Alumina-toughened zirconia nanocomposite: Aging effect on microstructural, optical, and mechanical properties

被引:6
|
作者
Piza, Mariana M. T. [1 ,4 ]
Bergamo, Edmara T. P. [1 ]
Campos, Tiago M. B. [1 ,2 ]
Carvalho, Laura F. [1 ]
Goulart, Celso A. [3 ]
Gutierres, Eliezer [1 ]
Lopes, Adolfo C. O. [1 ]
Jalkh, Ernesto B. Benalcazar [1 ]
Bonfante, Estevam A. [1 ]
机构
[1] Univ Sao Paulo, Bauru Sch Dent, Dept Prosthodont & Periodontol, Bauru, SP, Brazil
[2] Technol Inst Aeronaut, Dept Phys, Sao Jose Dos Campos, SP, Brazil
[3] Sao Paulo State Univ, Sch Sci & Engn, Tupa, SP, Brazil
[4] Univ Sao Paulo, Bauru Sch Dent FOB USP, Dept Prosthodont & Periodontol, 9-75 Octavio Pinheiro Brizolla, BR-17012901 Bauru, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zirconia; Ceramic Composites; Mechanical properties; Aging; LOW-TEMPERATURE DEGRADATION; COMPLICATION RATES; GRAIN-SIZE; CERAMICS; SURVIVAL; TRANSFORMATION; BEHAVIOR; FRACTURE; PHASE; ABUTMENTS;
D O I
10.1016/j.dental.2023.09.005
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To process an alumina-toughened zirconia (ATZ) nanocomposite and to characterize its crystalline phases, microstructure, residual stress, mechanical and optical properties before and after two different artificial aging methodologies. Methods: Disc-shaped specimens were obtained through uniaxial pressing of a commercial ATZ powder comprised of 80%ZrO2 / 20%Al2O3, with a particle size of 50 nm and 150 nm, respectively. Sintering was performed at 1500 degrees C for 2 h. Groups were established according to the aging protocol as immediate (ATZ-I) and aged either in autoclave (ATZ-A) or hydrothermal reactor (ATZ-R) at 134 degrees C for 20 h at 2.2 bar. Crystalline phases and microstructure were assessed by X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. Residual stress was evaluated by Raman spectroscopy. Contrast Ratio (CR) and Translucency Parameter (TP) were calculated to characterize optical properties. Mechanical properties were analyzed through Vickers microhardness, fracture toughness, and biaxial flexural strength test.Results: XRD spectra of both aging protocols revealed the presence of monoclinic zirconia (20-31%), where higher phase transformation was observed after aging in hydrothermal reactor. Optical properties evaluation demonstrated high opacity (CR: 0.99) and masking ability (TP: 0.26), with no significant differences after aging. Raman spectroscopy evidenced the presence of residual compressive stresses in the aged groups, being significantly higher for ATZ-R (-215.2 MPa). As-sintered specimens revealed hardness of-12.3 GPa and fracture toughness of-1.9 MPa.m1/2. Characteristic strength was 740 MPa for ATZ-I, 804 MPa for ATZ-A, and 879 MPa for ATZ-R, with significant differences between groups. Weibull modulus ranged from 16.5 to 18.8. All groups demonstrated high reliability up to 500 MPa stress missions (99-100%), with no significant differences after aging.Significance: The experimental ATZ nanocomposite presented high opacity and a high Weibull modulus. While aging created internal compressive stress responsible for an increase in characteristic strength, the nano-composite was susceptible to hydrothermal degradation. Further studies are required to evaluate its degradation kinetics at low temperatures.
引用
收藏
页码:1022 / 1031
页数:10
相关论文
共 50 条
  • [11] In vitro reaction of human osteoblasts on alumina-toughened zirconia
    Kohal, Ralf J.
    Baechle, Maria
    Han, Jung S.
    Hueren, Dennis
    Huebner, Ute
    Butz, Frank
    CLINICAL ORAL IMPLANTS RESEARCH, 2009, 20 (11) : 1265 - 1271
  • [12] MECHANICAL-PROPERTIES OF ZIRCONIA TOUGHENED ALUMINA
    SCHIOLER, LJ
    KATZ, RN
    BROG, T
    TIEN, TY
    AMERICAN CERAMIC SOCIETY BULLETIN, 1984, 63 (12): : 1478 - 1478
  • [13] Shear bond strengths between alumina-toughened zirconia cores and veneering ceramics and their susceptibility to aging
    Zhao, Yong-Qi
    Jiang, Li
    Zhang, Jing-Chao
    Liao, Yun-Mao
    Lu, Jun-Jun
    Li, Wei
    ASIAN PACIFIC JOURNAL OF TROPICAL MEDICINE, 2012, 5 (05) : 402 - 405
  • [14] Characterization of a hydrothermally aged experimental alumina-toughened zirconia composite
    Carvalho, Laura F.
    Bergamo, Edmara T. P.
    Campos, Tiago M. B.
    Fermino, Elisa S.
    Alves, Larissa M. M.
    Benalcazar-Jalkh, Ernesto B.
    Sousa, Edisa O.
    Coelho, Paulo G.
    Witek, Lukasz
    Tebcherani, Sergio M.
    Gierthmuehlen, Petra C.
    Thim, Gilmar Patrocinio
    Yamaguchi, Satoshi
    Carvalho, Alexandre M.
    Bonfante, Estevam A.
    DENTAL MATERIALS, 2024, 40 (09) : 1464 - 1476
  • [15] The Influence of Silicon Dioxide on the Stability of the Phase Composition and Mechanical Properties of Alumina-Toughened Zirconia-Based Ceramics
    A. A. Dmitrievskii
    A. O. Zhigachev
    D. G. Zhigacheva
    V. V. Rodaev
    Technical Physics, 2020, 65 : 2016 - 2025
  • [16] Shear bond strengths between alumina-toughened zirconia cores and veneering ceramics and their susceptibility to aging
    Yong-Qi Zhao
    Li Jiang
    Jing-Chao Zhang
    Yun-Mao Liao
    Jun-Jun Lu
    Wei Li
    Asian Pacific Journal of Tropical Medicine, 2012, (05) : 402 - 405
  • [17] Low temperature degradation of alumina-toughened zirconia in artificial saliva
    Zhao Yongqi
    Jiang Li
    Liao Yunmao
    Wang Chuanyong
    Lu Junjun
    Zhang Jingchao
    Li Wei
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2013, 28 (04): : 844 - 848
  • [18] The Influence of Silicon Dioxide on the Stability of the Phase Composition and Mechanical Properties of Alumina-Toughened Zirconia-Based Ceramics
    Dmitrievskii, A. A.
    Zhigachev, A. O.
    Zhigacheva, D. G.
    Rodaev, V. V.
    TECHNICAL PHYSICS, 2020, 65 (12) : 2016 - 2025
  • [19] Low temperature degradation of alumina-toughened zirconia in artificial saliva
    Yongqi Zhao
    Li Jiang
    Yunmao Liao
    Chuanyong Wang
    Junjun Lu
    Jingchao Zhang
    Wei Li
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2013, 28 : 844 - 848
  • [20] Thermal history of alumina-toughened ionic conductive zirconia ceramics
    Yuzaki, A
    Kishimoto, A
    Nakamura, Y
    SOLID STATE IONICS, 1998, 109 (3-4) : 273 - 277