Regulating the solventized structure to achieve highly reversible zinc plating/stripping for dendrite-free Zn anode by sulfolane additive

被引:23
作者
Cao, Heng [1 ]
Huang, Xiaomin [1 ]
Li, Yuanxia [1 ]
Liu, Yu [1 ]
Zheng, Qiaoji [1 ]
Huo, Yu [1 ]
Zhao, Ruyi [2 ,4 ]
Zhao, Jingxin [2 ,3 ]
Lin, Dunmin [1 ,2 ]
机构
[1] Sichuan Normal Univ, Coll Chem & Mat Sci, Chengdu 610066, Peoples R China
[2] Harbin Inst Technol, Sch Energy Sci & Engn, Harbin 150001, Peoples R China
[3] Hong Kong Polytech Univ, Nanotechnol Ctr, Sch Fash & Text, Hung Hom,Kowloon, Hong Kong 999077, Peoples R China
[4] Shanghai Electromech Engn Inst, Shanghai 201109, Peoples R China
关键词
Aqueous zinc ion battery; Electrolyte additive; Zinc dendrites; Side reactions; Sulfolane;
D O I
10.1016/j.cej.2022.140538
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Aqueous zinc ion batteries (AZIBs) are a kind of ideal rechargeable batteries due to their high theoretical ca-pacity, low cost and good safety. However, dendrite growth and side reactions prevent AZIBs from becoming excellent energy storage devices. Herein, an electrolyte additive of sulfolane (SL) is added to ZnSO4 electrolyte to inhibit zinc dendrite growth and side reactions. It is found that SL molecules replace water molecules in the solventized structure of [Zn(H2O)6]2+, reducing the number of highly chemically active water molecules at the interface between anode and electrolyte, thus inhibiting the growth of zinc dendrites and side reactions. As a result, a super long cycle life of > 4300 h is achieved at 2 mA cm-2/0.5 mAh cm-2 (>5700 h at 1 mA cm-2/0.25 mAh cm-2) for the Zn-Zn symmetrical cell with SL additive, which is much higher than that of the symmetrical battery without additive (50 h). The present work provides a general strategy to achieve the inhibition of zinc dendrites and side reactions via tailoring the solventized structure of [Zn(H2O)6]2+ by using small organic molecular as electrolyte additive to reduce the number of highly chemically active water molecules at the interface between zinc metal and aqueous electrolyte.
引用
收藏
页数:9
相关论文
共 57 条
  • [1] Elimination of Zinc Dendrites by Graphene Oxide Electrolyte Additive for Zinc-Ion Batteries
    Abdulla, Jufni
    Cao, Jin
    Zhang, Dongdong
    Zhang, Xinyu
    Sriprachuabwong, Chakrit
    Kheawhom, Soorathep
    Wangyao, Panyawat
    Qin, Jiaqian
    [J]. ACS APPLIED ENERGY MATERIALS, 2021, 4 (05): : 4602 - 4609
  • [2] Cationic Surfactant-Type Electrolyte Additive Enables Three-Dimensional Dendrite-Free Zinc Anode for Stable Zinc-Ion Batteries
    Bayaguud, Aruuhan
    Luo, Xiao
    Fu, Yanpeng
    Zhu, Changbao
    [J]. ACS ENERGY LETTERS, 2020, 5 (09) : 3012 - 3020
  • [3] An efficient electrolyte additive of tetramethylammonium sulfate hydrate for Dendritic-Free zinc anode for aqueous Zinc-ion batteries
    Cao, Heng
    Huang, Xiaomin
    Liu, Yu
    Hu, Qiang
    Zheng, Qiaoji
    Huo, Yu
    Xie, Fengyu
    Zhao, Jingxin
    Lin, Dunmin
    [J]. JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2022, 627 : 367 - 374
  • [4] Regulating solvation structure to stabilize zinc anode by fastening the free water molecules with an inorganic colloidal electrolyte
    Cao, Jin
    Zhang, Dongdong
    Yue, Yilei
    Chanajaree, Rungroj
    Wang, Shanmin
    Han, Jiantao
    Zhang, Xinyu
    Qin, Jiaqian
    Huang, Yunhui
    [J]. NANO ENERGY, 2022, 93
  • [5] Strategies of regulating Zn2+ solvation structures for dendrite-free and side reaction-suppressed zinc-ion batteries
    Cao, Jin
    Zhang, Dongdong
    Zhang, Xinyu
    Zeng, Zhiyuan
    Qin, Jiaqian
    Huang, Yunhui
    [J]. ENERGY & ENVIRONMENTAL SCIENCE, 2022, 15 (02) : 499 - 528
  • [6] Solvation Structure Design for Aqueous Zn Metal Batteries
    Cao, Longsheng
    Li, Dan
    Hu, Enyuan
    Xu, Jijian
    Deng, Tao
    Ma, Lin
    Wang, Yi
    Yang, Xiao-Qing
    Wang, Chunsheng
    [J]. JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2020, 142 (51) : 21404 - 21409
  • [7] Hydrogen Bond-Functionalized Massive Solvation Modules Stabilizing Bilateral Interfaces
    Chen, Wenyong
    Guo, Shan
    Qin, Liping
    Li, Lanyan
    Cao, Xinxin
    Zhou, Jiang
    Luo, Zhigao
    Fang, Guozhao
    Liang, Shuquan
    [J]. ADVANCED FUNCTIONAL MATERIALS, 2022, 32 (20)
  • [8] Polyvinyl alcohol coating induced preferred crystallographic orientation in aqueous zinc battery anodes
    Chen, Xiujuan
    Li, Wei
    Hu, Shanshan
    Akhmedov, Novruz G.
    Reed, David
    Li, Xiaolin
    Liu, Xingbo
    [J]. NANO ENERGY, 2022, 98
  • [9] Arginine Cations Inhibiting Charge Accumulation of Dendrites and Boosting Zn Metal Reversibility in Aqueous Rechargeable Batteries
    Chen, Zehai
    Chen, Hongzhan
    Che, Youcai
    Cheng, Luo
    Zhang, Hao
    Chen, Jian
    Xie, Fangyan
    Wang, Nan
    Jin, Yanshuo
    Meng, Hui
    [J]. ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2021, 9 (19) : 6855 - 6863
  • [10] In-situ grown porous protective layers with high binding strength for stable Zn anodes
    Cui, Mangwei
    Yan, Boxun
    Mo, Funian
    Wang, Xiaoqi
    Huang, Yan
    Fan, Jun
    Zhi, Chunyi
    Li, Hongfei
    [J]. CHEMICAL ENGINEERING JOURNAL, 2022, 434