
Fervel, V ;
Olsson, COA ;
Mischler, S .
ELECTROCHIMICA ACTA, 2004, 49 (13) :2167-2178
[6]   Electrochemical corrosion studies on Co-Cr-Mo implant alloy in biological solutions [J].
Hsu, RWW ;
Yang, CC ;
Huang, CA ;
Chen, YS .
MATERIALS CHEMISTRY AND PHYSICS, 2005, 93 (2-3) :531-538
[7]   Influence of electrochemical potential on the tribocorrosion behaviour of high carbon CoCrMo biomedical alloy in simulated body fluids by electrochemical impedance spectroscopy [J].
Igual Munoz, Anna ;
Casaban Julian, Leandre .
ELECTROCHIMICA ACTA, 2010, 55 (19) :5428-5439
[8]   Cobalt-based alloys for orthopaedic applications studied by electrochemical and XPS analysis [J].
Kocijan, A ;
Milosev, I ;
Pihlar, B .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 2004, 15 (06) :643-650
[9]   Corrosion behaviour and surface analysis of a Co-Cr and two Ni-Cr dental alloys before and after simulated porcelain firing [J].
Qiu, Jing ;
Yu, Wei-Qiang ;
Zhang, Fu-Qiang ;
Smales, Roger J. ;
Zhang, Yi-Lin ;
Lu, Chun-Hui .
EUROPEAN JOURNAL OF ORAL SCIENCES, 2011, 119 (01) :93-101
[10]   Effects of the porcelain-fused-to-metal firing process on the surface and corrosion of two Co-Cr dental alloys [J].
Qiu, Jing ;
Yu, Wei-qiang ;
Zhang, Fu-qiang .
JOURNAL OF MATERIALS SCIENCE, 2011, 46 (05) :1359-1368