Different aspects of hydrogen diffusion behavior in pipeline steel

被引:32
作者
Mohtadi-Bonab, M. A. [1 ]
Masoumi, Mohammad [2 ]
机构
[1] Univ Bonab, Dept Mech Engn, Bonab, Iran
[2] Univ Fed ABC, Ctr Engn Modelagem & Ciencias Sociais Aplicadas, BR-09210580 Santo Andre, SP, Brazil
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
基金
巴西圣保罗研究基金会;
关键词
Pipeline steel; Hydrogen diffusion; Hydrogen permeation; Inclusion; Reversible and irreversible traps; INDUCED BLISTER CRACKING; AUSTENITIC STAINLESS-STEEL; API 5L X60; MICROPRINT TECHNIQUE; ELECTROCHEMICAL PERMEATION; NONMETALLIC INCLUSIONS; TRAPPING EFFICIENCY; DELAYED FRACTURE; GRAIN-SIZE; EMBRITTLEMENT;
D O I
10.1016/j.jmrt.2023.04.026
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, hydrogen diffusion behavior in pipeline steel is thoroughly investigated. The effect of various microstructural factors affecting hydrogen diffusion are discussed using literature review. The results of this survey show that the hydrogen diffusion in pipeline steels depends strongly on the microstructure of steel, crystallographic texture, dislocation density, grain size, presence of different elements, precipitates and inclusions. Based on the results, the interfaces between the retained austenite and martensitic layer are considered as the possible hydrogen trap sites. Moreover, the apparent diffusivity decrease due to hydrogen trapping by dislocations is well documented without need for cyclic loading. The grain size and nature of grain boundaries plays an important role in the hydrogen diffusion and trapping. There is an optimum grain size in which the hydrogen diffusion reaches its maximum value. Various elements, inclusions and precipitates which are present in the microstructure of pipeline steel have a considerable role in hydrogen diffusion. Based on the hydrogen microprint technique results, the increase in the grain size decreases the hydrogen trapping by triple junctions and grain boundaries. & COPY; 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC
引用
收藏
页码:4762 / 4783
页数:22
相关论文
共 139 条
[1]   Sensitivity to hydrogen induced cracking, and corrosion performance of an API X65 pipeline steel in H2S containing environment: influence of heat treatment and its subsequent microstructural changes [J].
Anijdan, S. H. Mousavi ;
Arab, Gh ;
Sabzi, M. ;
Sadeghi, M. ;
Eivani, A. R. ;
Jafarian, H. R. .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 :1-16
[2]  
[Anonymous], 1969, FUNDAMENTAL ASPECTS
[3]  
[Anonymous], 2004, 170812004E ISO
[4]   Highly Sensitive Detection of Net Hydrogen Charged into Austenitic Stainless Steel with Secondary Ion Mass Spectrometry [J].
Awane, Tohru ;
Fukushima, Yoshihiro ;
Matsuo, Takashi ;
Matsuoka, Saburo ;
Murakami, Yukitaka ;
Miwa, Shiro .
ANALYTICAL CHEMISTRY, 2011, 83 (07) :2667-2676
[5]   Hydrogen embrittlement of X80 pipeline steel in H2S environment: Effect of hydrogen charging time, hydrogen-trapped state and hydrogen charging-releasing-recharging cycles [J].
Bai, Peng-peng ;
Zhou, Jie ;
Luo, Bing-wei ;
Zheng, Shu-qi ;
Wang, Peng-yan ;
Tian, Yu .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2020, 27 (01) :63-73
[6]   Comparison of dislocation density based approaches for prediction of defect structure evolution in aluminium and copper processed by ECAP [J].
Bratov, V. ;
Borodin, E. N. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 631 :10-17
[7]   Hydrogen Permeation in X65 Steel under Cyclic Loading [J].
Cabrini, Marina ;
Coppola, Luigi ;
Lorenzi, Sergio ;
Testa, Cristian ;
Carugo, Francesco ;
Bucella, Diego Pesenti ;
Pastore, Tommaso .
MATERIALS, 2020, 13 (10)
[8]   EFFECT OF RETAINED AUSTENITE ON THE HYDROGEN CONTENT AND EFFECTIVE DIFFUSIVITY OF MARTENSITIC STRUCTURE [J].
CHAN, SLI ;
LEE, HL ;
YANG, JR .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11) :2579-2586
[9]   Hydrogen trapping ability of steels with different microstructures [J].
Chan, SLI .
JOURNAL OF THE CHINESE INSTITUTE OF ENGINEERS, 1999, 22 (01) :43-53
[10]   Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel [J].
Chen, Y. -S. ;
Haley, D. ;
Gerstl, S. S. A. ;
London, A. J. ;
Sweeney, F. ;
Wepf, R. A. ;
Rainforth, W. M. ;
Bagot, P. A. J. ;
Moody, M. P. .
SCIENCE, 2017, 355 (6330) :1196-1199