Microwave-enhanced selective leaching calcium from steelmaking slag to fix CO2 and produce high value-added CaCO3

被引:12
作者
Liu, Lincheng [1 ,2 ]
Fan, Xiaohui [1 ,2 ]
Gan, Min [1 ,2 ]
Wei, Jiaoyang [1 ,2 ]
Gao, Zitan [1 ]
Sun, Zengqing [1 ,2 ]
Ji, Zhiyun [1 ,2 ]
Wu, Yufeng [1 ]
Li, Jinhua [1 ]
机构
[1] Cent South Univ, Sch Minerals Proc & Bioengn, 932 South LushanRoad, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Minist Educ Carbon Emiss Reduct Met Resource Explo, Engn Res Ctr, Changsha 410083, Peoples R China
基金
中国国家自然科学基金;
关键词
Steel slag; Microwave-enhanced; Leaching kinetics; CO2; fixation; Crystal whiskerCaCO3; KINETICS; EXTRACTION; OPTIMIZATION; CARBONATION; BATTERIES; ACID;
D O I
10.1016/j.seppur.2023.125395
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The abundant resources of steel slag make it an intriguing prospect for long-term CO2 storage by mineral carbonation. Herein, the dissolution of steel slag in an acetic acid (HAc) solution and the fixation of CO2 in the leachate of steel slag to synthesize high-value CaCO3 were investigated. Results show that the microwave water bath condition is beneficial for improving the leaching rate of Ca and Mg elements in steel slag, while the low-concentration HAc solution displays high selectivity for Ca + Mg. In a water bath reaction enhanced by microwave, the leaching rate and selectivity of Ca + Mg can be increased by elevating the reaction temperature, extending the leaching time, lowering the concentration of HAc solution, and increasing the stirring rate. The kinetic parameters of the calcium element, including the apparent activation energy, were determined to be 14.51 kJ & sdot;mol- 1, suggesting control by surface chemical reactions. Finally, high-purity CaCO3 crystal whiskers can be synthesized under 400 W ultrasonic conditions with a reaction temperature of 70 degrees C, reaction time of 15 min, and a solution pH at 9.1 by introducing 20 % CO2 into the leachate. This strategy facilitates the concurrent utilization of dilute CO2 flue gas and voluminous solid steel slag waste, thereby improving the economic and environmental performance of the steel industry.
引用
收藏
页数:14
相关论文
共 37 条
  • [1] Kinetic study on the leaching of spent nickel oxide catalyst with sulfuric acid
    Abdel-Aal, EA
    Rashad, MM
    [J]. HYDROMETALLURGY, 2004, 74 (3-4) : 189 - 194
  • [2] [Anonymous], 1998, Environ. Geosci., DOI DOI 10.1046/J.1526-0984.1998.08014.X
  • [3] Electric arc furnace slag and its use in hydraulic concrete
    Arribas, Idoia
    Santamaria, Amaia
    Ruiz, Estela
    Ortega-Lopez, Vanesa
    Manso, Juan M.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2015, 90 : 68 - 79
  • [4] Experimental investigation of enhanced carbonation by solvent extraction for indirect CO2 mineral sequestration
    Bao, Weijun
    Li, Huiquan
    Zhang, Yi
    [J]. GREENHOUSE GASES-SCIENCE AND TECHNOLOGY, 2014, 4 (06): : 785 - 799
  • [5] Leaching kinetics study of neodymium from the scrap magnet using acetic acid
    Behera, S. S.
    Parhi, P. K.
    [J]. SEPARATION AND PURIFICATION TECHNOLOGY, 2016, 160 : 59 - 66
  • [6] Cheng C., 2023, Sci. Total Environ., V891, P11, DOI [10.1016/j.scitotenv.2023.16420, DOI 10.1016/J.SCITOTENV.2023.16420]
  • [7] Economic perspectives and policy insights on carbon capture, storage, and utilization for sustainable development
    Gowd, Sarath C.
    Ganeshan, Prabakaran
    Vigneswaran, V. S.
    Hossain, Md Shahadat
    Kumar, Deepak
    Rajendran, Karthik
    Ngo, Huu Hao
    Pugazhendhi, Arivalagan
    [J]. SCIENCE OF THE TOTAL ENVIRONMENT, 2023, 883
  • [8] Integration of Two Waste Streams for Carbon Storage and Utilization: Enhanced Metal Extraction from Steel Slag Using Biogenic Volatile Organic Acids
    Hong, Sujin
    Huang, Haonan Danny
    Rim, Guanhe
    Park, Youngjune
    Park, Ah-Hyung Alissa
    [J]. ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2020, 8 (50) : 18519 - 18527
  • [9] IEA, 2020, Credible pathways to 1.5 C
  • [10] IEA - International Energy Agency, 2023, CO2 EM 2022