Prediction model for calculation of the limestone powder concrete carbonation depth

被引:6
作者
Radovic, Andrija [1 ]
Carevic, Vedran [2 ]
Marinkovic, Snezana [2 ]
Plavsic, Jasna [2 ]
Tesic, Ksenija [3 ]
机构
[1] Univ Pristina Kosovska Mitrovica, Fac Tech Sci, Knjaza Milosa 7, Kosovska Mitrovica 38220, Serbia
[2] Univ Belgrade, Fac Civil Engn, Bulevar Kralja Aleksandra 73, Belgrade 11000, Serbia
[3] Univ Zagreb, Fac Civil Engn, Fra Andrije Kacica Miosica 26, Zagreb 10000, Croatia
来源
JOURNAL OF BUILDING ENGINEERING | 2024年 / 86卷
关键词
Limestone powder concrete; Low clinker content; Carbonation resistance; Prediction model; LIFE-CYCLE ASSESSMENT; MECHANICAL-PROPERTIES; CEMENT REPLACEMENT; MIX DESIGN; DURABILITY; RESISTANCE; PORTLAND; PERMEABILITY; WATER;
D O I
10.1016/j.jobe.2024.108776
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The efficient way to mitigate the impact of the concrete industry on climate change is to reduce the clinker content in the concrete mix. Beside incorporating supplementary cementitious materials (SCMs), it is possible to use high filler content combined with concrete mix optimization. Limestone powder emerges as a promising filler mineral due to its availability and ready -to -use technology. In this work, the carbonation resistance of concrete with a high limestone powder content (45-65% of the powder phase) was experimentally tested. Test results showed that, with an optimized mix design featuring low water content and increased paste and plasticizer volume, concrete mixes satisfied high workability and strength demands for commonly applied strength classes. However, carbonation resistance remains a challenge. After two years in indoor natural conditions, carbonation depths were 8%, 28%, and 67% greater than referent Portland cement concrete for mixes with 47%, 58%, and 65% limestone powder content, respectively. Further analyses showed the inapplicability of the existing fib Model Code 2010 service life prediction model to limestone powder concrete. Based on a comprehensive database of experimental results, the modification of the fib prediction was proposed. A full probabilistic service life analysis revealed that for concrete with more than 20% limestone powder content and for both 50 and 100 -years' design service life, the currently prescribed concrete cover depths in European standards should be increased, depending on the carbonation exposure class.
引用
收藏
页数:15
相关论文
共 72 条
  • [1] [Anonymous], 2011, Methods of Testing Composition, Specifications and Conformity Criteria for Common Cements, DOI DOI 10.31030/1758792
  • [2] [Anonymous], 2006, Model Code for Service Life Design
  • [3] [Anonymous], 2004, Eurocode 2: Design of Concrete StructuresPart 1-1: General Rules and Rules for Buildings
  • [4] [Anonymous], 2009, EN 12350-2
  • [5] Estimates of self-compacting concrete 'potential' durability
    Assie, Stephan
    Escadeillas, Gilles
    Waller, Vincent
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2007, 21 (10) : 1909 - 1917
  • [6] EFFECTS OF CURING UPON CARBONATION OF CONCRETE
    BALAYSSAC, JP
    DETRICHE, CH
    GRANDET, J
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 1995, 9 (02) : 91 - 95
  • [7] Bertolini L., 2011, 12 DBMC INT C DURABI
  • [8] Bertolini L., 2007, P INT RILEM WORKSH I, P71
  • [9] By F.S., 2004, P 8 CANMET ACI INT C, P23
  • [10] Limit values of accelerated carbonation resistance to meet EC2 durability requirements
    Carevic, Vedran
    Ignjatovic, Ivan
    [J]. GRADEVNSKI MATERIJIALI I KONSTRUKCIJE-BUILDING MATERIALS AND STRUCTURES, 2022, 65 (01): : 1 - 6