Creep-oxidation interaction of a new martensitic steel 9Cr3W3Co in water vapor at 650 °C

被引:3
作者
Shang, C. G. [1 ]
Wang, M. L. [1 ]
Zhou, Z. C. [2 ]
Lu, Y. H. [1 ]
机构
[1] Univ Sci & Technol Beijing, Natl Ctr Mat Serv Safety, Beijing 100083, Peoples R China
[2] Inner Mongolia North Heavy Ind Grp Corp Ltd, Baotou 014033, Peoples R China
关键词
Martensite steel; Creep; Microstructure evolution; Creep-oxidation interaction; FAILURE;
D O I
10.1016/j.matchar.2023.112823
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the creep tests in air and water vapor environment at 650 & DEG;C under 155-220 MPa were carried out to study the effect of water vapor on the creep property, creep deformation and creep fracture mechanisms of 9Cr3W3Co steel. The results indicated that the water vapor environment did not affect the creep deformation mechanism but affected the creep behaviors and life, which was determined by the stress level. Under the high applied stress level (& GE; 180 MPa) in water vapor, the thin oxide particle dispersion strengthening layer formed on the surface increased the strength of the subsurface structure, which led to a decrease in the steady-creep rate and an increase in the time of the steady-creep stage than that in air. On the other hand, the crack blunting caused by the recrystallization of microstructures ahead of crack tip delayed the creep fracture. As a result, the creep life increased in the water vapor environment. Under low applied stress (& LE; 155 MPa) in water vapor, the increase of cavities number in the inner oxide layer and cracks number on the oxide film/matrix interface led to the reduction of the effective bearing area of the material, and thus the steady-state creep rate increased and the time of steady-state creep stage decreased. Different creep damage forms induced by the interaction of different applied stresses and creep environments affected creep fracture process and creep life. Oxidation in water vapor accelerated the connection of existing creep cavities on lath boundaries by promoting crack growth, thereby accelerating creep damage, which led to a significant reduction in creep life.
引用
收藏
页数:14
相关论文
共 31 条
  • [21] Microstructural Evolution of a Re-Containing 10% Cr-3Co-3W Steel during Creep at Elevated Temperature
    Fedoseeva, Alexandra
    Brazhnikov, Ivan
    Degtyareva, Svetlana
    Nikitin, Ivan
    Kaibyshev, Rustam
    [J]. METALS, 2023, 13 (10)
  • [22] The Laves Phase Evolution of 9Cr-3W-3Co Steel under Long Term Isothermal Treatment
    Ma, Longteng
    Bai, Yin
    Liu, Zhengdong
    [J]. STEEL RESEARCH INTERNATIONAL, 2017, 88 (08)
  • [23] Effect of Alloying on the Nucleation and Growth of Laves Phase in the 9-10%Cr-3%Co Martensitic Steels during Creep
    Fedoseeva, Alexandra
    Nikitin, Ivan
    Tkachev, Evgeniy
    Mishnev, Roman
    Dudova, Nadezhda
    Kaibyshev, Rustam
    [J]. METALS, 2021, 11 (01) : 1 - 19
  • [24] Morphology of Secondary Phase Particles and Stability of Subgrain Structure in Martensitic Steel 10Cr9Co3W2MoVNbB (ASTM A335 P92) Under Creep Conditions
    Tkachev, E. S.
    Kaibyshev, R. O.
    [J]. METAL SCIENCE AND HEAT TREATMENT, 2024, : 474 - 481
  • [25] Correlation of Creep Strength and Microstructural Evolution of a Boron Alloyed 9Cr3W3CoVNb Steel in as-received and Welded Condition
    Mayr, Peter
    Martin, Francisca Mendez
    Albu, Mihaela
    Cerjak, Horst
    [J]. CREEP & FRACTURE IN HIGH TEMPERATURE COMPONENTS: DESIGN & LIFE ASSESSMENT ISSUES, PROCEEDINGS, 2009, : 1029 - +
  • [26] Correlation of creep strength and microstructural evolution of a boron alloyed 9Cr3W3CoVNb steel in as-received and welded condition
    Mayr, Peter
    Martin, Francisca Mendez
    Albu, Mihaela
    Cerjak, Horst
    [J]. MATERIALS AT HIGH TEMPERATURES, 2010, 27 (01) : 67 - 72
  • [27] Precipitation Behavior in the Heat-Affected Zone of Boron-Added 9Cr-3W-3Co Steel During Post-Weld Heat Treatment and Creep Deformation
    Liu, Yuan
    Tsukamoto, Susumu
    Sawada, Kota
    Tabuchi, Masaaki
    Abe, Fujio
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (05): : 1843 - 1854
  • [28] Microstructural evolution and its effect on tensile properties of 10Cr-2W-3Co martensitic steel during thermal exposure
    Wang, Yuqi
    Zhao, Yihan
    Huang, Yao
    Yu, Shan
    Shang, Jiaxin
    Yang, Chengkun
    Zhang, Hexin
    Zhao, Chengzhi
    [J]. MATERIALS TODAY COMMUNICATIONS, 2025, 44
  • [29] The effect of ultra-fast surface hardening and strengthening on microstructure and mechanical properties of cast (9Cr-3Co-3W) heat-resistant steel
    Saood, Modar
    El-Kashif, Emad El-Din Farouk
    Rabeeh, Bakr Mohamed
    Enan, Lina Abdelkader
    [J]. JOURNAL OF MATERIALS SCIENCE, 2024, 59 (24) : 11110 - 11121
  • [30] Microstructure and Mechanical Properties of Thick 08Cr9W3Co3VNbCuBN Heat-Resistant Steel welded Joint by TIP TIG Welding
    Wang, Yongbin
    Liu, Peng
    Fan, Hongju
    Guo, Xinfang
    Wan, Fuwei
    [J]. MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2023, 26