An investigation into the role of non-metallic inclusions in cleavage fracture of medium carbon pearlitic steels for high-speed railway wheel

被引:15
作者
Zhou, Shi-tong [1 ,2 ]
Li, Zhao-dong [2 ]
Jiang, Lu [3 ]
Wang, Xin [2 ]
Xu, Pian [1 ]
Ma, Yu-xi [1 ]
Yan, Yu-ping [1 ]
Yang, Cai-fu [2 ]
Yong, Qi-long [2 ]
机构
[1] Nanchang Hangkong Univ, Natl Def Key Disciplines Lab Light Alloy Proc Sci, Nanchang 330063, Jiangxi, Peoples R China
[2] Cent Iron & Steel Res Inst, Dept Struct Steels, Beijing 100081, Peoples R China
[3] Deakin Univ, Inst Frontier Mat, Geelong, Vic 3216, Australia
基金
中国国家自然科学基金;
关键词
High-speed railway wheel steel; Pearlite; Cleavage fracture; Oxide and sulfide; Toughness improvement; HEAT-AFFECTED ZONE; C-MN STEEL; FRACTOGRAPHIC OBSERVATIONS; MICROALLOYED STEEL; BRITTLE-FRACTURE; IMPACT TOUGHNESS; TIN INCLUSIONS; INITIATION; BEHAVIOR; MECHANISM;
D O I
10.1016/j.engfailanal.2021.105860
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Non-metallic inclusions are often considered to be detrimental to the toughness of steels. Here, we found that, in a cleavage-dominated fracture mode, the toughness, particularly the room temperature fracture toughness of pearlitic wheel steel can be improved by refining oxide inclusions or by increasing sulfur content. The roles of these inclusions in crack initiation and propagation were carefully investigated. Intriguingly, no spherical oxides or elongated sulfides were found to be the direct sources of cracks in the cleavage fracture within both Charpy V-notch and compact tension specimens. Cleavage cracks were found to be originated only from the steel matrix. Based on the theory of cleavage fracture and direct microscopic observations, the mechanisms were proposed for understanding the inclusion-toughness relations: (i) the oxide inclusions could indirectly induce crack initiation by enhancing local stress concentration, therefore promoting cleavage fracture and being detrimental to the toughness; (ii) in addition to enveloping the oxides to reduce the local stress concentration, the sulfide inclusions could also break the continuous propagation of cleavage cracks in the longitudinal direction by sulfide cracking or debonding, which released the stress concentration at the crack tip and enhanced the plastic work of fracture, thereby being beneficial to the toughness improvement.
引用
收藏
页数:20
相关论文
共 42 条
[1]  
Alexander D, 1984, MICROSTRUCTURAL EFFE
[2]  
[Anonymous], 2015, ASTM E2298-15
[3]  
[Anonymous], 2004, EN13262 EUR COMM STA
[4]  
ASTM, 2012, E399 12E3 STANDARD T
[5]  
BAKER TJ, 1986, MATER SCI TECH SER, V2, P576, DOI 10.1179/026708386790329217
[6]   Cleavage initiation in Ti-V-N and V-N microalloyed ferritic-pearlitic forging steels [J].
Balart, MJ ;
Davis, CL ;
Strangwood, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 284 (1-2) :1-13
[7]   Observations of cleavage initiation at (Ti,V)(C,N) particles of heterogeneous composition in microalloyed steels [J].
Balart, MJ ;
Davis, CL ;
Strangwood, M .
SCRIPTA MATERIALIA, 2004, 50 (03) :371-375
[8]   INFLUENCE OF SULFIDE INCLUSION ON DUCTILITY AND FRACTURE-BEHAVIOR OF RESULFURIZED HY-80 STEEL [J].
BISWAS, DK ;
VENKATRAMAN, M ;
NARENDRANATH, CS ;
CHATTERJEE, UK .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1992, 23 (05) :1479-1492
[9]  
BROOKSBANK D, 1969, J IRON STEEL I, V207, P474
[10]  
BROOKSBANK D, 1970, J IRON STEEL I, V208, P582