Fracture behavior of multi-scale nano-SiO2 and polyvinyl alcohol fiber reinforced cementitious composites under the complex environments

被引:30
作者
Zhang, Peng [1 ,2 ]
Yuan, Peng [1 ,2 ]
Guan, Junfeng [3 ]
Guo, Jinjun [1 ,2 ]
机构
[1] Zhengzhou Univ, Yellow River Lab, Zhengzhou 450001, Peoples R China
[2] Zhengzhou Univ, Sch Water Conservancy Engn, Zhengzhou 450001, Peoples R China
[3] North China Univ Water Resources & Elect Power, Sch Civil Engn & Commun, Zhengzhou 450045, Peoples R China
基金
中国国家自然科学基金;
关键词
Fracture properties; Complex environments; Nano-SiO2; PVA fiber; Cementitious composites; QUASI-BRITTLE FRACTURE; DOUBLE-K CRITERION; MECHANICAL-PROPERTIES; CRACK-PROPAGATION; TOUGHNESS; CONCRETE; PARAMETERS; STRENGTH; ENERGY; DIFFUSION;
D O I
10.1016/j.tafmec.2022.103584
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper aims to investigate the fracture properties and microscopic mechanisms of multi-scale nano-SiO2 (NS) and polyvinyl alcohol (PVA) fiber-reinforced cementitious composites (MNFRCC) in complex environments. The complex environment was the coupling effect of wet-thermal and chloride salt environments (CEWTSE) simu-lated by an environmental simulation test chamber. And the parameters of temperature, relative humidity (RH), mass fraction of NaCl solution, and action time were determined as 50 degrees C, 100 %, 5 %, and 30 d, respectively. The Double-K Fracture model (DKFM), boundary effect fracture model (BEM), and work fracture method (WFM) were used to reveal that PVA fiber and NS improved the fracture properties of MNFRCC under the CEWTSE. And when the contents of PVA fiber and NS were 1.2 % and 0.5 %, respectively, the fracture parameters were significantly improved. Based on the comparative analysis of DKFM and BEM, the reasonable fracture parameters could be obtained by linking them through the crack propagation length. Moreover, the fictitious crack growth lengths and characteristic cracks increased with the increase of PVA fiber contents. On the microscopic level, PVA fiber and NS improved pores, microcracks and interfacial transition zone in the MNFRCC.
引用
收藏
页数:15
相关论文
共 65 条
  • [1] Effect of nano and micro SiO2 on brittleness and fracture parameters of self-compacting lightweight concrete
    Afzali-Naniz, Oveys
    Mazloom, Moosa
    Karamloo, Mohammad
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2021, 299 (299)
  • [2] [Anonymous], 1990, Materials and Structures, V23, P461, DOI DOI 10.1007/BF02472030
  • [3] [Anonymous], 1985, MAT STRUCT, V18, P285, DOI DOI 10.1007/BF02472918
  • [4] Prediction of chloride binding isotherms of cementitious materials by analytical model or numerical inverse analysis
    Baroghel-Bouny, V.
    Wang, X.
    Thiery, M.
    Saillio, M.
    Barberon, F.
    [J]. CEMENT AND CONCRETE RESEARCH, 2012, 42 (09) : 1207 - 1224
  • [5] Bazant Z.P., 1983, Mat. Constr, V16, P155, DOI [10.1007/BF02486267, DOI 10.1007/BF02486267]
  • [6] BAZANT ZP, 1987, ACI MATER J, V84, P463
  • [7] BAZANT ZP, 1984, J ENG MECH-ASCE, V110, P518
  • [8] Fracture behavior of cement mortar reinforced by hybrid composite fiber consisting of CaCO3 whiskers and PVA-steel hybrid fibers
    Cao, Mingli
    Xie, Chaopeng
    Guan, Junfeng
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2019, 120 : 172 - 187
  • [9] Mode I fracture toughness of fibre reinforced concrete
    Carpinteri, Andrea
    Fortese, Giovanni
    Ronchei, Camilla
    Scorza, Daniela
    Vantadori, Sabrina
    [J]. THEORETICAL AND APPLIED FRACTURE MECHANICS, 2017, 91 : 66 - 75
  • [10] The chemical composition and microstructure of hydration products in blended cements
    Escalante-Garcia, JI
    Sharp, JH
    [J]. CEMENT & CONCRETE COMPOSITES, 2004, 26 (08) : 967 - 976