Crack Initiation Mechanism of AISI 4340 Steel for High-Cycle Torsional Fatigue Loading

被引:1
作者
Xu, Zikuan [1 ]
Wang, Bin [1 ]
Zhang, Peng [1 ]
Zhu, Yankun [1 ]
Wang, Xuegang [1 ]
Zhang, Zhefeng [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shichangxu Innovat Ctr Adv Mat, Shenyang 110016, Peoples R China
基金
中国国家自然科学基金;
关键词
AISI; 4340; steels; crack initiations; high-cycle torsional fatigues; inclusions; lath martensite; HIGH-STRENGTH STEELS; INCLUSION TYPES; MARAGING-STEEL; BEHAVIOR; MICROSTRUCTURE; GROWTH; MODEL; SIZE; LIFE; INTRUSIONS;
D O I
10.1002/srin.202200976
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The nucleation of microstructural fatigue cracks in AISI 4340 steel is investigated. The pre-electropolished specimen is employed for the observation of the very early stage of fatigue crack initiation correlated with the microstructure. It is found that there are precipitate-free zones (PFZs) around the lath and packet boundary, and the strength of PFZ is lower than that of the lath due to the lack of second-phase strengthening. Therefore, the fatigue crack would first initiate within the PFZ. Besides, the initiated crack plane usually is the maximum shear stress plane. However, the MnS inclusions would cause stress concentration so that the lath boundary (LB) deviating from the maximum shear stress plane could also have sufficient driving force to crack. In contrast, when the LB is vertical to the cracked MnS inclusion, it would prevent the crack from propagating into the matrix because of the anisotropy of lath martensite. The effects of the stress concentration caused by the MnS inclusion on the maximum deviation angle and the S-N curve are discussed.
引用
收藏
页数:8
相关论文
共 44 条
  • [1] Significance of size and type of inclusions on giga-cycle fatigue in high-strength steels
    Abe, T
    Furuya, Y
    Matsuoka, S
    [J]. TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2003, 89 (06): : 711 - 717
  • [2] The role of microstructure in fatigue crack initiation of 9-12%Cr reduced activation ferritic-martensitic steel
    Batista, M. N.
    Marinelli, M. C.
    Herenu, S.
    Alvarez-Armas, I.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2015, 72 : 75 - 79
  • [3] A microstructure-based fatigue-crack-initiation model
    Chan, KS
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34 (01): : 43 - 58
  • [4] Effect of Hardness on the Ballistic Impact Behavior of High-Strength Steels Against 7.62-mm Armor Piercing Projectiles
    Demir, Teyfik
    Ubeyli, Mustafa
    Yildirim, R. O.
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2009, 18 (02) : 145 - 153
  • [5] A MODEL OF EXTRUSIONS AND INTRUSIONS IN FATIGUED METALS .2. SURFACE ROUGHENING BY RANDOM IRREVERSIBLE SLIP
    DIFFERT, K
    ESSMANN, U
    MUGHRABI, H
    [J]. PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1986, 54 (02): : 237 - 258
  • [6] A MODEL OF EXTRUSIONS AND INTRUSIONS IN FATIGUED METALS .1. POINT-DEFECT PRODUCTION AND THE GROWTH OF EXTRUSIONS
    ESSMANN, U
    GOSELE, U
    MUGHRABI, H
    [J]. PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1981, 44 (02): : 405 - 426
  • [7] GARRISON WM, 1990, JOM-J MIN MET MAT S, V42, P20
  • [8] 3-D growth of a short fatigue crack within a polycrystalline microstructure studied using combined diffraction and phase-contrast X-ray tomography
    Herbig, Michael
    King, Andrew
    Reischig, Peter
    Proudhon, Henry
    Lauridsen, Erik M.
    Marrow, James
    Buffiere, Jean-Yves
    Ludwig, Wolfgang
    [J]. ACTA MATERIALIA, 2011, 59 (02) : 590 - 601
  • [9] High cycle fatigue behavior of Ti-5Al-5Mo-5V-3Cr-1Zr titanium alloy with lamellar microstructure
    Huang, Chaowen
    Zhao, Yongqing
    Xin, Shewei
    Tan, Changsheng
    Zhou, Wei
    Li, Qian
    Zeng, Weidong
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 682 : 107 - 116
  • [10] Effect of microstructure on high cycle fatigue behavior of Ti-5Al-5Mo-5V-3Cr-1Zr titanium alloy
    Huang, Chaowen
    Zhao, Yongqing
    Xin, Shewei
    Tan, Changsheng
    Zhou, Wei
    Li, Qian
    Zeng, Weidong
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2017, 94 : 30 - 40