Influence of surface treatment on the metal dusting behavior of alloy 699 XA

被引:7
|
作者
White, Emma [1 ]
Schlereth, Clara [1 ]
Lepple, Maren [1 ]
Hattendorf, Heike [2 ]
Nowak, Benedikt [2 ]
Galetz, Mathias C. [1 ]
机构
[1] DECHEMA Forschungsinst, Mat & Corros Div, High Temp Mat, Theodor Heuss Allee 25, D-60486 Frankfurt, Germany
[2] VDM Met Int GmbH, Res & Dev Dept, Altena, Germany
来源
基金
欧盟地平线“2020”;
关键词
metal dusting; Ni-based alloy; oxide former; plastic deformation; shot peening; surface treatment; NI-BASE ALLOYS; RESISTANCE; MECHANISMS; INITIATION; KINETICS;
D O I
10.1002/maco.202213380
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Metal dusting attack is a serious problem in processing industries using carbonaceous gases and high temperatures. Ni-based alloy 699 XA was recently developed as an alloy for these types of environments with high resistance against metal dusting. In this study, different surface treatments of this chromium- and aluminum-rich alloy are shown to have an important influence on the metal dusting onset behavior. It was found that surface treatments that are traditionally considered to be helpful for fatigue performance, for example, shot peening, and pickling were detrimental to the metal dusting performance of alloy 699 XA. Additionally, the shot peening surface treatment promoted Fe surface contamination, resulting in a negative impact on the metal dusting pitting resistance of the alloy. Deformation accompanied by apparent BCC alpha-Cr precipitation in the bulk microstructure, but a comparison with cold-rolled materials shows that the surface treatment dominates the metal dusting resistance.
引用
收藏
页码:190 / 196
页数:7
相关论文
共 50 条
  • [31] Behavior of uncoated and coated pure Fe in metal dusting conditions
    Melo-Maximo, D.
    Murillo, A. E.
    Salas, O.
    Melo-Maximo, L.
    Oseguera, J.
    SURFACE & COATINGS TECHNOLOGY, 2016, 308 : 10 - 18
  • [32] Protection of high alloy steels against metal dusting by oxide scales
    Grabke, HJ
    Muller-Lorenz, EM
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1998, 49 (05): : 317 - 320
  • [33] Influence of Al and Fe additions on metal dusting of NiCr alloys
    Schlereth, Clara
    Oskay, Ceyhun
    Hattendorf, Heike
    Nowak, Benedikt
    Galetz, Mathias C.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2022, 73 (09): : 1346 - 1358
  • [34] Influence of Al and Fe additions on metal dusting of NiCr alloys
    Schlereth, Clara
    Oskay, Ceyhun
    Hattendorf, Heike
    Nowak, Benedikt
    Galetz, Mathias C.
    Materials and Corrosion, 2022, 73 (09) : 1346 - 1358
  • [35] Corrosion resistance of a high-silicon alloy in metal-dusting environments
    Chun, C. M.
    Ramanarayanan, T. A.
    OXIDATION OF METALS, 2007, 67 (3-4): : 215 - 234
  • [36] Pure bending testing of Cr-Mo alloy in metal dusting condition
    Xu, Tao
    Tu, Shan-Tung
    Song, Hong-Jian
    Gong, Jian-Ming
    PROGRESSES IN FRACTURE AND STRENGTH OF MATERIALS AND STRUCTURES, 1-4, 2007, 353-358 : 341 - 344
  • [37] Metal Dusting Behavior of 321 Stainless Steel: Effects of Edge and Corner
    Chang, Chia-Hao
    Tsai, Wen-Ta
    METALS AND MATERIALS INTERNATIONAL, 2011, 17 (02) : 267 - 273
  • [38] Metal dusting behavior of 321 stainless steel: Effects of edge and corner
    Chia-Hao Chang
    Wen-Ta Tsai
    Metals and Materials International, 2011, 17 : 267 - 273
  • [39] Damage of a heat-treatment retort by metal dusting attack
    Dettenwanger, F
    Grotmann, D
    Friedrich, H
    Berghof-Hasselbächer, E
    Schorr, M
    Schütze, M
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1999, 50 (05): : 289 - 293
  • [40] Influence of surface polishing on the degradation behavior of biodegradable Magnesium alloy
    Kumar, Lalit
    Jain, Arihan
    Kumar, Kamal
    Sharma, Gaurav Kumar
    ENGINEERING RESEARCH EXPRESS, 2023, 5 (04):