Experimental assessment of the damage tolerance of z-pinned T-stiffened composite panels

被引:63
作者
Koh, T. M. [1 ]
Isa, M. D. [1 ,2 ]
Feih, S. [1 ]
Mouritz, A. P. [1 ]
机构
[1] RMIT Univ, Sch Aerosp Mech & Mfg Engn, Melbourne, Vic 3001, Australia
[2] Univ Kuala Lumpur, Malaysian Inst Aviat Technol, Dengkil 43800, Selangor, Malaysia
关键词
3-Dimensional reinforcement; Damage tolerance; Mechanical properties; Joints/joining; I DELAMINATION TOUGHNESS; FAILURE MECHANISMS; CYCLIC TENSION; LAP JOINTS; Z-PINS; REINFORCEMENT; THICKNESS; IMPACT; RODS;
D O I
10.1016/j.compositesb.2012.02.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stiffened composite panels used in aircraft, buildings and other light-weight structural applications are susceptible to unstable bond-line cracking that results in poor damage tolerant properties. This paper presents an experimental study into the improvement to the damage tolerance of T-shaped stiffened carbon fibre/epoxy panels when reinforced with thin z-pins. Stiffener pull-off tests revealed that the ultimate failure load and absorbed energy capacity of the skin-to-stiffener flange connection to the panels increased rapidly with the volume content of z-pins due to suppression of bond-line cracking. Improvements to the ultimate load and absorbed energy capacity of over 75% and 600%, respectively, was achieved when the skin-stiffener flange connection to the panels were reinforced at the relatively modest z-pin content of 4% by volume. Experimental analysis also showed that z-pins were highly effective at improving the damage tolerance of T-stiffened panels that contained a single bond-line delamination crack or multiple cracks along and near the bond-line caused by impact loading. The residual mechanical properties of damaged z-pinned panels were much higher (typically in the range of 100-500%) than of the unpinned panel, and based on this research z-pinning is shown to be an effective technique for increasing the damage tolerance of T-stiffened composite panels for load-bearing structural applications. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:620 / 627
页数:8
相关论文
共 31 条
[1]   Damage tolerance of bonded aircraft structures [J].
Alderliesten, R. C. .
INTERNATIONAL JOURNAL OF FATIGUE, 2009, 31 (06) :1024-1030
[2]  
[Anonymous], 2001, P ICCM 13 13 INT C C
[3]  
[Anonymous], P 15 TECHN C AM SOC
[4]   Effect of z-pins on fracture in composite cocured double cantilever beams [J].
Birman, V ;
Byrd, LW .
JOURNAL OF AEROSPACE ENGINEERING, 2005, 18 (01) :51-59
[5]   Effectiveness of z-pins in preventing delamination of co-cured composite joints on the example of a double cantilever test [J].
Byrd, LW ;
Birman, V .
COMPOSITES PART B-ENGINEERING, 2006, 37 (4-5) :365-378
[6]   Mechanisms of crack bridging by composite and metallic rods [J].
Cartié, DDR ;
Cox, BN ;
Fleck, NA .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2004, 35 (11) :1325-1336
[7]   3D reinforcement of stiffener-to-skin T-joints by Z-pinning and tufting [J].
Cartie, Denis D. R. ;
Dell'Anno, Giuseppe ;
Poulin, Emilie ;
Partridge, Ivana K. .
ENGINEERING FRACTURE MECHANICS, 2006, 73 (16) :2532-2540
[8]   Elevated temperature properties of pinned composite lap joints [J].
Chang, P. ;
Mouritz, A. P. ;
Cox, B. N. .
JOURNAL OF COMPOSITE MATERIALS, 2008, 42 (08) :741-769
[9]   Properties and failure mechanisms of z-pinned laminates in monotonic and cyclic tension [J].
Chang, P. ;
Mouritz, A. P. ;
Cox, B. N. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2006, 37 (10) :1501-1513
[10]   Properties and failure mechanisms of pinned composite lap joints in monotonic and cyclic tension [J].
Chang, P. ;
Mouritz, A. P. ;
Cox, B. N. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2006, 66 (13) :2163-2176