In-situ X-ray diffraction study of the oxidation behavior of arc-evaporated TiAlSiN coatings with low Al contents

被引:5
作者
Moritz, Yvonne [1 ,5 ]
Saringer, Christian [1 ,6 ]
Tkadletz, Michael [2 ]
Fian, Alexander [3 ]
Czettl, Christoph [4 ]
Pohler, Markus [4 ]
Schalk, Nina [1 ]
机构
[1] Univ Leoben, Christian Doppler Lab Adv Coated Cutting Tools, Dept Mat Sci, Franz Josef Str 18, A-8700 Leoben, Austria
[2] Univ Leoben, Dept Mat Sci, Franz Josef Str 18, A-8700 Leoben, Austria
[3] JOANNEUM Res Forsch Gesell, Inst Surface Technol & Photon, Franz Pichler Str 30, A-8160 Weiz, Austria
[4] CERATIZIT Austria GmbH, Metallwerk Plansee Str 71, A-6600 Reutte, Austria
[5] Allnex Austria GmbH, Bundesstr 175, A-8402 Werndorf, Austria
[6] AT & S Austria Technol & Syst Tech Aktiengesell, Fabriksgasse 13, A-8700 Leoben, Austria
关键词
PVD; TiAlSiN hard coatings; Oxidation; In-situ XRD; Rietveld; THIN-FILMS; PHOTOELECTRON-SPECTROSCOPY; MECHANICAL-PROPERTIES; THERMAL-STABILITY; BINDING-ENERGIES; HARD COATINGS; MICROSTRUCTURE; TRANSITION; RESISTANCE; DEPOSITION;
D O I
10.1016/j.surfcoat.2023.130161
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
TiAlSiN hard coatings are commonly known to exhibit a high oxidation resistance, however, the influence of a varying Al content on the oxidation mechanism has not yet been examined in detail. Thus, in this work, the temperature dependent phase composition of two powdered TiAlSiN coatings with low Al contents (Ti37Al2Si7N54 and Ti33Al6Si7N54) was evaluated by in-situ X-ray diffraction (XRD) in ambient air up to 1200 degrees C and subsequent Rietveld refinement complemented by differential scanning calorimetry measurements. The in-situ XRD experiments revealed the formation of metastable anatase TiO2 during oxidation for both TiAlSiN coatings, however, the maximum wt% of this phase was found to be doubled for the coating with higher Al content from 9 to 21 wt% at -1025 degrees C. Furthermore, the microstructure of the compact Ti33Al6Si7N54 coating oxidized at 950 and 1100 degrees C was investigated comprehensively by means of XRD, Raman spectroscopy, X-ray photoelectron spectroscopy and scanning electron microscopy. These microstructural investigations revealed the formation of a thin protective Al2O3 layer, which was broken by the growth of TiO2 grains after oxidizing at 950 degrees C, leading to fully enclosed Al2O3 grains within coarsened TiO2 grains at 1100 degrees C. The present work allows to close the literature gap concerning the changes in oxidation mechanism of TiAlSiN coatings when exclusively varying the Al content and further illuminates the microstructure of an oxidized TiAlSiN with low Al content in detail.
引用
收藏
页数:10
相关论文
共 56 条
  • [1] Phase Stability and Elasticity of TiAlN
    Abrikosov, Igor A.
    Knutsson, Axel
    Alling, Bjorn
    Tasnadi, Ferenc
    Lind, Hans
    Hultman, Lars
    Oden, Magnus
    [J]. MATERIALS, 2011, 4 (09) : 1599 - 1618
  • [2] [Anonymous], XRAY PHOTOELECTRON S
  • [3] [Anonymous], 2017, I.S. 1832:2017, Indexable Inserts for Cutting Tools,
  • [4] ELASTIC RECOIL DETECTION ANALYSIS WITH HEAVY-IONS
    ASSMANN, W
    HUBER, H
    STEINHAUSEN, C
    DOBLER, M
    GLUCKLER, H
    WEIDINGER, A
    [J]. NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1994, 89 (1-4) : 131 - 139
  • [5] Growth and characterization of TiAlN/CrAlN superlattices prepared by reactive direct current magnetron sputtering
    Barshilia, Harish C.
    Deepthi, B.
    Rajam, K. S.
    Bhatti, Kanwal Preet
    Chaudhary, Sujeet
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2009, 27 (01): : 29 - 36
  • [6] Berezhinsky LI, 2005, SEMICOND PHYS QUANT, V8, P37
  • [7] Characterization of nitride coatings by XPS
    Bertóti, I
    [J]. SURFACE & COATINGS TECHNOLOGY, 2002, 151 : 194 - 203
  • [8] Microstructure and mechanical properties of nanocomposite (Ti,Si,Al)N coatings
    Carvalho, S
    Rebouta, L
    Cavaleiro, A
    Rocha, LA
    Gomes, J
    Alves, E
    [J]. THIN SOLID FILMS, 2001, 398 : 391 - 396
  • [9] X-ray photoelectron spectroscopy analyses of titanium oxynitride films prepared by magnetron sputtering using air/Ar mixtures
    Chan, Mu-Hsuan
    Lu, Fu-Hsing
    [J]. THIN SOLID FILMS, 2009, 517 (17) : 5006 - 5009
  • [10] Microstructure, corrosion and tribological behaviors of TiAlSiN coatings deposited by cathodic arc plasma deposition
    Chang, Chi-Lung
    Lee, Jyh-Wei
    Tseng, Ming-Don
    [J]. THIN SOLID FILMS, 2009, 517 (17) : 5231 - 5236