Influence of Surface Treatment and Accelerated Ageing on Biaxial Flexural Strength and Hardness of Zirconia

被引:3
作者
Rohr, Nadja [1 ]
Schonenberger, Angela Jacqueline [1 ]
Fischer, Jens [1 ]
机构
[1] Univ Basel, Univ Ctr Dent Med Basel UZB, Dept Reconstruct Dent, Biomat & Technol, CH-4058 Basel, Switzerland
关键词
zirconia implants; accelerated ageing; surface treatment; mechanical properties; OSTEOBLAST-LIKE CELLS; Y-TZP; MARTENS HARDNESS; TITANIUM; IMPLANTS; ROUGHNESS; CERAMICS;
D O I
10.3390/ma16030910
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aim was to investigate how the surface treatment and the process of accelerated ageing of zirconia for dental implants affect the biaxial flexural strength and hardness. Zirconia discs with a diameter of 12.6 mm were subjected to either one of the following treatments: polishing (Zp); polishing and heat treatment at 1250 degrees C for 1 h (Zpt); machining (Zm); machining and heat treatment (Zmt); or sandblasting, acid-etching, and heat treatment (Z14) (n = 45 per group). Biaxial flexural strength and Martens hardness (HM) were measured without further treatment and after accelerated ageing for 5 h or 5 x 5 h according to ISO 13356 (n = 15 per group). Two-way ANOVA was applied to test the effect of surface treatment and ageing (alpha = 0.05). The reliability of the specimens was described with Weibull two-parameter distribution of biaxial flexural strength data. Overall, the surface treatment (p < 0.001) and ageing (p = 0.012) revealed a significant effect on biaxial flexural strength values, while HM was only affected by the surface treatment (p < 0.001) but not ageing (p = 0.160). Surface treatment significantly affected HM (p < 0.001) but not ageing (p = 0.160). The applied surface treatments affected the biaxial flexural strength and HM of zirconia. For accelerated ageing, a duration of both 5 h and 5 x 5 h is recommended to evaluate the effect of surface treatments. Zm was the most reliable surface as it was least affected by ageing and provided low standard deviations of biaxial flexural strength values.
引用
收藏
页数:11
相关论文
共 31 条
[1]  
[Anonymous], HARDNESS TEST MARTEN
[2]  
[Anonymous], 2008, ISO 13356
[3]  
[Anonymous], 2015, 687273 ISO
[4]   Behavior of CAL72 osteoblast-like cells cultured on zirconia ceramics with different surface topographies [J].
Baechle, Maria ;
Butz, Frank ;
Huebner, Ute ;
Bakalinis, Emmanouil ;
Kohal, Ralf J. .
CLINICAL ORAL IMPLANTS RESEARCH, 2007, 18 (01) :53-59
[5]   Zirconia implants restored with single crowns or fixed dental prostheses: 5-year results of a prospective cohort investigation [J].
Balmer, Marc ;
Spies, Benedikt C. ;
Kohal, Ralf-Joachim ;
Haemmerle, Christoph Hans-Franz ;
Vach, Kirstin ;
Jung, Ronald E. .
CLINICAL ORAL IMPLANTS RESEARCH, 2020, 31 (05) :452-462
[6]   Three-year analysis of zirconia implants used for single-tooth replacement and three-unit fixed dental prostheses: A prospective multicenter study [J].
Balmer, Marc ;
Spies, Benedikt C. ;
Vach, Kirstin ;
Kohal, Ralf-Joachim ;
Hammerle, Christoph H. F. ;
Jung, Ronald E. .
CLINICAL ORAL IMPLANTS RESEARCH, 2018, 29 (03) :290-299
[7]   A prospective clinical study to evaluate the performance of zirconium dioxide dental implants in single-tooth edentulous area: 3-year follow-up [J].
Bormann, Kai-Hendrik ;
Gellrich, Nils-Claudius ;
Kniha, Heinz ;
Schild, Sabine ;
Weingart, Dieter ;
Gahlert, Michael .
BMC ORAL HEALTH, 2018, 18
[8]  
Branemark P I, 1970, Arsb Goteb Tandlak Sallsk, P9
[9]   Low-temperature degradation in zirconia with a porous surface [J].
Chevalier, Jerome ;
Loh, Joel ;
Gremillard, Laurent ;
Meille, Sylvain ;
Adolfson, Erik .
ACTA BIOMATERIALIA, 2011, 7 (07) :2986-2993
[10]   MECHANICAL-PROPERTIES AND SHORT-TERM INVIVO EVALUATION OF YTTRIUM-OXIDE-PARTIALLY-STABILIZED ZIRCONIA [J].
CHRISTEL, P ;
MEUNIER, A ;
HELLER, M ;
TORRE, JP ;
PEILLE, CN .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1989, 23 (01) :45-61