Effect of Quenching Temperature on the Strengthening Mechanism of Low-Carbon Microalloyed Quenching and Partitioning Steel

被引:1
作者
Chu, Xiaohong [1 ,2 ]
Chen, Weijian [1 ,2 ]
Liu, Jinhai [1 ,2 ]
Pan, Yinkui [1 ,2 ]
Sun, Hang [1 ,2 ]
Zhao, Zhengzhi [1 ,2 ]
机构
[1] Univ Sci & Technol Beijing, Collaborat Innovat Ctr Steel Technol, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Beijing Lab Modern Transportat Adv Met Mat & Proc, Beijing 100083, Peoples R China
关键词
mechanical properties; microstructures; quenching and partitioning steels; quenching temperatures; strengthening mechanism; HOT-ROLLED TI; RETAINED AUSTENITE; LATH MARTENSITE; FERRITE; MICROSTRUCTURE; TRANSFORMATION; PRECIPITATION; DISLOCATIONS; MORPHOLOGY; BEHAVIOR;
D O I
10.1002/srin.202200601
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Herein, the microstructures of the low-carbon microalloyed quenching and partitioning (Q-P) steels are multiphase with ferrite (F), martensite (M), and retained austenite (RA) at different quenching temperatures (QTs), i.e., 140, 180, 240, and 300 degrees C. The volume fraction of fresh martensite (FM) increases from 8.6% to 61.4%, but the tempered martensite (TM) decreases from 49.7% to 0% with the QT increase. Meanwhile, the size of the precipitates (Nb, Ti)C tends to increase, whereas the fraction of the precipitates decreases first and then increases. With the increase of the QT, the yield strength (YS) decreases, the tensile strength (TS) increases, and the elongation first increases and then decreases. Additionally, the strengthening mechanism of Q-P steel is quantitatively analyzed in terms of F, M, RA, and precipitation strengthening. This study shows that F makes the same contribution to YS for the tested steels. The major strengthening mechanism of the Q-P steel is contributed by M, which accounts for about 43.7% to 56.0% of total YS. RA greatly influences the plasticity of Q-P steel and provides little to YS. With an increase in QT, the precipitation strengthening values first decrease and then increase.
引用
收藏
页数:10
相关论文
共 50 条
[41]   Improving Tensile Properties of Room-Temperature Quenching and Partitioning Steel by Dislocation Engineering [J].
He, B. B. ;
Wang, M. ;
Huang, M. X. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (09) :4021-4026
[42]   Low-temperature bainite in low-carbon steel [J].
Long, X. Y. ;
Zhang, F. C. ;
Kang, J. ;
Lv, B. ;
Shi, X. B. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 594 :344-351
[43]   Effect of Quenching and Tempering on Mechanical Properties and Impact Fracture Behavior of Low-Carbon Low-Alloy Steel [J].
Zhang, Yajing ;
Yang, Jianhua ;
Xiao, Daheng ;
Luo, Deng ;
Tuo, Chende ;
Wu, Huibin .
METALS, 2022, 12 (07)
[44]   One-step quenching and partitioning treatment of a commercial low silicon boron steel [J].
Kong, H. ;
Chao, Q. ;
Cai, M. H. ;
Pavlina, E. J. ;
Rolfe, B. ;
Hodgson, P. D. ;
Beladi, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 707 :538-547
[45]   Work hardening behaviors of a low carbon Nb-microalloyed Si-Mn quenching-partitioning steel with different cooling styles after partitioning [J].
Zhang, Jun ;
Ding, Hua ;
Wang, Chao ;
Zhao, Jingwei ;
Ding, Ting .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 585 :132-138
[46]   Effect of partitioning treatment on the strengthening and plasticising mechanism of one-step quenching and partitioning steels [J].
Liu, Yajun ;
Gan, Xiaolong ;
Wang, Shuize ;
Liang, Liang ;
Xu, Yaowen ;
Xu, Guang ;
Liu, Man .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 :1091-1103
[47]   Effect of intercritical deformation on tensile performance of a low-carbon Si–Mn steel processed by quenching and bainitic partitioning [J].
Ya-qiang Tian ;
Zhong-qian Cao ;
Wang Li ;
Hong-bo Pan ;
Xiao-ping Zheng ;
Jin-ying Song ;
Ying-li Wei ;
Lian-sheng Chen .
Journal of Iron and Steel Research International, 2020, 27 :208-216
[48]   Effect of acicular ferrite on banded structures in low-carbon microalloyed steel [J].
Shi, Lei ;
Yan, Ze-sheng ;
Liu, Yong-chang ;
Yang, Xu ;
Zhang, Cheng ;
Li, Hui-jun .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (12) :1167-1174
[49]   Effect of helical rolling on the bainitic microstructure and impact toughness of the low-carbon microalloyed steel [J].
Derevyagina, L. S. ;
Gordienko, A., I ;
Surikova, N. S. ;
Volochaev, M. N. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 816
[50]   Effect of tempering temperature on microstructure and mechanical properties of a low carbon bainitic steel treated by quenching-partitioning-tempering (QPT) process [J].
Liu, Xingyu ;
Han, Ying ;
Wei, Junhu ;
Zu, Guoqing ;
Zhao, Yu ;
Zhu, Weiwei ;
Ran, Xu .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 23 :911-918