Alumina-toughened zirconia nanocomposite: Aging effect on microstructural, optical, and mechanical properties

被引:6
|
作者
Piza, Mariana M. T. [1 ,4 ]
Bergamo, Edmara T. P. [1 ]
Campos, Tiago M. B. [1 ,2 ]
Carvalho, Laura F. [1 ]
Goulart, Celso A. [3 ]
Gutierres, Eliezer [1 ]
Lopes, Adolfo C. O. [1 ]
Jalkh, Ernesto B. Benalcazar [1 ]
Bonfante, Estevam A. [1 ]
机构
[1] Univ Sao Paulo, Bauru Sch Dent, Dept Prosthodont & Periodontol, Bauru, SP, Brazil
[2] Technol Inst Aeronaut, Dept Phys, Sao Jose Dos Campos, SP, Brazil
[3] Sao Paulo State Univ, Sch Sci & Engn, Tupa, SP, Brazil
[4] Univ Sao Paulo, Bauru Sch Dent FOB USP, Dept Prosthodont & Periodontol, 9-75 Octavio Pinheiro Brizolla, BR-17012901 Bauru, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zirconia; Ceramic Composites; Mechanical properties; Aging; LOW-TEMPERATURE DEGRADATION; COMPLICATION RATES; GRAIN-SIZE; CERAMICS; SURVIVAL; TRANSFORMATION; BEHAVIOR; FRACTURE; PHASE; ABUTMENTS;
D O I
10.1016/j.dental.2023.09.005
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To process an alumina-toughened zirconia (ATZ) nanocomposite and to characterize its crystalline phases, microstructure, residual stress, mechanical and optical properties before and after two different artificial aging methodologies. Methods: Disc-shaped specimens were obtained through uniaxial pressing of a commercial ATZ powder comprised of 80%ZrO2 / 20%Al2O3, with a particle size of 50 nm and 150 nm, respectively. Sintering was performed at 1500 degrees C for 2 h. Groups were established according to the aging protocol as immediate (ATZ-I) and aged either in autoclave (ATZ-A) or hydrothermal reactor (ATZ-R) at 134 degrees C for 20 h at 2.2 bar. Crystalline phases and microstructure were assessed by X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. Residual stress was evaluated by Raman spectroscopy. Contrast Ratio (CR) and Translucency Parameter (TP) were calculated to characterize optical properties. Mechanical properties were analyzed through Vickers microhardness, fracture toughness, and biaxial flexural strength test.Results: XRD spectra of both aging protocols revealed the presence of monoclinic zirconia (20-31%), where higher phase transformation was observed after aging in hydrothermal reactor. Optical properties evaluation demonstrated high opacity (CR: 0.99) and masking ability (TP: 0.26), with no significant differences after aging. Raman spectroscopy evidenced the presence of residual compressive stresses in the aged groups, being significantly higher for ATZ-R (-215.2 MPa). As-sintered specimens revealed hardness of-12.3 GPa and fracture toughness of-1.9 MPa.m1/2. Characteristic strength was 740 MPa for ATZ-I, 804 MPa for ATZ-A, and 879 MPa for ATZ-R, with significant differences between groups. Weibull modulus ranged from 16.5 to 18.8. All groups demonstrated high reliability up to 500 MPa stress missions (99-100%), with no significant differences after aging.Significance: The experimental ATZ nanocomposite presented high opacity and a high Weibull modulus. While aging created internal compressive stress responsible for an increase in characteristic strength, the nano-composite was susceptible to hydrothermal degradation. Further studies are required to evaluate its degradation kinetics at low temperatures.
引用
收藏
页码:1022 / 1031
页数:10
相关论文
共 50 条
  • [21] Effect of PrAlO3 on Mechanical Properties of Zirconia Toughened Alumina Bioceramics After Hydrothermal Aging
    Li W.
    Bai M.
    Bai M.
    Kuei Suan Jen Hsueh Pao/Journal of the Chinese Ceramic Society, 2023, 51 (03): : 721 - 729
  • [22] Effect of inclusion size on mechanical properties of alumina toughened cubic zirconia
    Mirosław M. Bućko
    Waldemar Pyda
    Journal of Materials Science, 2005, 40 : 5191 - 5198
  • [23] Effect of inclusion size on mechanical properties of alumina toughened cubic zirconia
    Bucko, MM
    Pyda, W
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (19) : 5191 - 5198
  • [24] Influence of In-Situ Platelet Reinforcement on the Properties of Injection Moulded Alumina-Toughened Zirconia
    Kern, F.
    Gadow, R.
    JOURNAL OF CERAMIC SCIENCE AND TECHNOLOGY, 2011, 2 (01): : 47 - 53
  • [25] Low Temperature Degradation of Alumina-toughened Zirconia in Artificial Saliva
    赵永旗
    JIANG Li
    LIAO Yunmao
    WANG Chuanyong
    LU Junjun
    ZHANG Jingchao
    李伟
    Journal of Wuhan University of Technology(Materials Science), 2013, 28 (04) : 844 - 848
  • [26] Low Temperature Degradation of Alumina-toughened Zirconia in Artificial Saliva
    赵永旗
    JIANG Li
    LIAO Yunmao
    WANG Chuanyong
    LU Junjun
    ZHANG Jingchao
    李伟
    Journal of Wuhan University of Technology(Materials Science Edition), 2013, 28 (04) : 844 - 848
  • [27] Mechanical evaluation of DIW-printed carbon nanofibers- alumina-toughened zirconia composites
    dos Santos, Vivian Ines
    Ferey, Aziliz
    Chevalier, Eva
    Fredel, Marcio Celso
    Henriques, Bruno
    Gremillard, Laurent
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (15)
  • [28] Microstructure and Mechanical Properties of Alumina Toughened Zirconia (ATZ)
    Maji, Ambarish
    Choubey, Gautam
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (02) : 7457 - 7465
  • [29] High density polyethylene composites containing alumina-toughened zirconia particles: Mechanical and tribological behavior
    Di Maro, M.
    Duraccio, D.
    Malucelli, G.
    Faga, M. G.
    COMPOSITES PART B-ENGINEERING, 2021, 217
  • [30] Nanomechanical and microstructural characterization of a zirconia-toughened alumina composite after aging
    Lopes, A. C. O.
    Coelho, P. G.
    Witek, L.
    Benalcazar Jalkh, E. B.
    Genova, L. A.
    Monteiro, K. N.
    Cesar, P. F.
    Lisboa Filho, P. N.
    Bergamo, E. T. P.
    Ramalho, I. S.
    Bonfante, E. A.
    CERAMICS INTERNATIONAL, 2019, 45 (07) : 8840 - 8846