Microstructure evolution and precipitation behavior of Al-Mg-Si alloy during initial aging

被引:10
作者
Zheng, Ya-ya [1 ,3 ]
Luo, Bing-hui [2 ]
Xie, Wei [3 ]
Li, Wang [1 ]
机构
[1] Hunan Univ Humanities, Dept Mat Engn, Sci & Technol, Loudi 417000, Hunan, Peoples R China
[2] Cent South Univ, Coll Mat Sci & Engn, Changsha 410083, Peoples R China
[3] Changsha Univ Sci & Technol, Key Lab Safety Design & Reliabil Technol Engn Vehi, Changsha 410114, Peoples R China
关键词
Al-Mg-Si alloy; precipitation behavior; strengthening mechanism; strain field; beta; MECHANICAL-PROPERTIES; CORROSION BEHAVIOR; CU; SEGREGATION; COPPER;
D O I
10.1007/s41230-023-1113-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The microstructure evolution and precipitation behavior of Al-Mg-Si alloy during initial aging were studied using hardness testing, conductivity testing, differential scanning calorimetry (DSC), and high resolution transmission electron microscopy (HRTEM). The results show that the precipitation sequence of the Al-Mg-Si alloy during initial aging can be represented as: supersaturated solid solution -> spherical Mg/Si clusters -> needle-like Guinier Preston (GP) zone -> beta ''. Clusters are completely coherent with the Al matrix. The GP zone with relatively complete independent lattice parameters that differ slightly from the Al matrix parameters, is oriented along the direction of < 111 > Al and lying on {111}(Al) plane. The strength of the Al-Mg-Si alloy is greatly enhanced by the threedimensional strain field that exists between the beta '' phase and the two {200}(Al) planes. After aging at 170 degrees C for 6 h, the hardness reaches the peak of 127 HV and remains for a long time. At this stage, the electrical conductivity keeps relatively stable due to the formation of coherent precipitates (Mg/Si clusters/GP zones) and the reduction in solute atom concentration in the Al matrix. The severe coarsening and decreased number density of the beta '' phase during the over-aging stage result in a significant decrease in the hardness.
引用
收藏
页码:57 / 62
页数:6
相关论文
共 27 条
[1]   Formation and reversion of clusters during natural aging and subsequent artificial aging in an Al-Mg-Si alloy [J].
Aruga, Yasuhiro ;
Kozuka, Masaya ;
Takaki, Yasuo ;
Sato, Tatsuo .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 631 :86-96
[2]   First-principles calculation of interface binding strength and fracture performance of β′/Al interface in Al-Mg-Si-Cu alloy [J].
Chen, Bao ;
Zhang, Chuan-Hui ;
Jin, Ying .
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 830
[3]   First-principles study of the binding preferences and diffusion behaviors of solutes in vanadium alloys [J].
Deng, Lei ;
Zhang, Xingming ;
Tang, Jianfeng ;
Deng, Huiqiu ;
Xiao, Shifang ;
Hu, Wangyu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 660 :55-61
[4]   The structural and compositional evolution of precipitates in Al-Mg-Si-Cu alloy [J].
Ding, Lipeng ;
Jia, Zhihong ;
Nie, Jian-Feng ;
Weng, Yaoyao ;
Cao, Lingfei ;
Chen, Houwen ;
Wu, Xiaozhi ;
Liu, Qing .
ACTA MATERIALIA, 2018, 145 :437-450
[5]   Atomistic determination on stability, cluster and microstructures in terms of crystallographic and thermo-kinetic integration of Al-Mg-Si alloys [J].
Du, Jinglian ;
Zhang, Ang ;
Zhang, Yubing ;
Wang, Tianle ;
Xiong, Shoumei ;
Liu, Feng .
MATERIALS TODAY COMMUNICATIONS, 2020, 24
[6]   EFFECT OF REINFORCEMENT ON THE AGING RESPONSE OF CAST 6061 AL-AL2O3 PARTICULATE COMPOSITES [J].
DUTTA, I ;
ALLEN, SM ;
HAFLEY, JL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1991, 22 (11) :2553-2563
[7]   The precipitation sequence in Al-Mg-Si alloys [J].
Edwards, GA ;
Stiller, K ;
Dunlop, GL ;
Couper, MJ .
ACTA MATERIALIA, 1998, 46 (11) :3893-3904
[8]   Precipitation hardening processes in an Al-0.40%Mg-1.3%Si-0.25%Fe aluminum alloy [J].
Gupta, AK ;
Lloyd, DJ ;
Court, SA .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 301 (02) :140-146
[9]   Influence of Si Addition on Quenching Sensitivity and Formation of Nano-Precipitate in Al-Mg-Si Alloys [J].
Kim, JaeHwang ;
Hayashi, Minoru ;
Kobayashi, Equo ;
Sato, Tatsuo .
JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2016, 16 (02) :1814-1817
[10]   Effect of deformation temperature on precipitation, microstructural evolution, mechanical and corrosion behavior of 6082 Al alloy [J].
Kumar, Nikhil ;
Jayaganthan, R. ;
Brokmeier, Heinz-Guenter .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2017, 27 (03) :475-492