The corrosion behavior of Sc2O3-Y2O3 co-doped ZrO2 influenced by Sc2O3 content in CMAS at 1300 °C

被引:4
|
作者
Liao, Yuxuan [1 ,2 ]
Dai, Yifei [1 ,2 ]
Zhai, Yifan [1 ,2 ]
He, Aoping [1 ,2 ,3 ]
He, Huan [1 ,2 ,3 ]
Liang, Tianquan [1 ,2 ,3 ]
机构
[1] Guangxi Univ, State Key Lab Featured Met Mat & Life Cycle Safety, MOE Key Lab New Proc Technol Nonferrous Met & Mat, Nanning 530004, Peoples R China
[2] Guangxi Univ, Sch Resources Environm & Mat, Nanning 530004, Peoples R China
[3] Guangxi Univ, Ctr Ecol Collaborat Innovat Aluminum Ind Guangxi, Nanning 530004, Peoples R China
基金
中国国家自然科学基金;
关键词
ScYSZ; CMAS; Corrosion behavior; Reactivity; Mechanism; THERMAL BARRIER COATINGS; YTTRIA-STABILIZED ZIRCONIA; CALCIUM-MAGNESIUM ALUMINOSILICATE; PHYSICAL PROPERTIES; PHASE-STABILITY; PART I; RESISTANCE; CERAMICS; DEGRADATION; YB;
D O I
10.1016/j.jeurceramsoc.2023.09.025
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of Sc2O3 content on the corrosion behaviors of xSc2O3-3.5Y2O3 co-doped ZrO2 (ScYSZ, x = 4.5, 5.5 and 6.5 mol.%) in calcium-magnesium-alumino-silicate (CMAS) at 1300 degrees C was investigated in this paper. It is shown that the ScYSZ ceramic exhibits better resistance to molten CMAS attack when doping with more Sc2O3. The CMAS penetration depth in the ScYSZ ceramic decreases with increasing Sc2O3. It is about 18 mu m of CMAS penetrated depth in the 6.5Sc3.5YSZ after corrosion for 4 h at 1300 degrees C, including an 11 mu m and 7 mu m for the reaction-reprecipitation and grain-boundary infiltration layers, respectively. High thermochemical stability and weak reactivity of the ScYSZ to the glassy CMAS melt are beneficial to enhance the high temperature corrosion resistance, attributing to the low solubility in molten CMAS and the weak affinity to Ca2+ for small ionic radius Sc3+. The mechanism of enhancing the resistance to CMAS is discussed.
引用
收藏
页码:1179 / 1187
页数:9
相关论文
共 50 条
  • [21] Thermo-physical and mechanical properties of Yb2O3 and Sc2O3 co-doped Gd2Zr2O7 ceramics
    Guo, Yiqian
    He, Wenting
    Guo, Hongbo
    CERAMICS INTERNATIONAL, 2020, 46 (11) : 18888 - 18894
  • [22] Investigation of CMAS corrosion resistance for gradient Y 2 O 3 stabilized ZrO 2
    Wang, Wei
    Wen, Jiao
    He, Jian
    Cao, Pin
    Li, Chun
    Guo, Hongbo
    Peng, Hui
    SURFACE & COATINGS TECHNOLOGY, 2024, 487
  • [23] Hot corrosion evaluation of Gd2O3-Yb2O3 co-doped Y2O3 stabilized ZrO2 thermal barrier oxides exposed to Na2SO4+V2O5 molten salt
    Guo, Lei
    Zhang, Chenglong
    Li, Mingzhu
    Sun, Wei
    Zhang, Zhaoyang
    Ye, Fuxing
    CERAMICS INTERNATIONAL, 2017, 43 (02) : 2780 - 2785
  • [24] Hot corrosion behavior of ZrO29.5Y2O35.6Yb2O35.2Gd2O3TBCs in CMAS: CaO-MgO-Al2O3-SiO2
    Bahamirian, M.
    Hadavi, S. M. M.
    Farvizi, M.
    Keyvani, A.
    Rahimipour, M. R.
    JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2021, 57 (01) : 215 - 224
  • [25] Microstructure and Thermal Cycling Behavior of Ta2O5 and Y2O3 Co-doped ZrO2 Coatings
    Dong Chen
    Jing Lu
    Chengchuan Sun
    Quansheng Wang
    Xianjin Ning
    Journal of Thermal Spray Technology, 2023, 32 : 1327 - 1337
  • [26] Investigation on the phase stability, sintering and thermal conductivity of Sc2O3-Y2O3-ZrO2 for thermal barrier coating application
    Liu, Huaifei
    Li, Songlin
    Li, Qilian
    Li, Yongming
    MATERIALS & DESIGN, 2010, 31 (06): : 2972 - 2977
  • [27] Microstructure and Thermal Cycling Behavior of Ta2O5 and Y2O3 Co-doped ZrO2 Coatings
    Chen, Dong
    Lu, Jing
    Sun, Chengchuan
    Wang, Quansheng
    Ning, Xianjin
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2023, 32 (05) : 1327 - 1337
  • [28] Comparison of corrosion behaviors and wettability of CMAS on Ta2O5-Y2O3 co-stabilized ZrO2 and YSZ thermal barrier coatings
    Wang, Jinshuang
    Wang, Yinghui
    Lu, Xianjun
    Hu, Mengqiu
    Chen, Mengdi
    Shu, Chaoxi
    Zhang, Hao
    Tian, Yongshang
    Liu, Bing
    Jing, Qiangshan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2023, 43 (13) : 5636 - 5651
  • [29] Large scale synthesis of non-transformable tetragonal Sc2O3, Y2O3 doped ZrO2 nanopowders via the citric acid based gel method to obtain plasma sprayed coating
    Loghman-Estarki, Mohammad Reza
    Edris, Hossein
    Razavi, Reza Shoja
    CERAMICS INTERNATIONAL, 2013, 39 (07) : 7817 - 7829
  • [30] Phase stability of ZrO2 9.5Y2O3 5.6Yb2O3 5.2Gd2O3 compound at 1100 °C and 1300 °C for advanced TBC applications
    Bahamirian, M.
    Hadavi, S. M. M.
    Farvizi, M.
    Rahimipour, M. R.
    Keyvani, A.
    CERAMICS INTERNATIONAL, 2019, 45 (06) : 7344 - 7350