Alumina-toughened zirconia nanocomposite: Aging effect on microstructural, optical, and mechanical properties

被引:6
作者
Piza, Mariana M. T. [1 ,4 ]
Bergamo, Edmara T. P. [1 ]
Campos, Tiago M. B. [1 ,2 ]
Carvalho, Laura F. [1 ]
Goulart, Celso A. [3 ]
Gutierres, Eliezer [1 ]
Lopes, Adolfo C. O. [1 ]
Jalkh, Ernesto B. Benalcazar [1 ]
Bonfante, Estevam A. [1 ]
机构
[1] Univ Sao Paulo, Bauru Sch Dent, Dept Prosthodont & Periodontol, Bauru, SP, Brazil
[2] Technol Inst Aeronaut, Dept Phys, Sao Jose Dos Campos, SP, Brazil
[3] Sao Paulo State Univ, Sch Sci & Engn, Tupa, SP, Brazil
[4] Univ Sao Paulo, Bauru Sch Dent FOB USP, Dept Prosthodont & Periodontol, 9-75 Octavio Pinheiro Brizolla, BR-17012901 Bauru, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Zirconia; Ceramic Composites; Mechanical properties; Aging; LOW-TEMPERATURE DEGRADATION; COMPLICATION RATES; GRAIN-SIZE; CERAMICS; SURVIVAL; TRANSFORMATION; BEHAVIOR; FRACTURE; PHASE; ABUTMENTS;
D O I
10.1016/j.dental.2023.09.005
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To process an alumina-toughened zirconia (ATZ) nanocomposite and to characterize its crystalline phases, microstructure, residual stress, mechanical and optical properties before and after two different artificial aging methodologies. Methods: Disc-shaped specimens were obtained through uniaxial pressing of a commercial ATZ powder comprised of 80%ZrO2 / 20%Al2O3, with a particle size of 50 nm and 150 nm, respectively. Sintering was performed at 1500 degrees C for 2 h. Groups were established according to the aging protocol as immediate (ATZ-I) and aged either in autoclave (ATZ-A) or hydrothermal reactor (ATZ-R) at 134 degrees C for 20 h at 2.2 bar. Crystalline phases and microstructure were assessed by X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. Residual stress was evaluated by Raman spectroscopy. Contrast Ratio (CR) and Translucency Parameter (TP) were calculated to characterize optical properties. Mechanical properties were analyzed through Vickers microhardness, fracture toughness, and biaxial flexural strength test.Results: XRD spectra of both aging protocols revealed the presence of monoclinic zirconia (20-31%), where higher phase transformation was observed after aging in hydrothermal reactor. Optical properties evaluation demonstrated high opacity (CR: 0.99) and masking ability (TP: 0.26), with no significant differences after aging. Raman spectroscopy evidenced the presence of residual compressive stresses in the aged groups, being significantly higher for ATZ-R (-215.2 MPa). As-sintered specimens revealed hardness of-12.3 GPa and fracture toughness of-1.9 MPa.m1/2. Characteristic strength was 740 MPa for ATZ-I, 804 MPa for ATZ-A, and 879 MPa for ATZ-R, with significant differences between groups. Weibull modulus ranged from 16.5 to 18.8. All groups demonstrated high reliability up to 500 MPa stress missions (99-100%), with no significant differences after aging.Significance: The experimental ATZ nanocomposite presented high opacity and a high Weibull modulus. While aging created internal compressive stress responsible for an increase in characteristic strength, the nano-composite was susceptible to hydrothermal degradation. Further studies are required to evaluate its degradation kinetics at low temperatures.
引用
收藏
页码:1022 / 1031
页数:10
相关论文
共 52 条
  • [1] Effects of sintering additives on the densification and properties of aluminatoughened zirconia ceramic composites
    Abbas, M. K. G.
    Ramesh, S.
    Lee, K. Y. Sara
    Wong, Y. H.
    Ganesan, P.
    Ramesh, S.
    Alengaram, U. Johnson
    Teng, W. D.
    Purbolaksono, J.
    [J]. CERAMICS INTERNATIONAL, 2020, 46 (17) : 27539 - 27549
  • [2] [Anonymous], 2008, ISO:13356
  • [3] GRAIN-SIZE-DEPENDENT TRANSFORMATION BEHAVIOR IN POLYCRYSTALLINE TETRAGONAL ZIRCONIA
    BECHER, PF
    SWAIN, MV
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (03) : 493 - 502
  • [4] The breakdown of the Weibull behavior in dental zirconias
    Belli, Renan
    Lohbauer, Ulrich
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2021, 104 (09) : 4819 - 4828
  • [5] Alumina-toughened zirconia for dental applications: Physicochemical, mechanical, optical, and residual stress characterization after artificial aging
    Bergamo, Edmara T. P.
    Cardoso, Karina B.
    Lino, Lucas F. O.
    Campos, Tiago M. B.
    Monteiro, Kelli N.
    Cesar, Paulo F.
    Genova, Luis A.
    Thim, Gilmar P.
    Coelho, Paulo G.
    Bonfante, Estevam A.
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2021, 109 (08) : 1135 - 1144
  • [6] Mechanical behavior and microstructural characterization of different zirconia polycrystals in different thicknesses
    Calvache Arcila, Laura Viviana
    Ramos, Nathalia de Carvalho
    Bastos Campos, Tiago Moreira
    Dapieve, Kiara Serafini
    Valandro, Luiz Felipe
    de Melo, Renata Marques
    Bottino, Marco Antonio
    [J]. JOURNAL OF ADVANCED PROSTHODONTICS, 2021, 13 (06) : 385 - 395
  • [7] ADM guidance-Ceramics: Fracture toughness testing and method selection
    Cesar, Paulo Francisco
    Della Bona, Alvaro
    Scherrer, Susanne S.
    Tholey, Michael
    van Noort, Richard
    Vichi, Alessandro
    Kelly, Robert
    Lohbauer, Ulrich
    [J]. DENTAL MATERIALS, 2017, 33 (06) : 575 - 584
  • [8] Histologic and histomorphometric evaluation of new zirconia-based ceramic dental implants: A preclinical study in dogs
    Chacun, Doriane
    Lafon, Arnaud
    Courtois, Nicolas
    Reveron, Helen
    Chevalier, Jerome
    Margossian, Patrice
    Alves, Antoine
    Gritsch, Kerstin
    Grosgogeat, Brigitte
    [J]. DENTAL MATERIALS, 2021, 37 (09) : 1377 - 1389
  • [9] What future for zirconia as a biomaterial?
    Chevalier, J
    [J]. BIOMATERIALS, 2006, 27 (04) : 535 - 543
  • [10] Chevalier J, 1999, J AM CERAM SOC, V82, P2150