Study on the microstructures and tensile creep behaviors of extruded dilute Mg -Mn -Zn alloys

被引:2
|
作者
Chen, Jianhua [1 ,2 ]
Huang, Weiying [1 ,4 ]
Liu, Bing [2 ]
Nagaumi, Hiromi [3 ]
Yang, Xuyue [2 ]
机构
[1] Changsha Univ Sci & Technol, Sch Energy & Power Engn, Key Lab Efficient & Clean Energy Utilizat, Changsha 410114, Peoples R China
[2] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[3] Soochow Univ, Sch Iron & Steel, Suzhou 215100, Peoples R China
[4] Hunan 3T New Mat Co Ltd, Loudi 417000, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 25卷
基金
中国国家自然科学基金;
关键词
Magnesium alloys; Microstructure; Creep behavior; Dislocation; ALPHA-MN; MAGNESIUM; DEFORMATION; DUCTILITY; SR; PRECIPITATION; SLIP; RECRYSTALLIZATION; STRENGTH; TEXTURE;
D O I
10.1016/j.jmrt.2023.07.046
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, creep behaviors of dilute Mg-Mn-Zn alloys were investigated in extruded rods (ER) with bimodal grain microstructures and extruded sheets (ES) with homogeneous microstructures. Tensile creep tests were carried out at 423 K along the extrusion direction (ED) and transverse direction (TD). For brevity, the samples were named as ER-ED, ER-TD, ES-ED and ES-TD, respectively. All samples' creep is dominated by dislocation movement, and different types of dislocation slip are seen in the different samples under loading along each direction. For the ER sample, the creep mechanisms of the ER-ED sample were determined to be cross-slip accompanied by pyramidal slip. Differently, the creep of the ER-TD sample was dominated by basal slip and accompanied by grain boundary bulging, which induced the worst creep resistance. For the ES alloy, the creep mechanisms were pyramidal and cross-slip, but the cross-slip density of the ES-ED sample was higher. Accordingly, the creep test results indicated that the creep resistance was ranked in an order of ES-TD/ED > ER-ED >> ER-TD. Furthermore, bimodal grain microstructure accel-erates creep at a similar texture effect level, where grain boundary bulging was clearly observed, as well as the decreased KAM and increased fraction of M/HABs (middle-to-high angle boundaries). These typical softening characteristics might be responsible for weak-ening the ER-ED sample from the highest room-temperature yield strength to the inferior creep resistance to ES-TD/ED samples, meaning the thermal instability of this strong heterogeneous microstructure.(c) 2023 The Author(s). Published by Elsevier B.V.This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:5443 / 5456
页数:14
相关论文
共 50 条
  • [31] Microstructures and Tensile Properties of New Mg-0.9Zn-0.2Mn-0.5RE Alloys via Different Al Additions
    Fu, Li
    Zhang, Zhiqian
    Li, Xiaoqiang
    Jia, Zheng
    Lu, Lin
    Le, Qichi
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (10)
  • [32] Extruded Microstructures and Corrosion Properties of Biomedical Mg-6Zn-xGd Alloys
    Qi Wenjun
    Gong Xiaoyi
    Huang Zhenghua
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (10) : 2609 - 2614
  • [33] High-speed extrusion of dilute Mg-Zn-Ca-Mn alloys and its effect on microstructure, texture and mechanical properties
    Jiang, M. G.
    Xu, C.
    Nakata, T.
    Yan, H.
    Chen, R. S.
    Kamado, S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 678 : 329 - 338
  • [34] Role of Zn addition on the microstructure and tensile property in Mg-Mn-Nd alloys
    Zhao, Jun
    Xu, Jun
    Liu, Yang
    Wang, Qinghang
    Jiang, Bin
    Pan, Fusheng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 7964 - 7969
  • [35] Microstructures and tensile properties of as-extruded Mg-Sn binary alloys
    陈冬
    任玉平
    郭运
    裴文利
    赵宏达
    秦高梧
    TransactionsofNonferrousMetalsSocietyofChina, 2010, 20 (07) : 1321 - 1325
  • [36] In situ analysis of the tensile deformation mechanisms in extruded Mg-1Mn-1Nd (wt%)
    Boehlert, C. J.
    Chen, Z.
    Chakkedath, A.
    Gutierrez-Urrutia, I.
    Llorca, J.
    Bohlen, J.
    Yi, S.
    Letzig, D.
    Perez-Prado, M. T.
    PHILOSOPHICAL MAGAZINE, 2013, 93 (06) : 598 - 617
  • [37] Microstructures and Tensile Properties of Hot-extruded Mg-6Zn-xCe (x=0, 0.6, 1.0, 2.0) Alloys
    Yu, Heshuai
    Yang, Wenpeng
    Cui, Hongbao
    Guo, Xuefeng
    Wang, Ying
    Wu, Yali
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2019, 34 (01): : 150 - 155
  • [38] Effect of Mn content on the microstructure and mechanical properties of as-extruded Zn-0.2Mg-Mn (wt%) alloys
    Wang, Liqing
    Lou, Dongfang
    Ren, Yuping
    Qin, Gaowu
    Bai, Peikang
    Zhao, Zhanyong
    MATERIALS CHARACTERIZATION, 2022, 194
  • [39] Microstructures and mechanical properties of extruded Mg-1Mn-3.5Y and Mg-1Mn-1Y-2.5Nd alloys
    Fang Da-qing
    Jiang Zhong-hao
    Bi Guang-li
    Li Rong-guang
    Li Guang-yu
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 : S555 - S560
  • [40] Effect of Zn content on microstructure, mechanical properties and thermal conductivity of extruded Mg-Zn-Ca-Mn alloys
    Tang, Bei
    Fu, Jinlong
    Feng, Jingkai
    Zhong, Xiting
    Guo, Yangyang
    Wang, Haili
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2023, 30 (12) : 2411 - 2420