Experimental study on mechanical properties and low-cycle fatigue behaviour of stainless steels subjected to salt spray and dry/wet cycle

被引:11
作者
Dang, Hengyao [1 ]
Liang, Anrui [2 ]
Feng, Ran [2 ]
Zhang, Jingzhou [3 ]
Yu, Xin [4 ]
Shao, Yongbo [5 ]
机构
[1] Luoyang Ship Mat Res Inst, Luoyang 471023, Peoples R China
[2] Harbin Inst Technol, Sch Civil & Environm Engn, Shenzhen 518055, Peoples R China
[3] Guangzhou Univ, Sch Civil Engn, Guangzhou 510006, Peoples R China
[4] Fuzhou Univ, Coll Civil Engn, Fuzhou 350108, Peoples R China
[5] Southwest Petr Univ, Sch Civil Engn & Geomatics, Chengdu 610500, Peoples R China
基金
中国国家自然科学基金;
关键词
Dry; wet cycle; Fatigue life prediction model; Low-cycle fatigue; Salt spray cycle; 304; SS; 430; REINFORCING BARS; CORROSION; TEMPERATURE; 304-STAINLESS-STEEL; DEGRADATION; ATMOSPHERE; TENSILE;
D O I
10.1016/j.ijfatigue.2022.107187
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper presents experimental studies on the mechanical properties and low-cycle fatigue behaviour of corroded austenitic stainless steel (304) and ferritic stainless steel (430). Tensile and low-cycle fatigue tests are conducted on 28 specimens. The corrosion process of the specimens is finished by using salt spray and dry/wet cycle tests. In the tensile tests, the key parameters of the constitutive model proposed by both Rasmussen and Gardner were obtained for austenitic stainless steel (304) and ferritic stainless steel (430). In the low-cycle fatigue test, the relationships of the stress amplitude and fatigue life of the specimens were obtained. The relationships of the mass loss, corrosion rate and cross-sectional area loss with the corrosion time are established. The influences of corrosion pits and fatigue cracks on the low-cycle fatigue behaviour of these two materials are studied through both macro and micro fracture morphology analysis. It is found that compared with the salt spray, the dry/wet cycle condition causes more degradation on the strength and fatigue life of the ferritic stainless steel (430). The stress concentration and notch effect of corrosion pits are the main reasons for the degradation in fatigue life of ferritic stainless steel (430). Moreover, current codes Eurocode 3 (EC3), Australian Standard (AS), BSI Standard (BSI) and DNV Standard (DNV) could not provide accurate fatigue life assessment for these two materials after salt spray and dry/wet cycle corrosions.
引用
收藏
页数:18
相关论文
共 50 条
  • [31] Low-cycle fatigue behavior of gradient structured austenitic stainless steels under high strain amplitude
    Ho, Hsin Shen
    Lv, Cheng
    Zhou, Wenlong
    Zhang, Erliang
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2022, 45 (06) : 1818 - 1829
  • [32] Physics-informed machine learning for low-cycle fatigue life prediction of 316 stainless steels
    Jiang, Lvfeng
    Hu, Yanan
    Liu, Yuxuan
    Zhang, Xu
    Kang, Guozheng
    Kan, Qianhua
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2024, 182
  • [33] Mechanical properties of HRB400E/316L stainless steel clad rebar under low-cycle fatigue
    Li, Wei
    Wang, Qingfan
    Qu, Hui
    Xiang, Yong
    Li, Zhaodong
    [J]. STRUCTURES, 2022, 38 : 292 - 305
  • [34] Effect of 475°C embrittlement on the low cycle fatigue behaviour of lean duplex stainless steels
    Strubbia, Renata
    Sennour, Mohamed
    Herenu, Silvina
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 41 (02) : 473 - 482
  • [35] Low-cycle fatigue behaviour of reinforcing bars including the effect of inelastic buckling
    Tripathi, Mayank
    Dhakal, Rajesh P.
    Dashti, Farhad
    Massone, Leonardo M.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2018, 190 : 1226 - 1235
  • [36] LOW-CYCLE FATIGUE PROPERTIES OF TIAL INTERMETALLIC COMPOUNDS
    YAMAGUCHI, K
    SHIMODAIRA, M
    NISHIJIMA, S
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1992, 78 (01): : 134 - 140
  • [37] Study of low-cycle fatigue of AL6XN austenitic stainless steel
    Meng, L. J.
    Sun, J.
    Xing, H.
    Yu, W. W.
    Xue, F.
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2011, 241 (08) : 2839 - 2842
  • [38] Influence of temperature on a low-cycle fatigue behavior of a ferritic stainless steel
    S. M. Humayun Kabir
    Tae-in Yeo
    [J]. Journal of Mechanical Science and Technology, 2014, 28 : 2595 - 2607
  • [39] Microstructural effects on the short crack behaviour of a stainless steel weld metal during low-cycle fatigue
    Zhao, YX
    Gao, Q
    Wang, JN
    [J]. FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1999, 22 (06) : 469 - 480
  • [40] Influence of temperature on the low-cycle fatigue properties of compacted graphite iron
    Qiu, Y.
    Pang, J. C.
    Li, S. X.
    Zhang, M. X.
    Zhang, Z. F.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2018, 117 : 450 - 460