Effects of Manganese Content on Solidification Structures, Thermal Properties, and Phase Transformation Characteristics in Fe-Mn-Al-C Steels

被引:30
作者
Yang, Jian [1 ]
Wang, Yu-Nan [1 ]
Ruan, Xiao-Ming [1 ]
Wang, Rui-Zhi [1 ]
Zhu, Kai [1 ]
Fan, Zheng-Jie [1 ]
Wang, Ying-Chun [1 ]
Li, Cheng-Bin [1 ]
Jiang, Xiao-Fang [2 ]
机构
[1] Baosteel Grp Corp, Res Inst, Steelmaking Res Dept, Shanghai 201900, Peoples R China
[2] Baoshan Iron & Steel Co Ltd, Shanghai 201941, Peoples R China
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2015年 / 46卷 / 03期
关键词
HOT DUCTILITY; TWIP STEELS; TRANSVERSE CRACKING; INDUCED PLASTICITY; MECHANICAL-PROPERTIES; ALLOY-STEELS; LOW-CARBON; AUSTENITE; BEHAVIOR; ALUMINUM;
D O I
10.1007/s11663-015-0330-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To assist developments of the continuous-casting technology of Fe-Mn-Al-C steels, the solidification structures and the thermal properties of Fe-Mn-Al-C steel ingots with different manganese contents have been investigated and the phase transformation characteristics have been revealed by FactSage (CRCT-ThermFact Inc., Montr,al, Canada). The results show that the thermal conductivity of the 0Mn steel is the highest, whereas the thermal conductivity of the 8Mn steel is slightly higher than that of the 17Mn steel. Increasing the manganese content promotes a columnar solidification structure and coarse grains in steel. With the increase of manganese content, the mass fraction of austenite phase is increased. Finally, a single austenite phase is formed in the 17Mn steel. The mean thermal expansion coefficients of the steels are in the range from 1.3 x 10(-5) to 2.3 x 10(-5) K-1, and these values increase with the increase of manganese content. The ductility of the 17Mn steel and the 8Mn steel are higher than 40 pct in the temperature range from 873 K to 1473 K (600 A degrees C to 1200 A degrees C), and the cracking during the straightening operation should be avoided. However, the ductility of the 0Mn steel is lower than 40 pct at 973 K and 1123 K (700 A degrees C and 850 A degrees C), which indicates that the temperature of the straightening operation during the continuous-casting process should be above 1173 K (900 A degrees C). Manganese has the effect of enlarging the austenite phase region and reducing the delta-ferrite phase region and alpha-ferrite phase region. At the 2.1 mass pct aluminum level, the precipitate temperature of AlN is high. Thus, the formed AlN is too coarse to deteriorate the hot ductility of steel.
引用
收藏
页码:1365 / 1375
页数:11
相关论文
共 37 条
[1]   FactSage thermochemical software and databases [J].
Bale, C ;
Chartrand, P ;
Degterov, SA ;
Eriksson, G ;
Hack, K ;
Ben Mahfoud, R ;
Melançon, J ;
Pelton, AD ;
Petersen, S .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2002, 26 (02) :189-228
[2]   FactSage thermochemical software and databases - recent developments [J].
Bale, C. W. ;
Belisle, E. ;
Chartrand, P. ;
Decterov, S. A. ;
Eriksson, G. ;
Hack, K. ;
Jung, I. -H. ;
Kang, Y. -B. ;
Melancon, J. ;
Pelton, A. D. ;
Robelin, C. ;
Petersen, S. .
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2009, 33 (02) :295-311
[3]  
[常锷 Chang E], 2012, [钢铁, Iron and Steel], V47, P27
[4]   Austenite phase formation in rapidly solidified Fe-Cr-Mn-C steels [J].
Chen, SR ;
Davies, HA ;
Rainforth, WM .
ACTA MATERIALIA, 1999, 47 (18) :4555-4569
[5]   A modified damage model for advanced high strength steel sheets [J].
Chung, Kwansoo ;
Ma, Ning ;
Park, Taejoon ;
Kim, Dongun ;
Yoo, Donghoon ;
Kim, Chongmin .
INTERNATIONAL JOURNAL OF PLASTICITY, 2011, 27 (10) :1485-1511
[6]  
CROWTHER DN, 1986, MATER SCI TECH SER, V2, P671, DOI 10.1179/026708386790329019
[7]  
[董瀚 DONG Han], 2011, [钢铁, Iron and Steel], V46, P1
[8]   THERMAL DILATION OF COPPER [J].
EPPELSHEIMER, DS ;
PENMAN, RR .
PHYSICA, 1950, 16 (10) :792-794
[9]  
FU PX, 2009, ZHUZAO FOUNDRY, V58, P1037
[10]  
FURUKAWA T, 1994, MATER SCI TECH-LOND, V10, P964, DOI 10.1179/026708394790163537