Influence of surface treatment on the metal dusting behavior of alloy 699 XA

被引:7
|
作者
White, Emma [1 ]
Schlereth, Clara [1 ]
Lepple, Maren [1 ]
Hattendorf, Heike [2 ]
Nowak, Benedikt [2 ]
Galetz, Mathias C. [1 ]
机构
[1] DECHEMA Forschungsinst, Mat & Corros Div, High Temp Mat, Theodor Heuss Allee 25, D-60486 Frankfurt, Germany
[2] VDM Met Int GmbH, Res & Dev Dept, Altena, Germany
来源
基金
欧盟地平线“2020”;
关键词
metal dusting; Ni-based alloy; oxide former; plastic deformation; shot peening; surface treatment; NI-BASE ALLOYS; RESISTANCE; MECHANISMS; INITIATION; KINETICS;
D O I
10.1002/maco.202213380
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Metal dusting attack is a serious problem in processing industries using carbonaceous gases and high temperatures. Ni-based alloy 699 XA was recently developed as an alloy for these types of environments with high resistance against metal dusting. In this study, different surface treatments of this chromium- and aluminum-rich alloy are shown to have an important influence on the metal dusting onset behavior. It was found that surface treatments that are traditionally considered to be helpful for fatigue performance, for example, shot peening, and pickling were detrimental to the metal dusting performance of alloy 699 XA. Additionally, the shot peening surface treatment promoted Fe surface contamination, resulting in a negative impact on the metal dusting pitting resistance of the alloy. Deformation accompanied by apparent BCC alpha-Cr precipitation in the bulk microstructure, but a comparison with cold-rolled materials shows that the surface treatment dominates the metal dusting resistance.
引用
收藏
页码:190 / 196
页数:7
相关论文
共 50 条
  • [21] Evaluation of Metal Dusting Behavior in Reformer Tube Made of HP-Nb Alloy on the Outer Surfaces
    Shabani, A. M.
    Jalal, T.
    Saatchi, A.
    Vaghefi, M. Monir
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2017, 70 (06) : 1519 - 1525
  • [22] Metal dusting on an alumina forming Ni-base alloy
    Szakalos, P.
    Lundberg, M.
    Pettersson, R.
    CORROSION SCIENCE, 2006, 48 (07) : 1679 - 1695
  • [23] Metal dusting: relationship between alloy composition and degradation rate
    Hermse, C. G. M.
    van Wortel, J. C.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2009, 44 (03) : 182 - 185
  • [24] Initial Stages in the Metal-dusting Process on Alloy 800
    Daniel Röhnert
    Fritz Phillipp
    Helfried Reuther
    Till Weber
    Egbert Wessel
    Michael Schütze
    Oxidation of Metals, 2007, 68 : 271 - 293
  • [25] Oxidation of additive manufactured 699XA Ni-based alloy under different atmospheres
    Pedraza, Fernando
    Duval, Antoine
    Sulak, Ivo
    Nowak, Benedikt
    Kepa, Thomas
    Boissonnet, Germain
    Bonnet, Gilles
    CORROSION SCIENCE, 2024, 237
  • [26] A new nickel-base alloy for metal dusting resistance
    Baker, BA
    Hartmann, VW
    Shoemaker, LE
    McCoy, SA
    Rajendran, S
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2003, 56 (03): : 327 - 333
  • [27] Initial stages in the metal-dusting process on alloy 800
    Roehnert, Daniel
    Phillipp, Fritz
    Reuther, Helfried
    Weber, Till
    Wessel, Egbert
    Schuetze, Michael
    OXIDATION OF METALS, 2007, 68 (5-6): : 271 - 293
  • [28] Influence of H2S on metal dusting
    Schneider, A
    Viefhaus, H
    Inden, G
    Grabke, HJ
    Muller-Lorenz, EM
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 1998, 49 (05): : 336 - 339
  • [29] Characterisation of the coke formed during the metal dusting of low alloy steels
    Potter, Darren J.
    Tatlock, Gordon J.
    Romani, Simon
    MATERIALS AT HIGH TEMPERATURES, 2012, 29 (02) : 123 - 128
  • [30] Inhibition of metal dusting corrosion on Fe-based alloy by combined near surface severe plastic deformation (NS-SPD) and thermochemical treatment
    Guo, Xiaoyang
    Vullum, Per Erik
    Venvik, Hilde J.
    CORROSION SCIENCE, 2021, 190