Ni as the promoter on hydrogen spillover for better hydrogenative regeneration on Pt/Y based catalysts

被引:26
作者
Ren, Kui [1 ]
Jia, Fuxian [1 ]
Zhang, Chengxi [1 ]
Xing, Enhui [1 ]
Li, Yongxiang [1 ]
机构
[1] Sinopec, Res Inst Petr Proc, State Key Lab Catalyt Mat & React Engn, Beijing 100083, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
Isobutane; Butene; Solid acid alkylation; Hydrogen spillover; Hydrogenative regeneration; HIGHLY DISPERSED NOBLE; ETHYLENE-GLYCOL; REDUCTIVE AMINATION; CARBON NANOTUBES; LOW-TEMPERATURE; X ZEOLITES; METAL; ADSORPTION; CO2; DEACTIVATION;
D O I
10.1016/j.fuel.2022.127047
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Hydrogenative regeneration of Pt/YA catalysts is vital to continuous operation of solid acid isobutane/butene alkylation. From the view of H2 activation, the mechanism of hydrogenative regeneration was investigated experimentally and theoretically. Herein with Pt/YA as reference, (Ni-Pt)/YA catalysts were prepared with almost identical cell parameter and different Ni/Pt contents by wet impregnation method following by several characterization methods, such as XPS, H2-TPR, H2-TPD, STEM-CS and Elemental mapping. Strong interactions between Ni and Pt were proven by XPS and H2-TPR. Moreover Ni can increase the capability of hydrogen spillover, which could be observed by H2-TPD, with the higher desorption temperature and more desorbed H2. DFT calculations revealed that hydrogen spillover is the rate determining step for the overall H2 activation over Pt/YA, and Ni as the hydrogen spillover promoter could couple with Pt to enhance the overall H2 activation because of almost 30% lower energy barrier for hydrogen spillover. With rather low Pt content, no obvious loss in lifetime in the 10 cycles of reaction-regeneration was observed over (5Ni-0.1Pt)/YA with rather stable product distribution.
引用
收藏
页数:9
相关论文
共 62 条
[1]   Explaining the Size Dependence in Platinum-Nanoparticle-Catalyzed Hydrogenation Reactions [J].
Bai, Licheng ;
Wang, Xin ;
Chen, Qiang ;
Ye, Yifan ;
Zheng, Haoquan ;
Guo, Jinghua ;
Yin, Yadong ;
Gao, Chuanbo .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2016, 55 (50) :15656-15661
[2]   Hydrogen production from ethylene glycol reforming catalyzed by Ni and Ni-Pt hydrotalcite-derived catalysts [J].
Cesar, Deborah V. ;
Santori, Gerardo F. ;
Pompeo, Francisco ;
Baldanza, Maria A. ;
Henriques, Cristiane A. ;
Lombardo, Eduardo ;
Schmal, Martin ;
Cornaglia, Laura ;
Nichio, Nora N. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (47) :22000-22008
[3]   Reductive amination of polypropylene glycol using Ni-CeO2@Al2O3 with high activity, selectivity and stability [J].
Chang, Hung-Yen ;
Lai, Guan-Hung ;
Lin, Chih-Yuan ;
Lee, Chun-Yu ;
Chia, Chih-Cheng ;
Hwang, Chuen-Lih ;
Chang, Huan-Ming ;
Tsai, De-Hao .
CATALYSIS COMMUNICATIONS, 2019, 127 :15-19
[4]   SPILLOVER IN HETEROGENEOUS CATALYSIS [J].
CONNER, WC ;
FALCONER, JL .
CHEMICAL REVIEWS, 1995, 95 (03) :759-788
[5]   AN ALL-ELECTRON NUMERICAL-METHOD FOR SOLVING THE LOCAL DENSITY FUNCTIONAL FOR POLYATOMIC-MOLECULES [J].
DELLEY, B .
JOURNAL OF CHEMICAL PHYSICS, 1990, 92 (01) :508-517
[6]   From molecules to solids with the DMol3 approach [J].
Delley, B .
JOURNAL OF CHEMICAL PHYSICS, 2000, 113 (18) :7756-7764
[7]   Effect of catalyst deactivation on the acid properties of zeolites used for isobutane/butene alkylation [J].
Diaz-Mendoza, FA ;
Pernett-Bolano, L ;
Cardona-Martinez, N .
THERMOCHIMICA ACTA, 1998, 312 (1-2) :47-61
[8]   Solvent-free oxidation of primary alcohols to aldehydes using Au-Pd/TiO2 catalysts [J].
Enache, DI ;
Edwards, JK ;
Landon, P ;
Solsona-Espriu, B ;
Carley, AF ;
Herzing, AA ;
Watanabe, M ;
Kiely, CJ ;
Knight, DW ;
Hutchings, GJ .
SCIENCE, 2006, 311 (5759) :362-365
[9]   Enhanced activity of bimetallic Pd-Ni nanoparticles on KIT-6 for production of hydrogen from dodecahydro-N-ethylcarbazole [J].
Feng, Zhaolu ;
Bai, Xuefeng .
FUEL, 2022, 329
[10]   Steam reforming of naphthalene/benzene with various types of Pt- and Ni-based catalysts for hydrogen production [J].
Furusawa, Takeshi ;
Saito, Katsuhiko ;
Kori, Yoshihiko ;
Miura, Yasutomo ;
Sato, Masahide ;
Suzuki, Noboru .
FUEL, 2013, 103 :111-121