Soft machining-induced surface and edge chipping damage in pre-crystalized lithium silicate glass ceramics

被引:7
作者
Song, Xiao-Fei [1 ]
Ma, Hua-Run [1 ]
He, Yuan-Ping [1 ]
Yin, Ling [2 ]
机构
[1] Tianjin Univ, Sch Mech Engn, Key Lab Adv Ceram & Machining Technol, Minist Educ, Tianjin 300354, Peoples R China
[2] Univ Adelaide, Sch Mech Engn, North Terrace, Adelaide, SA 5005, Australia
基金
中国国家自然科学基金;
关键词
Lithium silicate ceramics; Mechanical property; Pre-crystallization; Soft machining; Surface and edge chipping damage; FLEXURAL STRENGTH; FRACTURE; ROUGHNESS; BRITTLENESS; RESIN; WEAR;
D O I
10.1016/j.jmbbm.2022.105224
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Soft machining is a key procedure in fabrication of high-strength lithium-based silicate glass ceramic (LS) restorations. This paper reports on the diamond machining-induced surface and edge chipping damage in two pre crystalized LS materials: pre-crystallized lithium metasilicate/orthophosphate glass ceramic (Pre-LS, IPS e.max CAD) and pre-crystallized zirconia-containing lithium metasilicate glass ceramic (Pre-ZLS, Vita Suprinity). Indentation techniques were used to measure the material mechanical properties. Soft machining was conducted using a robotic controlled apparatus mimicking dental CAD/CAM machining processes at different removal rates and enabling in-process force measurement. Machined surface roughness was assessed using 3D confocal optical profilometry in terms of the average and maximum surface heights. Scanning electron microscopy was used to assess diamond tool and machined surface and edge morphology. Soft machining of both materials was dominated by brittle fracture mixed with localized ductile flow. However, the higher brittleness index of Pre-ZLS than Pre-LS yielded higher degrees of machining-induced conchoidal fractures in Pre-ZLS in comparison with irregular fractures in Pre-LS. Thus, much larger surface roughness and deeper edge chipping damage were produced in Pre-ZLS than Pre-LS. Machining forces for Pre-ZLS were significantly smaller than Pre-LS, due to the lower machinability index associated with a complex relation of the mechanical properties as well as less debris adhesion for Pre-ZLS than Pre-LS. Further, increased material removal rates resulted in significantly increased machining forces, maximum surface roughness and fracture, and edge chipping damage in both Pre-ZLS and Pre LS materials. Therefore, optimization of soft machining processes needs to be practiced to achieve accepted surface and edge quality at balanced removal rates.
引用
收藏
页数:10
相关论文
共 42 条
  • [1] Influence of CAD/CAM milling, sintering and surface treatments on the fatigue behavior of lithium disilicate glass ceramic
    Alao, Abdur-Rasheed
    Stoll, Richard
    Zhang, Yu
    Yin, Ling
    [J]. JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2021, 113
  • [2] Fracture, roughness and phase transformation in CAD/CAM milling and subsequent surface treatments of lithium metasilicate/disilicate glass-ceramics
    Alao, Abdur-Rasheed
    Stoll, Richard
    Song, Xiao-Fei
    Abbott, John R.
    Zhang, Yu
    Abduo, Jaafar
    Yin, Ling
    [J]. JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2017, 74 : 251 - 260
  • [3] Advancements in CAD/CAM technology: Options for practical implementation
    Alghazzawi, Tariq F.
    [J]. JOURNAL OF PROSTHODONTIC RESEARCH, 2016, 60 (02) : 72 - 84
  • [4] Edge chipping resistance and flexural strength of polymer infiltrated ceramic network and resin nanoceramic restorative materials
    Argyrou, Renos
    Thompson, Geoffrey A.
    Cho, Seok-Hwan
    Berzins, David W.
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2016, 116 (03) : 397 - 403
  • [5] Belli Renan, 2016, Case Studies in Engineering Failure Analysis, V7, P71, DOI 10.1016/j.csefa.2016.10.001
  • [6] Fracture Rates and Lifetime Estimations of CAD/CAM All-ceramic Restorations
    Belli, R.
    Petschelt, A.
    Hofner, B.
    Hajto, J.
    Scherrer, S. S.
    Lohbauer, U.
    [J]. JOURNAL OF DENTAL RESEARCH, 2016, 95 (01) : 67 - 73
  • [7] Crack-healing during two-stage crystallization of biomedical lithium (di)silicate glass-ceramics
    Belli, Renan
    Lohbauer, Ulrich
    Goetz-Neunhoeffer, Friedlinde
    Hurle, Katrin
    [J]. DENTAL MATERIALS, 2019, 35 (08) : 1130 - 1145
  • [8] Fracture toughness testing of biomedical ceramic-based materials using beams, plates and discs
    Belli, Renan
    Wendler, Michael
    Petschelt, Anselm
    Lube, Tanja
    Lohbauer, Ulrich
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (16) : 5533 - 5544
  • [9] Chairside CAD/CAM materials. Part 1: Measurement of elastic constants and microstructural characterization
    Belli, Renan
    Wendler, Michael
    de Ligny, Dominique
    Cicconi, Maria Rita
    Petschelt, Anselm
    Peterlik, Herwig
    Lohbauer, Ulrich
    [J]. DENTAL MATERIALS, 2017, 33 (01) : 84 - 98
  • [10] Cracking of Porcelain Surfaces Arising from Abrasive Grinding with a Dental Air Turbine
    Chang, Chee W.
    Waddell, J. Neil
    Lyons, Karl M.
    Swain, Michael V.
    [J]. JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2011, 20 (08): : 613 - 620