Surface integrity of SLM manufactured meso-size gears in laser shock peening without coating

被引:13
|
作者
Pathak, Sunil [1 ]
Bohm, Marek [1 ,2 ]
Kaufman, Jan [1 ]
Kopecek, Jaromir [3 ]
Zulic, Sanin [1 ]
Stransky, Ondrej [1 ,4 ]
Shukla, Ashish [5 ]
Brajer, Jan [1 ]
Beranek, Libor [4 ]
Radhakrisnan, J. [6 ]
Rostohar, Danijela [7 ]
Mocek, Tomas [1 ]
机构
[1] Czech Acad Sci, Inst Phys, HiLASE Ctr, Prague, Czech Republic
[2] Czech Tech Univ, Fac Nucl Sci & Phys Engn, Prague, Czech Republic
[3] Czech Acad Sci, Inst Phys, Prague, Czech Republic
[4] Czech Tech Univ, Fac Mech Engn, Prague, Czech Republic
[5] Atlas Skilltech Univ, Navi Murnbai, Maharashtra, India
[6] Univ Politecn Madrid, ETS Ingenieros Ind, C Jose Gutierrez Abascal 2, Madrid 28006, Spain
[7] Coventry Univ, Inst Adv Mfg & Engn, Coventry CV6 5LZ, W Midlands, England
关键词
Laser shock peening; Meso; Gear; Surface quality; Residual stresses; Microstructure;
D O I
10.1016/j.jmapro.2022.12.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work aimed to improve the surface integrity of the selective laser melting manufacturing (SLM) manufactured 10 mm sized meso gears using the unconventional Laser Peening without Coating (LPwC) tech-nique. To accomplish LPwC on meso gears low energy in the range of 200 mJ to 1000 mJ at 10 Hz were applied underwater in the gear root and fillet gap generating significant surface compressive residual stresses (from +73 MPa to-298 MPa). Besides the surface, residual stresses, average surface roughness (Ra), arithmetical mean height (Sa) and parameters of the material ratio curve were also considered as a part of the study. Notable improvement was achieved in Sa, as it improved over 50 % while considerable improvement in Ra and the material ratio curve parameters has also been observed. Scanning electron microscopy confirmed that the void and porosity seen in the unpeened gears were filled. The electron backscatter diffraction analysis confirms the grain refinement in LPwC region up to 100 mu m depth. It was observed that multifold dislocation occurs within the grain, and dislocation generates sub-grain. The sub-grain formation substantially inhibits further nucleation and crack propagation owing to an increase in grain boundary density. Such improvement justifies the set objectives, and the outcome of this research will pave a foundation to improve the overall performance of the micro/meso parts using the LPwC process.
引用
收藏
页码:764 / 773
页数:10
相关论文
共 50 条
  • [41] Tailoring the surface integrity and wear resistance of WE43 Mg alloy by warm laser shock peening
    Li, Bowen
    Wang, Zongshen
    Kong, Meng
    Li, Jin
    Wang, Wenquan
    Zang, Tong
    Zheng, Hongyu
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 35 : 1504 - 1518
  • [42] Understanding the Mechanism of Stress Corrosion Cracking Resistance in Stainless Steel Welds Subjected to Laser Shock Peening without Coating for Nuclear Canister Applications
    John, Merbin
    Ralls, Alessandro M.
    Misra, Manoranjan
    Menezes, Pradeep L.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (08) : 3957 - 3977
  • [43] Enhanced fretting wear resistance of 2A12 aluminium alloys through laser shock peening without coating
    He, Gengchao
    Guo, Weiling
    Zhou, Longlong
    Li, Ke
    Huang, Yanfei
    Wang, Haidou
    Cai, Zhenbing
    Xing, Zhiguo
    TRIBOLOGY INTERNATIONAL, 2025, 208
  • [44] The effect of laser shock peening on surface integrity and high and very high cycle fatigue properties of 2024-T351 aluminum alloy
    Qin, Zhi
    Li, Bin
    Huang, Xia
    Zhang, Han
    Chen, Rui
    Adeel, Muhammad
    Xue, Hongqian
    OPTICS AND LASER TECHNOLOGY, 2022, 149
  • [45] Numerical simulation study of combined shot peening and laser shock peening on surface integrity of Ti-6Al-4V titanium alloy
    Wang, Quanwen
    Ma, Yue
    Fu, Xuesong
    Liu, Mengjin
    Cao, Ziwen
    Gai, Pengtao
    Zhou, Wenlong
    SURFACE & COATINGS TECHNOLOGY, 2024, 487
  • [46] Influence of Ultrasonic-Assisted Laser Shock Peening on Surface Integrity of IN718 Nickel-Based Alloy
    Meng Xiankai
    Chen Weiyu
    Wang Chunyan
    Cheng Zilong
    Yao Zhehe
    Wang Kun
    Song Fuyang
    Lin Ke
    ACTA OPTICA SINICA, 2024, 44 (11)
  • [47] Surface modification of 17-4 PH stainless steel by laser peening without protective coating process
    Karthik, D.
    Kalainathan, S.
    Swaroop, S.
    SURFACE & COATINGS TECHNOLOGY, 2015, 278 : 138 - 145
  • [48] Effect of laser shock peening without coating on fretting wear behavior of GH4169 superalloy at high-temperature
    Yu, Yanqing
    Ma, Tianbing
    Gong, Jianen
    Chen, Taili
    Zhou, Liucheng
    Cai, Zhenbing
    WEAR, 2024, 546
  • [49] The effect of laser shock peening with and without coating on microstructure and electrochemical corrosion behavior of AZ31b magnesium alloy
    Luo, Kaiyu
    Sun, Muran
    Lu, Jiajia
    Zhang, Qianwei
    Jiang, Xuxu
    Wang, Changyu
    Lu, Jinzhong
    SURFACE & COATINGS TECHNOLOGY, 2025, 496
  • [50] High energy laser shock peening of Ti6Al4V alloy without any protective coating
    Maharjan, Niroj
    Ramesh, Thivyaa
    Wang, Zichen
    APPLIED SURFACE SCIENCE, 2023, 638