Effect of Zr Treatment on Inclusion and Solidification Microstructure in Ti Deoxidized Low Carbon Microalloyed Steel

被引:5
|
作者
Yang, Yongkun [1 ]
Wang, Yang [1 ]
Zhu, Jiayu [1 ]
Li, Xiaoming [1 ]
Zhan, Dongping [2 ]
机构
[1] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710055, Peoples R China
[2] Northeastern Univ, Sch Met, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
ACICULAR FERRITE NUCLEATION; IN-SITU OBSERVATION; MECHANICAL-PROPERTIES; OXIDE PARTICLES; COOLING PROCESS; ALLOY; EVOLUTION; DEFORMATION; DEOXIDATION; BEHAVIOR;
D O I
10.1007/s11837-023-05908-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Inclusion-induced acicular ferrite (AF) is a preferred microstructure that could refine grains and improve strength and toughness. As a prerequisite, the effective inclusions generated by the optimal range of Zr mass fraction are essential for refining inclusion size and obtaining AF in Ti deoxidized low-carbon microalloyed steel. Scanning electron microscopy, electron probe micro-analysis, and electron backscattered diffraction were used to systematically investigate the effect of Zr treatment on the inclusion and solidification microstructure. The mechanisms of AF nucleation induced by different types of effective inclusions were also revealed. The results show that when the Zr mass fraction is 0.0020%, the inclusion size is refined, the effective inclusions are TiN and Ti2ZrO6, the AF volume fraction and HAGB proportion reach the maximum value, and the effective grain size reaches the minimum value. The low lattice mismatch is the main mechanism of AF nucleation induced by TiO, TiN, and TiN containing composite inclusions. AF nucleation induced by Ti2O3, Ti2ZrO6, and other oxides is mainly the MDZ mechanism. Considering the inclusion characteristics and solidification microstructure, the optimal control range of Zr mass fraction in Ti deoxidized low-carbon microalloyed steel is 0.0020-0.0046%.
引用
收藏
页码:2841 / 2852
页数:12
相关论文
共 50 条
  • [21] Effect of Zr content on strain-induced precipitation behavior of Ti-Zr microalloyed low-carbon steel
    Luo, Hanyu
    Xiong, Xuegang
    Lai, Yiyue
    Cao, Jianchun
    Yang, Lisheng
    Zhang, Jinchang
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2025, 116 (02) : 130 - 140
  • [22] Characterization of Microstructure and Non-metallic Inclusions in Zr-Al Deoxidized Low Carbon Steel
    Jiang, Min
    Hu, Zhiyong
    Wang, Xinhua
    Pak, Jong-Jin
    ISIJ INTERNATIONAL, 2013, 53 (08) : 1386 - 1391
  • [23] Effect of microstructure on low-temperature toughness of a low carbon Nb-V-Ti microalloyed pipeline steel
    Wang, Bingxin
    Lian, Jingbao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 592 : 50 - 56
  • [24] Effect of Zr on microstructure evolution of Ti-Mo composite microalloyed steel during rolling
    Zhang, JinChang
    Zhang, FanLin
    Luo, HanYu
    Cao, JianChun
    Yang, LiSheng
    Xu, ChaoYong
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2024,
  • [25] Effect of Ti de-oxidation on solidification and post-solidification microstructure in low carbon high manganese steel
    Kikuchi, Naoki
    Nabeshima, Seiji
    Kishimoto, Yasuo
    Iviatsushita, Taishi
    Sridhar, Seetharaman
    ISIJ INTERNATIONAL, 2007, 47 (09) : 1255 - 1264
  • [26] Effect of Cooling Rate on Phase Transformation Kinetics and Microstructure of Nb–Ti Microalloyed Low Carbon HSLA Steel
    Rishabh Bharadwaj
    Aditya Sarkar
    Bhushan Rakshe
    Metallography, Microstructure, and Analysis, 2022, 11 : 661 - 672
  • [27] Formation of Non-Metallic Inclusion and Acicular Ferrite in Ti-Zr Deoxidized Steel
    Yang, Yongkun
    Zhan, Dongping
    Lei, Hong
    Qiu, Guoxing
    Jiang, Zhouhua
    Zhang, Huishu
    ISIJ INTERNATIONAL, 2019, 59 (09) : 1545 - 1551
  • [28] Influence of Oxide Particles and Residual Elements on Microstructure and Toughness in the Heat-Affected Zone of Low-Carbon Steel Deoxidized with Ti and Zr
    Suito, Hideaki
    Karasev, Andrey Vladimirovich
    Hamada, Masahiko
    Inoue, Ryo
    Nakajima, Keiji
    ISIJ INTERNATIONAL, 2011, 51 (07) : 1151 - 1162
  • [29] Effect of carbon and nitrogen content on microstructure of V-N-Ti microalloyed steel
    Wang, An-Dong
    Liu, Guo-Quan
    Yang, Cai-Fu
    Xiang, Song
    Han, Qing-Li
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2007, 28 (05): : 51 - 56
  • [30] Effect of Microstructure on Post-Rolling Induction Treatment in a Low C Ti-Mo Microalloyed Steel
    Larzabal, Gorka
    Isasti, Nerea
    Rodriguez-Ibabe, Jose M.
    Uranga, Pello
    METALS, 2018, 8 (09):