The corrosion behavior of Sc2O3-Y2O3 co-doped ZrO2 influenced by Sc2O3 content in CMAS at 1300 °C

被引:4
|
作者
Liao, Yuxuan [1 ,2 ]
Dai, Yifei [1 ,2 ]
Zhai, Yifan [1 ,2 ]
He, Aoping [1 ,2 ,3 ]
He, Huan [1 ,2 ,3 ]
Liang, Tianquan [1 ,2 ,3 ]
机构
[1] Guangxi Univ, State Key Lab Featured Met Mat & Life Cycle Safety, MOE Key Lab New Proc Technol Nonferrous Met & Mat, Nanning 530004, Peoples R China
[2] Guangxi Univ, Sch Resources Environm & Mat, Nanning 530004, Peoples R China
[3] Guangxi Univ, Ctr Ecol Collaborat Innovat Aluminum Ind Guangxi, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
ScYSZ; CMAS; Corrosion behavior; Reactivity; Mechanism; THERMAL BARRIER COATINGS; YTTRIA-STABILIZED ZIRCONIA; CALCIUM-MAGNESIUM ALUMINOSILICATE; PHYSICAL PROPERTIES; PHASE-STABILITY; PART I; RESISTANCE; CERAMICS; DEGRADATION; YB;
D O I
10.1016/j.jeurceramsoc.2023.09.025
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of Sc2O3 content on the corrosion behaviors of xSc2O3-3.5Y2O3 co-doped ZrO2 (ScYSZ, x = 4.5, 5.5 and 6.5 mol.%) in calcium-magnesium-alumino-silicate (CMAS) at 1300 degrees C was investigated in this paper. It is shown that the ScYSZ ceramic exhibits better resistance to molten CMAS attack when doping with more Sc2O3. The CMAS penetration depth in the ScYSZ ceramic decreases with increasing Sc2O3. It is about 18 mu m of CMAS penetrated depth in the 6.5Sc3.5YSZ after corrosion for 4 h at 1300 degrees C, including an 11 mu m and 7 mu m for the reaction-reprecipitation and grain-boundary infiltration layers, respectively. High thermochemical stability and weak reactivity of the ScYSZ to the glassy CMAS melt are beneficial to enhance the high temperature corrosion resistance, attributing to the low solubility in molten CMAS and the weak affinity to Ca2+ for small ionic radius Sc3+. The mechanism of enhancing the resistance to CMAS is discussed.
引用
收藏
页码:1179 / 1187
页数:9
相关论文
共 50 条
  • [31] Hot corrosion behavior of ZrO2 9.5Y2O3 5.6Yb2O3 5.2Gd2O3 TBCs in CMAS: CaO-MgO-Al2O3-SiO2
    M. Bahamirian
    S. M. M. Hadavi
    M. Farvizi
    A. Keyvani
    M. R. Rahimipour
    Journal of the Australian Ceramic Society, 2021, 57 : 215 - 224
  • [32] High-temperature phase stability of Y2O3 and SiO2 co-doped ZrO2 powder
    Gong, Jianping
    Gao, Pengfei
    Han, Guofeng
    Ma, Qianqian
    Wang, Xiaoming
    Chen, Silin
    Yang, Baijun
    JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2024, 109 (03) : 619 - 625
  • [33] Stability of Sc2O3 and CeO2 co-doped ZrO2 electrolyte during the operation of solid oxide fuel cells: Part III. Detailed mechanism of the decomposition
    Shimazu, Megumi
    Yamaji, Katsuhiko
    Kishimoto, Haruo
    Ueno, Akira
    Isobe, Toshihiro
    Katsumata, Ken-ichi
    Yokokawa, Harumi
    Okada, Kiyoshi
    SOLID STATE IONICS, 2012, 224 : 6 - 14
  • [34] Hot corrosion behavior of Sc2O3-Y2O3-ZrO2 thermal barrier coatings in presence of Na2SO4 + V2O5 molten salt
    Liu, Huai-fei
    Xiong, Xiang
    Li, Xiao-bin
    Wang, Ya-lei
    CORROSION SCIENCE, 2014, 85 : 87 - 93
  • [35] Corrosion behavior of GeO2 and Sc2O3 Coatings on AZ31 Alloy
    Sutha, L.
    Cyril, A.
    ORIENTAL JOURNAL OF CHEMISTRY, 2021, 37 (02) : 433 - 439
  • [36] Tailoring the thermal conductivity of Sc2O3-Yb2O3 Co-stabilized ZrO2 thermal barrier materials and mechanism insight
    Zhang, Jing
    Wang, Zhi-Gang
    Song, Xiwen
    Xie, Min
    Zhang, Yonghe
    Mu, Rende
    An, Shengli
    CERAMICS INTERNATIONAL, 2023, 49 (09) : 13601 - 13609
  • [37] CMAS corrosion resistance of Y 2 O 3-Al 2 O 3 binary ceramic materials
    Li, Chenguang
    Lai, Chenbiao
    Wu, Yaoyan
    Ouyang, Hanxiang
    Sun, Junbin
    Lu, Weihong
    CERAMICS INTERNATIONAL, 2024, 50 (08) : 13721 - 13731
  • [38] Residual Stress and Biaxial Strength in Sc2O3-CeO2-ZrO2/Y2O3-ZrO2 Layered Electrolytes
    Chen, Y.
    Aman, A.
    Lugovy, M.
    Orlovskaya, N.
    Wang, S.
    Huang, X.
    Graule, T.
    Kuebler, J.
    FUEL CELLS, 2013, 13 (06) : 1068 - 1075
  • [39] Effects of laser glazing on CMAS corrosion behavior of Y2O3 stabilized ZrO2 thermal barrier coatings
    Yan, Zheng
    Guo, Lei
    Li, Zhihua
    Yu, Yang
    He, Quanjun
    CORROSION SCIENCE, 2019, 157 : 450 - 461
  • [40] Improvement on corrosion resistance of molten calcium-magnesium-alumina-silicate (CMAS) by Yb2O3-Y2O3 co-stabilized ZrO2 ceramic pellets
    Liu, Yangguang
    Liu, Wei
    Wang, Weize
    Zhang, Wenkang
    Yang, Ting
    Li, Kaibin
    Tang, Zhongxiang
    Liu, Chen
    Zhang, Chengcheng
    CORROSION SCIENCE, 2024, 227