Surface integrity of SLM manufactured meso-size gears in laser shock peening without coating

被引:13
|
作者
Pathak, Sunil [1 ]
Bohm, Marek [1 ,2 ]
Kaufman, Jan [1 ]
Kopecek, Jaromir [3 ]
Zulic, Sanin [1 ]
Stransky, Ondrej [1 ,4 ]
Shukla, Ashish [5 ]
Brajer, Jan [1 ]
Beranek, Libor [4 ]
Radhakrisnan, J. [6 ]
Rostohar, Danijela [7 ]
Mocek, Tomas [1 ]
机构
[1] Czech Acad Sci, Inst Phys, HiLASE Ctr, Prague, Czech Republic
[2] Czech Tech Univ, Fac Nucl Sci & Phys Engn, Prague, Czech Republic
[3] Czech Acad Sci, Inst Phys, Prague, Czech Republic
[4] Czech Tech Univ, Fac Mech Engn, Prague, Czech Republic
[5] Atlas Skilltech Univ, Navi Murnbai, Maharashtra, India
[6] Univ Politecn Madrid, ETS Ingenieros Ind, C Jose Gutierrez Abascal 2, Madrid 28006, Spain
[7] Coventry Univ, Inst Adv Mfg & Engn, Coventry CV6 5LZ, W Midlands, England
关键词
Laser shock peening; Meso; Gear; Surface quality; Residual stresses; Microstructure;
D O I
10.1016/j.jmapro.2022.12.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work aimed to improve the surface integrity of the selective laser melting manufacturing (SLM) manufactured 10 mm sized meso gears using the unconventional Laser Peening without Coating (LPwC) tech-nique. To accomplish LPwC on meso gears low energy in the range of 200 mJ to 1000 mJ at 10 Hz were applied underwater in the gear root and fillet gap generating significant surface compressive residual stresses (from +73 MPa to-298 MPa). Besides the surface, residual stresses, average surface roughness (Ra), arithmetical mean height (Sa) and parameters of the material ratio curve were also considered as a part of the study. Notable improvement was achieved in Sa, as it improved over 50 % while considerable improvement in Ra and the material ratio curve parameters has also been observed. Scanning electron microscopy confirmed that the void and porosity seen in the unpeened gears were filled. The electron backscatter diffraction analysis confirms the grain refinement in LPwC region up to 100 mu m depth. It was observed that multifold dislocation occurs within the grain, and dislocation generates sub-grain. The sub-grain formation substantially inhibits further nucleation and crack propagation owing to an increase in grain boundary density. Such improvement justifies the set objectives, and the outcome of this research will pave a foundation to improve the overall performance of the micro/meso parts using the LPwC process.
引用
收藏
页码:764 / 773
页数:10
相关论文
共 50 条
  • [31] Surface strengthening and fatigue life improvement of single crystal Ni-based superalloys via laser shock peening without coating
    Dang, Xiaofeng
    Liang, Xiaoqing
    Luo, Sihai
    Li, Yao
    Jiao, Yang
    Tian, Zeng
    He, Weifeng
    MATERIALS & DESIGN, 2023, 232
  • [32] Surface modification technique to enhance metallurgical and mechanical properties of alloy C-276 weldment by laser shock peening without coating
    S A Nithin Joseph Reddy
    E Thrinadh
    S Prabhakaran
    S Kalainathan
    N Arivazhagan
    M Manikandan
    Sādhanā, 2018, 43
  • [33] Surface Integrity and Oxidation of a Powder Metallurgy Ni-Based Superalloy Treated by Laser Shock Peening
    Tan, Qing
    Yan, Zhiran
    Huang, Hua
    Li, Shilei
    Wang, Yandong
    Feng, Yefei
    Zhou, Xin
    Li, Yinghong
    Ren, Yang
    Antonov, Stoichko
    JOM, 2020, 72 (05) : 1803 - 1810
  • [34] Effect of laser shock peening on surface integrity and tensile fatigue behavior of TB8 bolts
    Zhang, Yalong
    Jian, Xingming
    Xia, Feiyan
    Shi, Dapeng
    Wu, Luji
    Liu, Le
    Ji, Vincent
    ENGINEERING FAILURE ANALYSIS, 2024, 157
  • [35] Surface integrity integrity and fatigue lives of Ti17 compressor blades subjected to laser shock peening with square spots
    Zou, Shikun
    Wu, Junfeng
    Zhang, Yongkang
    Gong, Shuili
    Sun, Guifang
    Ni, Zhonghua
    Cao, Ziwen
    Che, Zhigang
    Feng, Aixin
    SURFACE & COATINGS TECHNOLOGY, 2018, 347 : 398 - 406
  • [36] Research on surface integrity of Ti-6Al-4V alloy with compound treatment of laser shock peening and shot peening
    Zhou, Liucheng
    Pan, Xinlei
    Shi, Xiaosong
    Du, Tianhan
    Wang, Lingfeng
    Luo, Sihai
    He, Weifeng
    Chen, Peiming
    VACUUM, 2022, 196
  • [37] Effect of laser shock peening without coating (LPwC) on a surface and sub-surface characteristics of aged Ti 15 V-3Al-3Cr-3Sn alloy
    Jose, Bibin
    Patil, Tejas
    Rajan, S. Sudhagara
    Praveenkumar, K.
    Manivasagam, Geetha
    Swaroop, S.
    MATERIALS TODAY-PROCEEDINGS, 2021, 46 : 578 - 582
  • [38] Effect of laser shock peening on the surface integrity and fretting fatigue properties of high-strength titanium alloy TC21
    Song, Bowen
    Wang, Xibin
    Xie, Lijing
    Xiang, Junfeng
    Zou, Xiangping
    Zou, Shikun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 4533 - 4547
  • [39] Influence of laser shock peening pulse density and spot size on the surface integrity of X2NiCoMo18-9-5 maraging steel
    Petan, Luca
    Luis Ocana, Jose
    Grum, Janez
    SURFACE & COATINGS TECHNOLOGY, 2016, 307 : 262 - 270
  • [40] Effect of Laser Shock Peening without Coating on Friction and Wear Properties of 40CrNiMo Structural Steel
    Chen C.-L.
    Feng A.-X.
    Wei Y.-C.
    Wang Y.
    Pan X.-M.
    Qiu H.
    Surface Technology, 2023, 52 (05): : 356 - 363and397