Hydrogen Embrittlement Behavior and Mechanism of Low Carbon Medium Manganese Steel Gas Metal Arc Welding Joints

被引:0
|
作者
Du, Y. [1 ,2 ]
Gao, X. H. [2 ]
Wang, X. N. [1 ]
Dong, Y. [2 ]
Zhang, B. [2 ]
Wu, H. Y. [2 ]
Sun, C. [3 ]
Du, L. X. [2 ]
机构
[1] Soochow Univ, Sch Iron & Steel, Suzhou 215021, Jiangsu, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Liaoning, Peoples R China
[3] Nanjing Iron & Steel Co Ltd, Nanjing 210035, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
ASSISTED CRACKING; REVERSED AUSTENITE; TRAPPING SITES; STRENGTH; MICROSTRUCTURE; SUSCEPTIBILITY; TOUGHNESS; ATOMS;
D O I
10.1007/s11837-023-06064-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The hydrogen embrittlement behavior of two low-carbon medium manganese steel welding joints was elucidated using a slow strain rate tensile experiment, hydrogen permeation experiment, and hydrogen concentration test. The fracture starting position becomes heat-affected zone (HAZ) after hydrogen charging. The hydrogen concentration of HAZ is higher than weld material (WM) for two welding joints after hydrogen charging for both 1 h and 2 h. The hydrogen embrittlement susceptibility of the welding joint with high hydrogen concentration, which contains about 0.03 Ti in both WM and HAZ, is larger than the welding joint that does not contain Ti. When the hydrogen charging time of the Ti-contained welding joints increases from 1 h to 2 h, the fractography of WM changes from small shallow dimples (hydrogen enhanced localized plasticity) to quasi-cleavage and cleavage (hydrogen enhanced decohesion), and the fractography of HAZ changes from quasi-cleavage (hydrogen enhanced decohesion) to intergranular (hydrogen enhanced decohesion).
引用
收藏
页码:4407 / 4420
页数:14
相关论文
共 50 条
  • [21] Influence of Welding Consumables on Ballistic Performance of Gas Metal Arc Welded Ultra-high Hard Armor Steel Joints
    Subramani, Naveen Kumar
    Visvalingam, Balasubramanian
    Sudersanan, Malarvizhi
    Abdur, Hafeezur Rahman
    Vadivel, Balaguru
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2021, 10 (01) : 443 - 462
  • [22] Improvement of localised corrosion resistance of AISI 2205 Duplex Stainless Steel joints made by gas metal arc welding under electromagnetic interaction of low intensity
    Garcia-Renteria, M. A.
    Lopez-Morelos, V. H.
    Garcia-Hernandez, R.
    Dzib-Perez, L.
    Garcia-Ochoa, E. M.
    Gonzalez-Sanchez, J.
    APPLIED SURFACE SCIENCE, 2014, 321 : 252 - 260
  • [23] Application of acoustic emission method for investigation of hydrogen embrittlement mechanism in the low-carbon steel
    Merson, E.
    Vinogradov, A.
    Merson, D. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 645 : S460 - S463
  • [24] Effect of strain rate on hydrogen embrittlement in low-carbon martensitic steel
    Momotani, Yuji
    Shibata, Alzinobu
    Terada, Daisuke
    Tsuji, Nobuhiro
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (05) : 3371 - 3379
  • [25] Enhancing the hydrogen embrittlement resistance of medium-carbon high-strength steel by optimizing the tempering temperature
    Saha, Sourav Kr.
    Moon, Byungrok
    Lee, Changhoon
    Lee, Seung-gun
    Chung, Junho
    Kang, Namhyun
    MATERIALS CHARACTERIZATION, 2024, 207
  • [26] Influence of carbon content on microstructure and mechanical properties of 1000 MPa deposited metal by gas metal arc welding
    An, Tong-bang
    Wei, Jin-shan
    Zhao, Lin
    Shan, Ji-guo
    Tian, Zhi-ling
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2019, 26 (05) : 512 - 518
  • [27] Behavior of a superaustenitic stainless steel weld cladding deposited by the gas metal arc welding process
    Matias, Joao V. S.
    Lourenco, Manuel J. C.
    Jorge, Jorge C. F.
    de Souza, Luis Felipe G.
    Farneze, Humberto N.
    Mendes, Matheus C.
    da Silva, Cilene Labre Alves
    Araujo, Leonardo S.
    MATERIALS TODAY COMMUNICATIONS, 2023, 34
  • [28] Wear behavior of ceramic powder cladded on carbon steel surface by gas tungsten arc welding
    Peng, De-Xing
    Kang, Yuan
    Li, Zheng-Xian
    Chang, Shih-Yen
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2013, 65 (02) : 129 - 134
  • [29] Effects of defect on the hydrogen embrittlement behavior of X80 pipeline steel in hydrogen-blended natural gas environments
    Yang, Hongchao
    Zhang, Huimin
    Liu, Cuiwei
    Wang, Cailin
    Fan, Xin
    Cheng, Frank
    Li, Yuxing
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 58 : 158 - 173
  • [30] Linear Friction Stir Welding of Medium Carbon Steel at Low Temperature
    Aoki, Yasuhiro
    Kuroiwa, Ryosuke
    Fujii, Hidetoshi
    Murayama, Gen
    Yasuyama, Masanori
    ISIJ INTERNATIONAL, 2019, 59 (10) : 1853 - 1859