Prediction of initiation and total life in fretting fatigue considering kinked cracks

被引:15
作者
Rangel, Danilo [1 ]
Erena, Diego [2 ]
Vazquez, Jesus [2 ]
Araujo, J. A. [1 ]
机构
[1] Univ Brasilia, Fac Technol, Dept Mech Engn, Campus Darcy Ribeiro, Brasilia, DF, Brazil
[2] Univ Seville, Dept Ingn Mecan & Fabricac, Escuela Tecn Super Ingenieros, Camino Descubrimientos S-N, Seville 41092, Spain
关键词
Fretting fatigue; Fatigue crack initiation; Crack path; SHEAR-STRESS AMPLITUDE; WOHLER CURVE; MECHANICS; GROWTH; MODEL; PATH;
D O I
10.1016/j.tafmec.2022.103345
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This work proposes a methodology to compute fretting fatigue crack initiation and total life by iterative models calibrated with fatigue stress-strain-life curves. One of the main novelty of such models is the assumption that the crack initiation length is determined by the size of the critical distance. To separate initiation and propagation lives, a numerical approach with finite elements is used. The methodology incorporates not only the multiaxial non-proportional characteristic of the stress field in fretting problems, but also the stress gradient effect. Crack initiation path is obtained by means of the SWT parameter, and to validate it, the analysed results are compared with tests considering a cylindrical-flat configuration (Aluminium 7075-T651 alloy). Most of the life initiation estimates, as well as the total life ones, are within a scatter band of 3.
引用
收藏
页数:10
相关论文
共 51 条
[1]  
[Anonymous], 2017, NIMS FAT DAT SHEET 1
[2]  
[Anonymous], 1991, MILITARY HDB MIL HDB
[3]  
[Anonymous], 2001, SPD10037
[4]   On the use of the Theory of Critical Distances and the Modified Wohler Curve Method to estimate fretting fatigue strength of cylindrical contacts [J].
Araujo, J. A. ;
Susmel, L. ;
Taylor, D. ;
Ferro, J. C. T. ;
Mamiya, E. N. .
INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (01) :95-107
[5]   Early cracking orientation under high stress gradients: The fretting case [J].
Araujo, J. A. ;
Almeida, G. M. J. ;
Ferreira, J. L. A. ;
da Silva, C. R. M. ;
Castro, F. C. .
INTERNATIONAL JOURNAL OF FATIGUE, 2017, 100 :611-618
[6]   A multiaxial stress-based critical distance methodology to estimate fretting fatigue life [J].
Araujo, J. A. ;
Susmel, L. ;
Pires, M. S. T. ;
Castro, F. C. .
TRIBOLOGY INTERNATIONAL, 2017, 108 :2-6
[7]   An alternative definition of the shear stress amplitude based on the Maximum Rectangular Hull method and application to the C-S (Carpinteri-Spagnoli) criterion [J].
Araujo, J. A. ;
Carpinteri, A. ;
Ronchei, C. ;
Spagnoli, A. ;
Vantadori, S. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2014, 37 (07) :764-771
[8]   On the characterization of the critical plane with a simple and fast alternative measure of the shear stress amplitude in multiaxial fatigue [J].
Araujo, J. A. ;
Dantas, A. P. ;
Castro, F. C. ;
Mamiya, E. N. ;
Ferreira, J. L. A. .
INTERNATIONAL JOURNAL OF FATIGUE, 2011, 33 (08) :1092-1100
[9]   The effect of rapidly varying contact stress fields on fretting fatigue [J].
Araújo, JA ;
Nowell, D .
INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (07) :763-775
[10]  
Belytschko T, 1999, INT J NUMER METH ENG, V45, P601, DOI 10.1002/(SICI)1097-0207(19990620)45:5<601::AID-NME598>3.0.CO