Effect of Tungsten Carbide Additions on the Microstructure, Mechanical, and Tribological Properties of M2 High-Speed Steel Matrix Composites

被引:2
|
作者
Zhou, Zhenyu [1 ,2 ]
Luo, Cong [1 ,2 ]
Xiong, Yifan [1 ,2 ]
Xiong, Hanqing [3 ]
Li, Fengren [1 ,2 ]
机构
[1] Hunan Inst Sci & Technol, Sch Mech Engn, Yueyang 414006, Peoples R China
[2] Key Lab Intelligent Mfg & Serv Performance Optimiz, Yueyang 414006, Peoples R China
[3] Changsha Univ, Dept Mech & Elect Engn, Changsha 410083, Peoples R China
关键词
mechanical properties; microstructure; steel matrix composites; WC; Wear resistance; CEMENTED CARBIDES; WEAR BEHAVIOR; TEMPERATURE; EVOLUTION; ALLOYS;
D O I
10.1007/s11665-024-09218-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The dense WC-M2 high-speed steel matrix composites (WC-M2 HSS MMCs) with different WC content were prepared by mechanical alloying and vacuum sintering process. Tungsten Carbide (WC) with 0, 2, 5, 8, and 10 (by weight %) were dispersed in the matrix. The effects of WC content on the densification mechanism, phase composition, microstructure, fracture morphology, and mechanical and wear properties of the sintered composites were systematically investigated. The experimental results showed that at a vacuum sintering temperature of 1260 degrees C, the composite material specimens achieved near-full densification, with predominant phases being Martensitic, M7C3, M6C, M2C, MC, WC, alpha-Fe, and gamma-Fe. Reasonable WC addition has improved grain uniformity and reduced micro-defects, which enhanced the overall mechanical properties. With an increase in WC content, the hardness and relative density of the composites showed a gradual increase, whereas transverse rupture strength and impact toughness initially improved but subsequently decreased. The friction coefficient displayed an initial increase followed by a decrease, while the wear rate showed an opposite trend. The impact fracture morphology is dominated by the interfacial separation between the WC particle phase and the binder phase, supplemented by the plastic tearing of the binder phase. The impact toughness mainly depended on the fracture of the binder phase. During crack propagation, both intergranular and transgranular fractures exist, of which the intergranular fracture prevails and coarse grains are more prone to transgranular fracture. With 5 wt.% WC, the steel matrix composites obtained peak mechanical performance, with impact toughness, bending strength, and hardness measuring 13.2 J cm-2, 1584.3 MPa, and 780.9 HV, respectively, which also yielded the highest wear resistance.
引用
收藏
页码:2553 / 2566
页数:14
相关论文
共 50 条
  • [31] Influence of Tempering Time on the Microstructure and Mechanical Properties of AISI M42 High-Speed Steel
    Luo, Yi-Wa
    Guo, Han-Jie
    Sun, Xiao-Lin
    Guo, Jing
    Wang, Fei
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (12): : 5976 - 5986
  • [32] Microstructure and properties of modified Al-bearing high boron high-speed steel
    Zhang, Ya-guang
    Fu, Han-guang
    Ma, Sheng-qiang
    Lin, Jian
    Guo, Xing-ye
    Wang, Chang-an
    Lei, Yong-ping
    IRONMAKING & STEELMAKING, 2020, 47 (06) : 693 - 703
  • [33] Effect of cryogenic and electrolytic passivation treatment on wear resistance of M2 high-speed steel
    Chen, Zhi
    Zhang, Yangwei
    Yan, Xianguo
    Li, Jiale
    Li, Fan
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2023, 127 (5-6): : 3049 - 3060
  • [34] Effect of tungsten carbide additions on the microstructure and properties of hot-pressed alumina
    Acchar, W
    Cairos, CA
    Segadaes, AM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 406 (1-2): : 74 - 77
  • [35] Effect of heat treatment on microstructure and mechanical properties of ZrC particles reinforced tungsten-matrix composites
    Zhang, Taiquan
    Wang, Yujin
    Zhou, Yu
    Song, Guiming
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 512 (1-2): : 19 - 25
  • [36] Effect of Cryogenic Treatment on AISI M2 High Speed Steel: Metallurgical and Mechanical Characterization
    Gill, Simranpreet Singh
    Singh, Jagdev
    Singh, Rupinder
    Singh, Harpreet
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (07) : 1320 - 1326
  • [37] The Inclusion Characteristics and Mechanical Properties of M2 High-Speed Steel Treated with a Vacuum Carbon Deoxidation Process
    Dai, Yuheng
    Man, Tinghui
    Wang, Zhongliang
    Liu, Yu
    Bao, Yanping
    Wei, Xicheng
    METALS, 2024, 14 (10)
  • [38] Microstructure, mechanical and tribological properties of CoCrFeNiMn high entropy alloy matrix composites with addition of Cr3C2
    Guo, Zhiming
    Zhang, Aijun
    Han, Jiesheng
    Meng, Junhu
    TRIBOLOGY INTERNATIONAL, 2020, 151
  • [39] Effect of Mo and Tempering Treatment on the Microstructural Evolution and Mechanical Properties of M2 High-Speed Steel Prepared by Laser-Directed Energy Deposition
    Wang, Jiale
    Chen, Changjun
    Zhang, Min
    STEEL RESEARCH INTERNATIONAL, 2021, 92 (11)
  • [40] Optimisation of Thermochemical Treatment of M2 High-Speed Steel
    Chaus A.S.
    Sahul M.
    Sitkevich M.V.
    Kusý M.
    Defect and Diffusion Forum, 2022, 420 : 43 - 52