Strain ageing embrittlement behaviour of X80 self-shielded flux-cored girth weld metal

被引:22
作者
Guo, Lei [1 ]
Su, Xin [2 ]
Dai, Lianshuang [3 ]
Wang, Leilei [1 ]
Sun, Qiaofei [2 ]
Fan, Chaohai [2 ]
Wang, Yalei [4 ]
Li, Xueda [4 ]
机构
[1] PipeChina West East Gas Pipeline Co, Prod & operat Dept, Shanghai, Peoples R China
[2] China Petr Pipeline Res Inst CO LTD, Pipeline Mat & Anticorros Technol Ctr, Langfang, Peoples R China
[3] China Oil & Gas Piping Network Corp, Sci & Technol informat Ctr, Beijing, Peoples R China
[4] China Univ Petr East China, Sch Mat Sci & Engn, Beijing, Peoples R China
关键词
Pipeline; self-shielded flux-cored welding (FCAW); girth weld metal; strain ageing; embrittlement; TOUGHNESS;
D O I
10.1080/10667857.2023.2164978
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Strain ageing embrittlement behaviour of X80 self-shielded flux-cored arc welding (FCAW) girth weld metal at different strain ageing conditions (1% prestrain, and aged at 150 degrees C/100 degrees C for 1 -6 h, and 80 degrees C for 1-30 days) was studied. Microstructure of FCAW girth weld generally consisted of coarse granular bainite and lath bainite. After strain ageing, toughness notably decreased, and higher ageing temperature or longer ageing induced lower toughness, until ageing is fully yielded. At initial stage of strain ageing, more dimples were found accompanying with cleavage facet. With the progress of strain ageing, the embrittlement was more obvious, while larger cleavage facet and less dimples were found. Meanwhile, the critical size for cleavage fracture initiation site became smaller. Martensite-austenite constituent (1-2 mu m) was found to initiate cleavage fracture when partially strain aged, while submicron inclusions could initiate cleavage facet when fully strain aged.
引用
收藏
页数:7
相关论文
共 24 条
[1]   Effect of nitrogen on toughness and strain age embrittlement of ferritic steel weld metal [J].
Achar, DRG ;
Kocak, M ;
Evans, GM .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 1998, 3 (05) :233-243
[2]  
Baird J. D., 1971, Metallurgical Reviews, P1
[3]  
Cheng YF, 2020, OIL GAS STORAGE TRAN, V39, P1
[4]   DISLOCATION THEORY OF YIELDING AND STRAIN AGEING OF IRON [J].
COTTRELL, AH ;
BILBY, BA .
PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON SECTION A, 1949, 62 (349) :49-62
[5]  
[崔天成 Cui Tiancheng], 2010, [机械工程材料, Materials for Mechanical Engineering], V34, P30
[6]   Effect of prestraining and strain-aging on toughness of MnMoNi steel weld metal [J].
do Patrocínio, AB ;
Novovic, M ;
Bowen, P .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2004, 155 :1124-1131
[7]  
[高杉杉 Gao Shanshan], 2021, [焊接学报, Transactions of the China Welding Institution], V42, P22
[8]   EFFECT OF ARTIFICIAL STRAIN AGING ON MICRO-STRUCTURE AND MECHANICAL-PROPERTIES OF A SINGLE-BEAD FERRITIC WELD METAL [J].
HOEKSTRA, S ;
SCHMIDTVANDERBURG, MAM ;
MANDZIEJ, S ;
BEYER, J .
MATERIALS SCIENCE AND TECHNOLOGY, 1985, 1 (03) :234-239
[9]   Correlation of microstructure with tensile behavior and properties of API X70 pipeline steels subjected to strain aging [J].
Lee, Sang-in ;
Hwang, Byoungchul .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2020, 27 (03) :319-324
[10]   Effect of strain aging on properties of X90 line pipe [J].
Li Yan-hua ;
Chi Qiang ;
Feng Hui ;
Chen Hong-yuan ;
Xu Xiao-feng .
ENGINEERING FAILURE ANALYSIS, 2020, 118