Effect of Graphite Powder Addition on Microstructure and Room Temperature Mechanical Properties of Ti-45Al-8Nb Alloys

被引:2
作者
Wang, Sheng [1 ]
Jin, Yuliang [2 ]
Chen, Xiguo [1 ]
Yang, Xiaohong [3 ,4 ]
机构
[1] Quzhou Coll Technol, Dept Mech Engn, Quzhou 324000, Peoples R China
[2] Anhui Polytech Univ, Sch Mat Sci & Engn, Wuhu 241000, Peoples R China
[3] Jinhua Polytech, Academician Expert Workstn, Jinhua 321017, Peoples R China
[4] Key Lab Crop Harvesting Equipment Technol Zhejiang, Jinhua 321017, Peoples R China
关键词
TiAl alloys; graphite powder; Ti2AlC; microstructure; mechanical properties; TIAL ALLOYS; EVOLUTION; BEHAVIOR;
D O I
10.3390/coatings14010021
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The enhancement of the mechanical properties of TiAl alloys through the introduction of a second-phase reinforcement is highly essential. In this paper, using graphite powder as a carbon source, the Ti2AlC phase is introduced to improve the compression and friction properties of the TiAl alloy. Concurrently, the effects of graphite powder additions on the microstructure and room-temperature mechanical properties of Ti-45Al-8Nb-xC (mass%) alloys are investigated. The results show that as the volume fraction of Ti2AlC and the interdendritic gamma phase increases, the length-diameter ratio of the Ti2AlC phase decreases with increases in the graphite powder addition. The addition of graphite powder results in a refining effect on the grain size and lamellar spacing of the Ti-45Al-8Nb-xC (mass%) alloys. As the graphite powder content increases from 0 to 0.9 mass%, the microhardness increases from 557 HV to 647 HV. The room-temperature compressive strength and strain of the Ti-45Al-8Nb-xC (mass%) alloys first increase and then decrease with the addition of graphite powder. Specifically, when the content of graphite powder is 0.6 mass%, the alloy exhibits a maximum compressive strength and strain of 1652 MPa and 22.2%, respectively. Compared with the alloy without the graphite powder addition, the compressive strength and strain are improved by 37.7% and 62.1%, respectively. The wear resistance of the alloys is improved through the addition of graphite powder and the wear rate decreases from 5.062 to 2.125 x 10(-4) mm(3)<middle dot>N-1<middle dot>m(-1) as the content of graphite powder increases from 0 to 0.9 mass%.
引用
收藏
页数:13
相关论文
共 34 条
  • [1] Dry-Sliding Tribological Properties of TiAl/Ti2AlC Composites
    Cheng, Jun
    Li, Fei
    Fu, Licai
    Qiao, Zhuhui
    Yang, Jun
    Liu, Weimin
    [J]. TRIBOLOGY LETTERS, 2014, 53 (02) : 457 - 467
  • [2] Design of novel β-solidifying TiAl alloys with adjustable β/B2-phase fraction and excellent hot-workability
    Clemens, Helmut
    Wallgram, Wilfried
    Kremmer, Sascha
    Guether, Volker
    Otto, Andreas
    Bartels, Arno
    [J]. ADVANCED ENGINEERING MATERIALS, 2008, 10 (08) : 707 - 713
  • [3] Microstructure and Nanohardness of Ti-48Al-2Cr Alloy Solidified under High Pressure
    Dong, Duo
    Liu, Li
    Zhu, Dongdong
    Liu, Yang
    Wang, Ye
    Wang, Xiaohong
    Wei, Zunjie
    [J]. APPLIED SCIENCES-BASEL, 2020, 10 (15):
  • [4] The effects of the formation of a multi-scale reinforcing phase on the microstructure evolution and mechanical properties of a Ti2AlC/TiAl alloy
    Fang, Hongze
    Wang, Shu
    Chen, Ruirun
    Xu, Qin
    Yan, Yongda
    Su, Yanqing
    Guo, Jingjie
    [J]. NANOSCALE, 2021, 13 (29) : 12565 - 12576
  • [5] Effects of Tantalum on Microstructure Evolution and Mechanical Properties of High-Nb TiAl Alloys Reinforced by Ti2AlC
    Fang, Hongze
    Chen, Ruirun
    Yang, Yong
    Su, Yanqing
    Ding, Hongsheng
    Guo, Jingjie
    [J]. RESEARCH, 2019, 2019
  • [6] Effect of Ta element on microstructure formation and mechanical properties of high-Nb TiAl alloys
    Fang, Hongze
    Chen, Ruirun
    Chen, Xiaoyu
    Yang, Yong
    Su, Yanqing
    Ding, Hongsheng
    Guo, Jingjie
    [J]. INTERMETALLICS, 2019, 104 : 43 - 51
  • [7] Electron beam melted TiC/high Nb?TiAl nanocomposite: Microstructure and mechanical property
    Gao, B.
    Peng, H.
    Liang, Y.
    Lin, J.
    Chen, B.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 811
  • [8] Microstructural configuration and compressive deformation behavior of a TiAl composite reinforced by Mn and in situ Ti2AlC particles
    Gao, Yun-lei
    Kou, Shu-qing
    Dai, Jun-nan
    Wang, Zhi-fa
    Shu, Shi-li
    Zhang, Shuang
    Qiu, Feng
    Jiang, Qi-chuan
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 823 (823):
  • [9] Effects of degree of deformation on the microstructure, mechanical properties and texture of hybrid-reinforced titanium matrix composites
    Guo, Xianglong
    Wang, Liqiang
    Wang, Minmin
    Qin, Jining
    Zhang, Di
    Lu, Weijie
    [J]. ACTA MATERIALIA, 2012, 60 (6-7) : 2656 - 2667
  • [10] Wear mechanisms analysis for turning Ti-6Al-4V-towards the development of suitable tool coatings
    Jaffery, Syed H. Imran
    Mativenga, Paul T.
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2012, 58 (5-8) : 479 - 493