Industrial-scale fabrication of FeSiCr magnetic powder cores with high magnetic permeability and low loss

被引:10
|
作者
Wang, Pu [1 ]
Zhu, Zhengqu [1 ]
Liu, Jiaqi [1 ]
Wang, Chengfei [1 ]
Pang, Jing [2 ]
Zhang, Jiaquan [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Qingdao Yunlu Adv Mat Technol Co Ltd, Qingdao 266232, Shandong, Peoples R China
关键词
Soft magnetic powder cores; Industrial-scale process; Insulating layer; Soft magnetic properties; Corrosion resistance; PHOSPHATE COATINGS; COMPOSITES; FE; EVOLUTION; MICROSTRUCTURE;
D O I
10.1016/j.jallcom.2023.171095
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
FeSiCr magnetic powders is the key raw material for inductive components such as molding choke and power factor correction (PFC) inductors. In this paper, the industrial-scale insulation coating process of high-performance FeSiCr soft magnetic powder cores (SMPCs) were studied by using mature and environmentally friendly silica sol (SiO2), aluminum dihydrogen phosphate solution (AHP), glass powders (GP), and phosphoric acid (PA) as insulators and water-soluble sodium silicate (NSO) as an inorganic binder, respectively. A comprehensive analysis of the SEM, EDS, and XPS results showed that the surface insulation layer uniformity of the four coating powders is poor due to the irregular morphology of the FeSiCr powder, with the glass powder having the worst coating uniformity due to partial agglomeration occurring in mechanical mixing. The four coated powders all had high saturation magnetization (173.1-176.5 emu.g(-1)), in which the chemical reaction of FeSiCr in the phosphoric acid coating process consumed Fe atoms, resulting in the lowest M-s of the powders in the several coating processes. At the corresponding optimum heat treatment temperature, the FeSiCr@SiO2 @NSO SMPCs had the highest permeability of 96.1, while the FeSiCr@PA@NSO SMPCs had the lowest at 75.5, due to the phosphoric acid consuming part of the ferromagnetic material and the loose porous structure of the phosphate layer further reducing the density of SMPCs. The total losses of the four powder cores are low (228.9-259.2 mW.cm(-3), 100 Gs, 1000 kHz), while loss separation and experiments with different pressing tonnages showed that the eddy current losses of SMPCs was higher than the hysteresis losses, which was caused by the irregular morphology of FeSiCr powders. The FeSiCr@SiO2 @NSO SMPCs exhibit optimum corrosion resistance due to the uniform coating of the SiO2 nano-insulating layer on the powders surface as a result of the strong bonding of the silica sol with FeSiCr. As can be seen, FeSiCr@SiO2 @NSO SMPCs prepared using silica sols have very high saturation magnetization, very high permeability, low core loss, and good corrosion resistance compared to the other three insulation processes and can be industrially produced on a large scale, offering great application prospects in the field of high current and high frequency.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] FeSiCr Alloy Powder to Carbonyl Iron Powder Mixing Ratio Effects on the Magnetic Properties of the Iron-Based Alloy Powder Cores Prepared Using Screen Printing
    Hsiang, Hsing-I.
    Chuang, Kai-H.
    Lee, Wen-H.
    MATERIALS, 2021, 14 (04) : 1 - 8
  • [22] Development of FeCoMnAl multi-principal element alloys and soft magnetic powder cores with excellent magnetic properties and high temperature magnetic stability
    Yang, Liping
    Dong, Yaqiang
    Gao, Wei
    Jia, Xingjie
    Zhang, Junyao
    Li, Yanqiu
    Li, Qiang
    Man, Qikui
    Shen, Baogen
    MATERIALS & DESIGN, 2024, 239
  • [23] Low core loss combined with high permeability for Fe-based amorphous powder cores produced by gas atomization powders
    Chang, Chuntao
    Dong, Yaqiang
    Liu, Min
    Guo, Houqiang
    Xiao, Qiang
    Zhang, Yunfan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 766 : 959 - 963
  • [24] Effects of structural transformation on magnetic properties of AlCoFeCr high-entropy soft magnetic powder cores by adjusting Co/Fe ratio
    Gao, Wei
    Dong, Yaqiang
    Ma, Yan
    Wu, Hang
    Jia, Xingjie
    Liu, Zhonghao
    Li, Xubin
    Zhao, Ronglin
    Wu, Shouding
    Li, Qiang
    He, Aina
    Li, Jiawei
    MATERIALS & DESIGN, 2023, 225
  • [25] Study on the High-Efficiency Smoothness Grinding of Soft Magnetic Powder Cores
    Ueno, Tomoyuki
    Ishimine, Tomoyuki
    Matsunuma, Kenji
    Nishioka, Takao
    Mochida, Yasushi
    Shimada, Yoshiyuki
    ADVANCES IN ABRASIVE TECHNOLOGY XV, 2012, 565 : 10 - +
  • [26] Enhanced high frequency properties of FeSiBPC amorphous soft magnetic powder cores with novel insulating layer
    Chi, Qiang
    Chang, Liang
    Dong, Yaqiang
    Zhang, Yiqun
    Zhou, Bang
    Zhang, Chengzhong
    Pan, Yan
    Li, Qiang
    Li, Jiawei
    He, Aina
    Wang, Xinmin
    ADVANCED POWDER TECHNOLOGY, 2021, 32 (05) : 1602 - 1610
  • [27] Realizing high-resistivity and low-loss Fe-Si-Al based soft magnetic powder cores through interfacial chemistry regulation
    Wu, Z. Y.
    Kang, L.
    Liao, X. W.
    Kong, H.
    Wang, H. C.
    Wang, R.
    CERAMICS INTERNATIONAL, 2023, 49 (12) : 19870 - 19878
  • [28] Fabrication of high-performance FeSiCr-based soft magnetic composites using thermal decomposition of salt compounds
    Huang, Huaqin
    Wang, Rui
    Li, Kaixuan
    Dai, Bing
    Wu, Zhaoyang
    Lyu, Peisheng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 : 3291 - 3302
  • [29] Strategy to Enhance Magnetic Properties of Fe78Si9B13 Amorphous Powder Cores in the Industrial Condition
    Sun, Haibo
    Wang, Ce
    Chen, Weihong
    Lin, Jiexin
    METALS, 2019, 9 (03):
  • [30] Soft magnetic properties of Fe-Ni powder cores in the high frequency range
    Nguyen, Mai Phuong
    Yoshida, Shigeyoshi
    Okamoto, Satoshi
    Muroga, Sho
    Miyazaki, Takamichi
    Endo, Yasushi
    AIP ADVANCES, 2024, 14 (01)