Experimental research and numerical analysis of welding residual stress of butt welded joint of thick steel plate

被引:27
作者
Lu, Wen-Liang [1 ]
Sun, Jing-Long [2 ]
Su, Han [1 ]
Chen, Liang-Jiang [3 ]
Zhou, Yong-Zheng [3 ]
机构
[1] Beijing Jiaotong Univ, Sch Civil Engn, Beijing 100044, Peoples R China
[2] China Railway Shanghai Design Inst Grp Corp Ltd, Shanghai 200072, Peoples R China
[3] China Railway Econ & Planning Res Inst, Beijing 100038, Peoples R China
关键词
Steel bridge; Thick steel plate; Welding residual stress; X-ray diffraction method; Finite element analysis; CRACK;
D O I
10.1016/j.cscm.2023.e01991
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The thickness of steel plates used in the member has gradually increased to meet the load-bearing capacity requirements of long-span steel bridges. As the primary connection method of thick steel plate, welding will result in considerable welding residual stress with complex distribution. Large welding residual stress will significantly impact the performance of steel bridges. In this paper, the distribution of residual stress in welded thick steel plate is systematically studied, a specimen with a thickness of 80 mm was designed and fabricated, and the welding residual stress was measured by X-ray diffraction. The finite element model was established and verified by test results. Subsequently, the finite element calculation of the welding residual stress of steel plates with thicknesses of 20, 40, 60, 80, and 100 mm was carried out, and the distribution of surface residual stress and the influence of plate thickness on residual surface stress were studied; then the spatial evolution mechanism of welding residual stress was studied, and the distribution of residual stress inside steel plate and the influence of plate thickness on the distribution of residual stress were revealed. The results show that the surface and internal residual stresses of 20-100 mm thick plates have good symmetry on the paths perpendicular to the weld seam, and asymmetry only occurs in the weld seam and heat-affected zone where the stress fluctuates. On the paths perpendicular to the weld seam, the stress in the X direction transitions from the "M" shape distribution on the surface to the "pi" shape distribution inside for 20-40 mm thick plates, and the residual stress near the weld seam gradually changes from compressive to tensile; The distribution of stress in the X direction in the 80-100 mm thick plate has experienced the transition from "M" shape to "pi" shape to "M" shape, and the stress near the weld seam has experienced the transition from compressive to tensile to compressive. The stress change in the X direction of the 60 mm thick plate is between the above two cases. On the path of internal stress along the thickness, the maximum stress in the X direction is 310-400 MPa for 20-40 mm thick plates, which appears at about 1/2 plate thickness. The maximum stress in the X direction for 60-100 mm thick plates is 400-480 MPa, which appears at 0.2-0.3 times the thickness of the plate from the upper surface. The results could serve as a reference for welding residual stress analysis and guide optimization design of steel bridges made of thick steel plate.
引用
收藏
页数:21
相关论文
共 36 条
[1]   Neutron diffraction investigations on residual stresses contributing to the fatigue crack growth in ferritic steel tubular bridges [J].
Acevedo, C. ;
Evans, A. ;
Nussbaumer, A. .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2012, 95 :31-38
[2]   Welding Residual Stress Analysis and Fatigue Strength Assessment of Multi-Pass Dissimilar Material Welded Joint between Alloy 617 and 12Cr Steel [J].
Ahmad, Hafiz Waqar ;
Hwang, Jeong Ho ;
Lee, Ju Hwa ;
Bae, Dong Ho .
METALS, 2018, 8 (01)
[3]   Welding Residual Stress Effect in Fracture Toughness [J].
An, Gyubaek ;
Woo, Wanchuck ;
Park, Jeongung .
JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2019, 19 (04) :2323-2328
[4]   Residual stress distributions in arc, laser and electron-beam welds in 30 mm thick SA508 steel: A cross-process comparison [J].
Balakrishnan, J. ;
Vasileiou, A. N. ;
Francis, J. A. ;
Smith, M. C. ;
Roy, M. J. ;
Callaghan, M. D. ;
Irvine, N. M. .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2018, 162 :59-70
[5]   A study on mechanical and microstructure characteristics of the STS304L butt joints using hybrid CO2 laser-gas metal arc welding [J].
Bang, Hee Seon ;
Bang, Han Sur ;
Kim, You Chul ;
Oh, Ik Hyun .
MATERIALS & DESIGN, 2011, 32 (04) :2328-2333
[6]  
Banik S.D., 2021, J MATER PROCESS TECH, V289
[7]   Dissimilar weldments of P91 and Incoloy 800HT: Microstructure, mechanical properties, and residual stresses [J].
Bhanu, Vishwa ;
Pandey, Shailesh M. ;
Gupta, Ankur ;
Pandey, Chandan .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2022, 199
[8]   Dissimilar joining of the martensitic grade P91 and Incoloy 800HT alloy for AUSC boiler application: Microstructure, mechanical properties and residual stresses [J].
Bhanu, Vishwa ;
Pandey, Chandan ;
Gupta, Ankur .
CIRP JOURNAL OF MANUFACTURING SCIENCE AND TECHNOLOGY, 2022, 38 :560-580
[9]   Residual stresses and fracture mechanics analysis of a crack in welds of high strength steels [J].
Chang, Kyong-Ho ;
Lee, Chin-Hyung .
ENGINEERING FRACTURE MECHANICS, 2007, 74 (06) :980-994
[10]   Microstructure anomaly during welding and its influence on the mechanical properties of dissimilar weldments of P92 martensitic steel and AISI 304L austenitic stainless steel [J].
Dak, Gaurav ;
Pandey, Chandan .
JOURNAL OF MANUFACTURING PROCESSES, 2022, 80 :829-851