共 50 条
Impact of alumina powder bed on hardness and fracture toughness in the sintering process of NiO-GDC-Bi2O3 composite prepared by sol-gel method
被引:0
|作者:
La Cruz, A. Ramirez-De
[1
]
Bocanegra-Bernal, M. H.
[1
]
Aguilar-Elguezabal, A.
[1
]
Reyes-Rojas, A.
[1
]
机构:
[1] Ctr Invest Mat Avanzados SC, Miguel Cervantes 120,Complejo Ind Chihuahua, Chihuahua 31136, Mexico
关键词:
NiO-GDC;
Bismuth oxide;
Sintering;
Fracture toughness;
Hardness;
WALL CARBON NANOTUBES;
MECHANICAL-PROPERTIES;
ELECTRICAL-PROPERTIES;
IONIC-CONDUCTIVITY;
SILICON-NITRIDE;
OXIDE;
MICROHARDNESS;
TEMPERATURE;
ELECTROLYTES;
CERAMICS;
D O I:
10.1007/s10971-024-06369-x
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
This study explores the sintering process of NiO-Ce0.9Gd0.1O1.95 + 35 wt% Bi2O3 ceramic composites synthesized via the sol-gel method, with a focus on the influence of an alumina powder bed during sintering. Uniaxially pressed disks were sintered at 890 degrees C for varying durations (0, 12, 24, and 61 h), with an additional disc sintered at 1450 degrees C for 6 h for comparative analysis. Sintering processes employed alumina as a powder bed, and subsequent evaluation included hardness and fracture toughness assessments. Relative densities of 53% and 48% were achieved for composites sintered at 890 and 1450 degrees C, respectively. The maximum hardness of 4.13 +/- 0.13 GPa was attained by the composite sintered at 890 degrees C for 61 h, while the highest fracture toughness (2.98 +/- 0.35 MPa.m(1/2)) was observed in the composite sintered at 1450 degrees C for 6 h. Evidence indicates that an interaction between Bi2O3 and the alumina bed occurred, adversely affecting the mechanical properties by promoting the depletion of Bi2O3, especially at elevated sintering temperatures. [GRAPHICS] .