The effect of milling time and heat treatment on the synthesis of the Cr2AlC MAX phase

被引:2
作者
Mansouri, Bahman [1 ]
Rafiei, Mahdi [1 ,3 ]
Ebrahimzadeh, Iman [1 ]
Naeimi, Farid [1 ]
Barekat, Masoud [2 ]
机构
[1] Islamic Azad Univ, Adv Mat Res Ctr, Dept Mat Engn, Najafabad Branch, Najafabad, Iran
[2] Malek Ashtar Univ Technol, Fac Mat & Mfg Engn, Tehran, Iran
[3] Islamic Azad Univ, Adv Mat Res Ctr, Dept Mat Engn, Najafabad Branch, Najafabad 8514143131, Isfahan Provinc, Iran
关键词
Cr2AlC MAX phase; mechanical alloying; intermetallic compounds; heat treatment; phase analysis; Thermodynamics; DTA; Microstructure; MECHANICAL-PROPERTIES; TRIBOLOGICAL BEHAVIOR; ELECTRICAL-PROPERTIES; ELEMENTAL POWDERS; HOT CORROSION; OXIDATION; TI3ALC2; SALT; CRYSTALLIZATION; MICROSTRUCTURE;
D O I
10.1080/00084433.2023.2251210
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Synthesis of the Cr2AlC MAX phase was investigated by mechanical alloying. Cr, Al, and C powders were milled and heat treated at temperature range of 500-1300 degrees C for 1 h. X-ray diffraction and differential thermal analysis were used to study the reaction mechanisms and a scanning electron microscope was used to observe the microstructures. The Cr7C3 and Cr-Al compounds were formed by reactions among the initial elements. These compounds transformed to the Cr2AlC phase by increasing the temperature. The maximum amount of Cr2AlC phase was equal to 97.23 wt.%, which was related to the sample with 45 h of ball milling and subsequent heat treatment at temperature of 700 degrees C. DTA results showed a major exothermic peak at about 685 degrees C, which represents the formation of the Cr2AlC. This indicates that most conversions are completed in a single stage, below the temperature of 800 degrees C.
引用
收藏
页码:970 / 980
页数:11
相关论文
共 67 条
[11]   Synthesis of Cr2AlC from Elemental Powders with Modified Pressureless Spark Plasma Sintering [J].
Ge Mengni ;
Wang Xiaofan ;
Li Gaiye ;
Lu Chen ;
Zhang Jianfeng ;
Tu Rong .
JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2019, 34 (02) :287-292
[12]   Effect of sintering method on the microstructure of pure Cr2AlC MAX phase ceramics [J].
Gonzalez-Julian, Jesus ;
Onrubia, Sara ;
Bram, Martin ;
Guillon, Olivier .
JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2016, 124 (04) :415-420
[13]   CHEMICALLY VAPOR-DEPOSITED TI3SIC2 [J].
GOTO, T ;
HIRAI, T .
MATERIALS RESEARCH BULLETIN, 1987, 22 (09) :1195-1201
[14]   Reaction Synthesis of Cr2AlC Ceramics Powders [J].
Guan, Chunlong ;
Zhang, Ziping ;
Shan, Yingchun ;
Wang, Chunhua .
CHINESE CERAMICS COMMUNICATIONS III, 2013, 624 :13-+
[15]   Tribological behavior of select MAX phases against Al2O3 at elevated temperatures [J].
Gupta, S. ;
Filimonov, D. ;
Palanisamy, T. ;
Barsoum, M. W. .
WEAR, 2008, 265 (3-4) :560-565
[16]   Ambient and 550°C tribological behavior of select MAX phases against Ni-based superalloys [J].
Gupta, S. ;
Filimonov, D. ;
Zaitsev, V. ;
Palanisamy, T. ;
Barsoum, M. W. .
WEAR, 2008, 264 (3-4) :270-278
[17]   Thermodynamic evaluation of the Al-Cr-C system [J].
Hallstedt, Bengt ;
Music, Denis ;
Sun, Zhimei .
INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2006, 97 (05) :539-542
[18]   Physical and mechanical properties of bulk Ta4AIC3 ceramic prepared by an in situ reaction Synthesis/Hot-Pressing method [J].
Hu, Chunfeng ;
Lin, Zhijun ;
He, Lingfeng ;
Bao, Yiwang ;
Wang, Jingyang ;
Li, Meishuan ;
Zhou, Yanchun .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2007, 90 (08) :2542-2548
[19]   Saturation of ion irradiation effects in MAX phase Cr2AlC [J].
Huang, Qing ;
Han, Han ;
Liu, Renduo ;
Lei, Guanhong ;
Yan, Long ;
Zhou, Jie ;
Huang, Qing .
ACTA MATERIALIA, 2016, 110 :1-7
[20]   KOHLENSTOFFHALTIGE TERNARE VERBINDUNGEN (H-PHASE) [J].
JEITSCHKO, W ;
NOWOTNY, H ;
BENESOVSKY, F .
MONATSHEFTE FUR CHEMIE, 1963, 94 (04) :672-&