Retained austenite grain size as a strength-plasticity relationship indicator in Al-alloyed medium-Mn steel processed by intercritical annealing

被引:9
|
作者
Skowronek, Adam [1 ]
Grajcar, Adam [1 ]
Sozanska-Jedrasik, Liwia [2 ]
Radwanski, Krzysztof [2 ]
Matus, Krzysztof [3 ]
Opara, Jaroslaw [2 ]
机构
[1] Silesian Tech Univ, Fac Mech Engn, Dept Engn Mat & Biomat, Konarskiego 18a St, PL-44100 Gliwice, Poland
[2] Lukasiewicz Upper Silesian Inst Technol, 12-14 K Miarki St, PL-44100 Gliwice, Poland
[3] Silesian Tech Univ, Fac Mech Engn, Mat Res Lab, Konarskiego 18a St, PL-44100 Gliwice, Poland
关键词
Metastable retained austenite; Intercritical annealing; Plasticity; Medium-Mn; Microstructural evolution; Mechanical properties; MECHANICAL-PROPERTIES; THERMAL-STABILITY; MANGANESE; TRANSFORMATION; STABILIZATION; MARTENSITE; CARBON; AHSS;
D O I
10.1016/j.jmrt.2023.08.114
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Although most studies focus on the impact of the fraction of retained austenite (RA) on the relationship between strength and plasticity, this research explores the influence of the mechanical stability of RA, which is primarily affected by its grain size. To investigate this, samples of 5% Mn steel with varying fractions of RA, as well as different sizes and concentrations of carbon (C) and manganese (Mn), were produced by adjusting the soaking time during intercritical annealing (IA) between 1 and 300 min at a temperature of 680 degrees C. The mechanical properties of the samples were evaluated using static tensile tests. Detailed microstructural analyses were conducted before and after deformation through hardness tests, X-ray diffraction measurements (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM) images, TEM-EDS microanalysis, and electron backscatter diffraction (EBSD) phase and orientation maps. Additionally, thermodynamic calculations were used to supplement the experimental findings. The results suggest that both chemical enrichment and grain size reduction have comparable effects on stabilizing the RA. The wide variation of RA grain sizes from 0.02 to 0.15 mm(3) promotes a gradual and continuous martensitic transformation under strain throughout the entire strain range, leading to a uniform elongation exceeding 19% in the steel analyzed. However, the presence of an appropriate average size of RA (from similar to 0.07 to similar to 0.11 mm(3)) is crucial because grains smaller than similar to 0.02 mm(3) impede martensitic transformation, while coarse grains characterized by a volume greater than similar to 0.13 mm(3) result in significant transformation in an early stage of deformation. (C) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY license (http://creativecommons.org/licenses/by/4.0/).
引用
收藏
页码:3201 / 3213
页数:13
相关论文
共 50 条
  • [31] Microstructure evolution of medium-manganese Al-alloyed steel manufactured by double-step intercritical annealing: Effects of heating and cooling rates
    Kozlowska, Aleksandra
    Morawiec, Mateusz
    Petrov, Roumen H.
    Grajcar, Adam
    MATERIALS CHARACTERIZATION, 2023, 199
  • [32] Intercritical annealing temperature dependence of hydrogen embrittlement behavior of cold-rolled Al-containing medium-Mn steel
    Zhang, Yongjian
    Shao, Chengwei
    Wang, Jiaojiao
    Zhao, Xiaoli
    Hui, Weijun
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (39) : 22355 - 22367
  • [33] Transformation and Twinning-Induced Plasticity Effect in a Novel Heterogeneous Microstructural Medium-Mn Steel Processed by ART Annealing
    Hao Chen
    Haifeng Xu
    Tianpeng Zhou
    Zejun Chen
    JOM, 2022, 74 : 2826 - 2837
  • [34] Transformation and Twinning-Induced Plasticity Effect in a Novel Heterogeneous Microstructural Medium-Mn Steel Processed by ART Annealing
    Chen, Hao
    Xu, Haifeng
    Zhou, Tianpeng
    Chen, Zejun
    JOM, 2022, 74 (07) : 2826 - 2837
  • [35] Microstructural Characteristics and Tensile Behavior of a Hot-Rolled Medium-Mn Steel (0.25C-8.5Mn-0.5Si-2.5Al) Processed by Intercritical Annealing Treatment
    Yongjian Zhang
    JiaoJiao Wang
    Zhiqi Xie
    Xiaoli Zhao
    Weijun Hui
    Journal of Materials Engineering and Performance, 2020, 29 : 2623 - 2634
  • [36] Microstructural Characteristics and Tensile Behavior of a Hot-Rolled Medium-Mn Steel (0.25C-8.5Mn-0.5Si-2.5Al) Processed by Intercritical Annealing Treatment
    Zhang, Yongjian
    Wang, JiaoJiao
    Xie, Zhiqi
    Zhao, Xiaoli
    Hui, Weijun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (04) : 2623 - 2634
  • [37] Microstructure-Tensile Properties Relationship and Austenite Stability of a Nb-Mo Micro-Alloyed Medium-Mn TRIP Steel
    Liu, Chunquan
    Peng, Qichun
    Xue, Zhengliang
    Deng, Mingming
    Wang, Shijie
    Yang, Chengwei
    METALS, 2018, 8 (08):
  • [38] Tailoring retained austenite and mechanical property improvement in Al-Si-V containing medium Mn steel via direct intercritical rolling
    Hu, Jun
    Li, XuYang
    Meng, QingWang
    Wang, LingYu
    Li, YiZhuang
    Xu, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 855
  • [39] Effect of Intercritical Annealing Parameters and Starting Microstructure on the Microstructural Evolution and Mechanical Properties of a Medium-Mn Third Generation Advanced High Strength Steel
    Bhadhon, Kazi M. H.
    Wang, Xiang
    McNally, Elizabeth A.
    McDermid, Joseph R.
    METALS, 2022, 12 (02)
  • [40] Retained Austenite Stabilization Through Solute Partitioning During Intercritical Annealing in C-, Mn-, Al-, Si-, and Cr-Alloyed Steels
    Singon Kang
    Emmanuel De Moor
    John G. Speer
    Metallurgical and Materials Transactions A, 2015, 46 : 1005 - 1011