Mechanical properties, biosafety, and shearing bonding strength of glass fiber-reinforced PEEK composites used as post-core materials

被引:7
|
作者
Zhao, Ting [1 ]
Jiang, Zilong [2 ]
Ge, Yongcheng [1 ]
Yin, Haoyu [1 ]
Yang, Qi [1 ]
Li, Ruozhu [3 ]
Chen, Zheng [2 ]
Zhang, Haibo [2 ]
Liu, Xiaoqiu [1 ]
机构
[1] Jilin Univ, Hosp Stomatol, Dept Geriatr Dent, Changchun, Peoples R China
[2] Jilin Univ, Coll Chem, Natl & Local Joint Engn Lab Synthet Technol High P, Changchun, Peoples R China
[3] Jilin Univ, Hosp Stomatol, Dept Pediat Dent, Changchun, Peoples R China
关键词
Dental; Post; -core; PEEK; Glass fiber; POLYETHERETHERKETONE PEEK; FRACTURE-RESISTANCE; POSTS; RESIN; SURFACE; CORE;
D O I
10.1016/j.jmbbm.2023.106047
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Objective: To investigate the mechanical properties, biosafety, and shearing bonding strength of glass fibers-reinforced polyether-ether-ketone (PEEK-GF) for post-core materials.Methods: PEEK-GF composites with different glass fiber contents were prepared by extrusion injection and named PEEK-GF30, PEEK-GF40, and PEEK-GF50. Mechanical properties including flexural modulus, flexural strength, Vickers hardness, and compression strength were tested. The cross-sectional morphology was examined using scanning electron microscopy (SEM). Cytotoxicity was studied in vitro with Cell-counting kit-8 (CCK-8). Cell morphology was observed under a microscope. Cell growth on the composites' surfaces was analyzed with DAPI staining. The shearing bonding strength (SBS) of PEEK-GF50 was assessed after applying different pretreatments. Failure modes were evaluated by microscopy. SEM and contact-angle measurements were performed on the surfaces. Statistical analysis was conducted using one-way ANOVA (P < 0.05).Results: The mechanical properties of PEEK-GF composites improved with increased GF content. The PEEK-GF50 group exhibited flexural modulus (17.4 & PLUSMN; 0.5 GPa) close to that of dentin (18.6 GPa) and showed the highest flexural strength (350.0 & PLUSMN; 2.9 MPa), Vickers hardness (47.6 & PLUSMN; 4.5 HV), and compressive strength (264.0 & PLUSMN; 18.0 MPa). The SEM analysis demonstrated that the PEEK matrix combined well with glass fibers. The CCK-8 results confirmed the biosafety of all groups. DAPI staining indicated that cells were growing well on the composites' surface. The sample that was pretreated with sandblasting and plasma showed the highest SBS (16.0 & PLUSMN; 1.7 MPa). Significance: The PEEK-GF composites demonstrated excellent mechanical properties, biosafety, and SBS, and have great potential to serve as post-core materials.
引用
收藏
页数:9
相关论文
共 50 条
  • [1] Mechanical properties of woven glass fiber-reinforced composites
    Kanie, Takahito
    Arikawa, Hiroyuki
    Fujii, Koichi
    Ban, Seiji
    DENTAL MATERIALS JOURNAL, 2006, 25 (02) : 377 - 381
  • [2] Bonding of Core Build-Up Composites with Glass Fiber-Reinforced Posts
    Fragkouli, Margarita
    Tzoutzas, Ioannis
    Eliades, George
    DENTISTRY JOURNAL, 2019, 7 (04)
  • [3] Mechanical properties of woven glass fiber-reinforced polymer composites
    Gao, Guangfa
    Li, Yongchi
    EMERGING MATERIALS RESEARCH, 2016, 5 (02) : 201 - 208
  • [4] Mechanical Properties of Long Glass Fiber-Reinforced Polyolefin Composites
    Tan, Hong-Sheng
    Yu, Yuan-Zhang
    Li, Li-Ping
    Liu, Xue-Jing
    Tan, Zhe-Xing
    Gong, Yan-Yan
    Li, Ai-Xiang
    POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2015, 54 (13) : 1343 - 1348
  • [5] STRENGTH PROPERTIES OF FIBER-REINFORCED COMPOSITES
    VASILOS, T
    WOLFF, EG
    JOURNAL OF METALS, 1966, 18 (05): : 583 - &
  • [6] Fracture resistance and marginal gap formation of post-core restorations: influence of different fiber-reinforced composites
    Márk Fráter
    Lippo Lassila
    Gábor Braunitzer
    Pekka K. Vallittu
    Sufyan Garoushi
    Clinical Oral Investigations, 2020, 24 : 265 - 276
  • [7] Fracture resistance and marginal gap formation of post-core restorations: influence of different fiber-reinforced composites
    Frater, Mark
    Lassila, Lippo
    Braunitzer, Gabor
    Vallittu, Pekka K.
    Garoushi, Sufyan
    CLINICAL ORAL INVESTIGATIONS, 2020, 24 (01) : 265 - 276
  • [8] Mechanical and structural properties of glass fiber-reinforced polypropylene (PPGF) composites
    Kallel, Tasnim Kossentini
    Taktak, Rym
    Guermazi, Noamen
    Mnif, Nizar
    POLYMER COMPOSITES, 2018, 39 (10) : 3497 - 3508
  • [9] MECHANICAL AND ELECTRICAL-PROPERTIES OF GLASS AND CARBON FIBER-REINFORCED COMPOSITES
    HEADIFEN, GR
    FAHRENTHOLD, EP
    JOURNAL OF ENERGY RESOURCES TECHNOLOGY-TRANSACTIONS OF THE ASME, 1991, 113 (03): : 176 - 181
  • [10] Ultimate strength properties of fiber-reinforced composites
    Hild, F
    Feillard, P
    RELIABILITY ENGINEERING & SYSTEM SAFETY, 1997, 56 (03) : 225 - 235