Fatigue behavior of silicon nitride ceramics

被引:7
|
作者
Ye, C. C. [1 ,2 ]
Ru, H. Q. [2 ]
Chen, D. L. [3 ]
机构
[1] Weifang Univ, Sch Machinery & Automat, Weifang 261061, Shandong, Peoples R China
[2] Northeastern Univ, Inst Ceram & Powder Met, Sch Mat Sci & Engn, Key Lab Anisotropy & Texture Mat,Minist Educ, Shenyang 110819, Liaoning, Peoples R China
[3] Toronto Metropolitan Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Silicon nitride ceramics; Sintering additives; Compressive residual stresses; Fatigue life; MECHANICAL-PROPERTIES; THERMAL-CONDUCTIVITY; PHASE-TRANSFORMATION; FRACTURE-TOUGHNESS; RESIDUAL-STRESSES; SI3N4; CERAMICS; CRACK-GROWTH; MG; AL; MICROSTRUCTURE;
D O I
10.1016/j.ceramint.2023.06.095
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This work was aimed to identify the effects of sintering additives on the fatigue life of silicon nitride (Si3N4) ceramics sintered via hot pressing, focusing on the salient toughening mechanisms. The fatigue life and probability of survival of YMH samples using MgO and Y2O3 as sintering additives were observed to be higher than those of YAH samples using Al2O3 and Y2O3 as sintering additives. This was attributed to 1) the higher aspect ratio of the elongated & beta;-Si3N4 grains in the YMH sample which were formed via phase transformation from the initial & alpha;-Si3N4 powders during sintering, promoting a higher extent of crack deflection and crack bridging; 2) the larger compressive residual stresses existing in the YMH sample to suppress fatigue crack initiation and propagation; and 3) the presence of only amorphous (or glassy) phase at & beta;-Si3N4 grain boundaries stemming from the reaction of MgO-Y2O3 additives with the SiO2 layer on the & alpha;-Si3N4 powder surface during sintering, without the formation of an unfavorable crystalline & beta;& PRIME;-SiAlON layer in-between the & beta;-Si3N4 grains and amorphous phase. This further contributed to the increasing crack deflection via more readily debonding, thus enhancing the fatigue life of the YMH sample.
引用
收藏
页码:28405 / 28414
页数:10
相关论文
共 50 条
  • [21] Silicon nitride ceramics
    Petzow, G
    Herrmann, M
    HIGH PERFORMANCE NON-OXIDE CERAMICS II, 2002, 102 : 47 - 167
  • [22] COMPRESSION CREEP-BEHAVIOR OF SILICON-NITRIDE CERAMICS
    BIRCH, JM
    WILSHIRE, B
    JOURNAL OF MATERIALS SCIENCE, 1978, 13 (12) : 2627 - 2636
  • [23] Behavior of crack growth resistance in toughened silicon nitride ceramics
    Kawamoto, H
    Hiramatsu, K
    Takigawa, Y
    Okada, A
    Usami, H
    FRACTURE AND DUCTILE VS. BRITTLE BEHAVIOR-THEORY, MODELLING AND EXPERIMENT, 1999, 539 : 113 - 118
  • [24] Behavior of crack growth resistance in toughened silicon nitride ceramics
    Kawamoto, H.
    Hiramatsu, K.
    Takigawa, Y.
    Okada, A.
    Usami, H.
    Materials Research Society Symposium - Proceedings, 1999, 539 : 113 - 118
  • [25] Crack-healing and oxidation behavior of silicon nitride ceramics
    Houjou, K
    Ando, K
    Liu, SP
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (08) : 2329 - 2338
  • [26] Fracture behavior of silicon nitride ceramics subjected to hypervelocity impact
    Kawai, N.
    Tsurui, K.
    Shindo, D.
    Motoyashiki, Y.
    Sato, E.
    INTERNATIONAL JOURNAL OF IMPACT ENGINEERING, 2011, 38 (07) : 542 - 545
  • [27] Corrosion behavior of porous silicon nitride ceramics in different atmospheres
    Hou, Xinmei
    Wang, Enhui
    Li, Bin
    Chen, Junhong
    Chou, Kuo-Chih
    CERAMICS INTERNATIONAL, 2017, 43 (05) : 4344 - 4352
  • [28] Tribological behavior of silicon nitride-based ceramics - A review
    Subramaniam, Shankar
    Nithyaprakash, R.
    Abbas, G.
    Pramanik, A.
    Basak, Animesh Kumar
    JURNAL TRIBOLOGI, 2021, 29 : 57 - 71
  • [29] Deformation and relaxation behavior of silicon nitride ceramics with different microstructure
    Hvizdos, P.
    Dusza, J.
    Rudnayova, E.
    Ceramic Engineering and Science Proceedings, 1995, 16 (05): : 1135 - 1144
  • [30] EFFECTS OF CRACK SIZE ON FATIGUE BEHAVIOR IN SILICON-NITRIDE
    NIWA, T
    URASHIMA, K
    TAJIMA, Y
    WATANABE, M
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1991, 99 (04): : 296 - 299