Effect of Tungsten Carbide Additions on the Microstructure, Mechanical, and Tribological Properties of M2 High-Speed Steel Matrix Composites

被引:3
作者
Zhou, Zhenyu [1 ,2 ]
Luo, Cong [1 ,2 ]
Xiong, Yifan [1 ,2 ]
Xiong, Hanqing [3 ]
Li, Fengren [1 ,2 ]
机构
[1] Hunan Inst Sci & Technol, Sch Mech Engn, Yueyang 414006, Peoples R China
[2] Key Lab Intelligent Mfg & Serv Performance Optimiz, Yueyang 414006, Peoples R China
[3] Changsha Univ, Dept Mech & Elect Engn, Changsha 410083, Peoples R China
关键词
mechanical properties; microstructure; steel matrix composites; WC; Wear resistance; CEMENTED CARBIDES; WEAR BEHAVIOR; TEMPERATURE; EVOLUTION; ALLOYS;
D O I
10.1007/s11665-024-09218-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The dense WC-M2 high-speed steel matrix composites (WC-M2 HSS MMCs) with different WC content were prepared by mechanical alloying and vacuum sintering process. Tungsten Carbide (WC) with 0, 2, 5, 8, and 10 (by weight %) were dispersed in the matrix. The effects of WC content on the densification mechanism, phase composition, microstructure, fracture morphology, and mechanical and wear properties of the sintered composites were systematically investigated. The experimental results showed that at a vacuum sintering temperature of 1260 degrees C, the composite material specimens achieved near-full densification, with predominant phases being Martensitic, M7C3, M6C, M2C, MC, WC, alpha-Fe, and gamma-Fe. Reasonable WC addition has improved grain uniformity and reduced micro-defects, which enhanced the overall mechanical properties. With an increase in WC content, the hardness and relative density of the composites showed a gradual increase, whereas transverse rupture strength and impact toughness initially improved but subsequently decreased. The friction coefficient displayed an initial increase followed by a decrease, while the wear rate showed an opposite trend. The impact fracture morphology is dominated by the interfacial separation between the WC particle phase and the binder phase, supplemented by the plastic tearing of the binder phase. The impact toughness mainly depended on the fracture of the binder phase. During crack propagation, both intergranular and transgranular fractures exist, of which the intergranular fracture prevails and coarse grains are more prone to transgranular fracture. With 5 wt.% WC, the steel matrix composites obtained peak mechanical performance, with impact toughness, bending strength, and hardness measuring 13.2 J cm-2, 1584.3 MPa, and 780.9 HV, respectively, which also yielded the highest wear resistance.
引用
收藏
页码:2553 / 2566
页数:14
相关论文
共 46 条
[41]   Influence of powder mixing processes and WC contents on microstructure, shrinkage behavior, and mechanical properties of WC-Si3N4 composites [J].
Yin, Chaohui ;
Wang, Zhenhua ;
Yuan, Juntang .
CERAMICS INTERNATIONAL, 2023, 49 (16) :26747-26758
[42]   Effect of the dissolution characteristic of tungsten carbide particles on microstructure and properties of Ni-WC/W2C reinforcement coating manufactured by TIG cladding [J].
Yuan, Jiong ;
Huang, Yiming ;
Wang, Lixin ;
Jia, Chenpeng ;
Zhang, Feng ;
Yang, Lijun .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 110
[43]   Effects of Ti(C,N) additions on the microstructure and properties of the carbon-free high speed steel reinforced by intermetallic compounds [J].
Yuan, Ziren ;
He, Yuehui ;
Xie, Fengwei ;
Kang, Xiyue .
INTERMETALLICS, 2023, 152
[44]  
Zeng WM, 2017, CERAM INT, V43, P167, DOI 10.1016/j.ceramint.2016.09.129
[45]   Effects of niobium addition on microstructure and properties of CPM121 powder metallurgy high-speed steel [J].
Zhang Qian-kun ;
Li Su-wang ;
Xiao Yi-feng ;
Wu Liang ;
Qian Jin-wen ;
Chen Ze-min ;
Shen Wei-jun ;
Lin Nan ;
He Yue-hui .
JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2021, 28 (04) :1206-1218
[46]   Direct fabrication of high-performance high speed steel products enhanced by LaB6 [J].
Zhang Qiankun ;
Jiang Yao ;
Shen Weijun ;
Zhang Huibin ;
He Yuehui ;
Lin Nan ;
Liu, C. T. ;
Huang Han ;
Huang Xiaolin .
MATERIALS & DESIGN, 2016, 112 :469-478