Atomic clusters induced rapid hardening behavior in an early stage of isothermal aging for a high-strength Al alloy produced by laser powder bed fusion additive manufacturing

被引:2
|
作者
Zhang, Han [1 ]
Dai, Donghua [1 ]
Guo, Meng [1 ]
Yang, Jiankai [1 ]
Liu, He [1 ]
Gu, Dongdong [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Jiangsu Prov Engn Lab Laser Addit Mfg High Perform, Yudao St 29, Nanjing 210016, Peoples R China
基金
中国国家自然科学基金;
关键词
MG-ZR ALLOYS; MECHANICAL-PROPERTIES; SOLUTE CLUSTERS; PRECIPITATION; SC; MICROSTRUCTURE; TEMPERATURE; EVOLUTION; KINETICS; SCANDIUM;
D O I
10.1063/5.0125303
中图分类号
O59 [应用物理学];
学科分类号
摘要
Due to the transient interaction between laser and powder and layer-by-layer rapid melting and solidification, laser additive manufacturing-fabricated metal components can exhibit unique microstructure evolution behaviors and strengthening mechanisms that are normally not available in traditional processes. In this work, a previously unreported rapid hardening behavior at the very early stage of isothermal aging for laser powder bed fusion-processed high-strength Al-5024 alloy was revealed. The microstructures and mechanical properties of specimens aged from 10 min to 120h were systematically analyzed. It showed that the specimens underwent two peak hardening processes during an isothermal aging at 325?. The mechanical properties of the specimens including microhardness, yield strength, and elastic modulus were significantly enhanced after an extremely short aging time of 10 min and then reached a secondary peak hardening at an aging time of 4h, where the yield strength of 450 +/- 10.3 and 463.2 +/- 13.2 MPa were obtained, respectively. The unusual aging responses were attributed to the formation and decomposition of Sc-rich clusters with a high number density of 2.7 x 10(23 )m(-3) and nano-size of 2.71 nm. These clusters were characterized by transmission electron microscopy analyses and further supported by differential scanning calorimetry measurements, where a significantly higher activation energy of 147.6 +/- 21.1 kJ/mol corresponding to the precipitation/coarsening process of Al-3(Sc,Zr) was measured for rapid hardening specimens. In addition, the relationship between the aging process, the evolution of nano-precipitates, and the mechanical properties was systematically demonstrated.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Laser Powder Bed Fusion of an Al-Mg-Sc-Zr Alloy: Manufacturing, Peak Hardening Response and Thermal Stability at Peak Hardness
    Mehta, Bharat
    Svanberg, Arvid
    Nyborg, Lars
    METALS, 2022, 12 (01)
  • [22] In-situ aging treatment by preheating to obtain high-strength ZK60 Mg alloy processed by laser powder bed fusion
    Liang, Jingwei
    Wu, Shibo
    Lei, Zhenglong
    Chen, Yanbin
    Zhang, Xinrui
    Li, Bingwei
    Jiang, Meng
    Chen, Yuan
    MATERIALS CHARACTERIZATION, 2022, 194
  • [23] A novel high-strength Al-Li alloy printed by laser powder bed fusion: Microstructural evolution and strengthenin mechanism
    Wang, Chen
    Wu, Shibo
    Lei, Zhenglong
    Zhang, Xinrui
    Fu, Weijie
    Li, Xudong
    Sun, Haoran
    He, Peng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 6520 - 6535
  • [24] Nanoparticle-Enabled Additive Manufacturing of High Strength 6061 Aluminum Alloy via Laser Powder Bed Fusion
    Zheng, Tianqi
    Ma, Changyu
    Killips, Alexander
    Li, Bingbing
    Li, Xiaochun
    MANUFACTURING LETTERS, 2024, 41 : 753 - 757
  • [25] Additive manufacturing of high-strength and ductile high entropy alloy CoCrFeNiW0.2 composites via laser powder bed fusion and post-annealing
    Ng C.K.
    Bai K.
    Wuu D.
    Lau K.B.
    Lee J.J.
    Cheong A.K.H.
    Wei F.
    Cheng B.
    Wang P.
    Tan D.C.C.
    Zhang Y.-W.
    Journal of Alloys and Compounds, 2022, 906
  • [26] Processability of high-strength aluminum 6182 series alloy via laser powder bed fusion (LPBF)
    Riener, Kirstin
    Pfalz, Tino
    Funcke, Florian
    Leichtfried, Gerhard
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 119 (7-8) : 4963 - 4977
  • [27] Microstructural Evolution of a High-Strength Zr-Ti-Modified 2139 Aluminum Alloy for Laser Powder Bed Fusion
    Larini, Federico
    Casati, Riccardo
    Marola, Silvia
    Vedani, Maurizio
    METALS, 2023, 13 (05)
  • [29] High-cycle fatigue induced twinning in CoCrFeNi high-entropy alloy processed by laser powder bed fusion additive manufacturing
    Chen, Yinan
    Li, Bo
    Chen, Bo
    Xuan, Fuzhen
    ADDITIVE MANUFACTURING, 2023, 61
  • [30] Excellent strength-ductility synergy in metastable high entropy alloy by laser powder bed additive manufacturing
    Agrawal, P.
    Thapliyal, S.
    Nene, S. S.
    Mishra, R. S.
    McWilliams, B. A.
    Cho, K. C.
    ADDITIVE MANUFACTURING, 2020, 32