Influence of fiber-matrix bond strength on the performance of Nicalon/CAS-II composite

被引:6
作者
Kahraman, R [1 ]
Mandell, JF [1 ]
机构
[1] MONTANA STATE UNIV,DEPT CHEM ENGN,BOZEMAN,MT 59717
关键词
composites; ceramic matrix; glass ceramic; silicon carbide; bond strength; mechanical properties; interface; oxidation;
D O I
10.1177/002199839603000801
中图分类号
TB33 [复合材料];
学科分类号
摘要
The influence of the fiber-matrix interphase on the tensile behavior of unidirectional Nicalon fiber-reinforced GAS-II glass-ceramic matrix composite has been investigated. The failure strain decreases at high temperatures (1000 degrees C) to a value comparable to the matrix cracking strain. The embrittlement process appears to be the result of oxidation of the carbon interphase as the matrix crack encounters fibers (given sufficient strain and/or time), the interphase subsequently fuses with a high bond strength and the crack grows through the fibers. In the absence of matrix cracking (at high temperatures) the oxidation process does not penetrate more than a few fiber diameters in from exposed surfaces transverse to the fiber direction. The contribution of the degradation of the fibers to the embrittlement appears to be less important.
引用
收藏
页码:864 / 884
页数:21
相关论文
共 52 条