Effect of Molten Steel Composition on Inclusion Modification by Calcium Treatment in Al-Killed Tinplate Steel

被引:5
|
作者
Li, Xiaoao [1 ,2 ]
Wang, Nan [2 ,3 ]
Chen, Min [1 ,2 ]
Du, Zhiqiang [2 ]
机构
[1] Northeastern Univ, Key Lab Ecol Met Multimetall Ores, Minist Educ, 3-11 Wenhua Rd, Shenyang 110819, Peoples R China
[2] Northeastern Univ, Sch Met, Shenyang 110819, Liaoning, Peoples R China
[3] Inst Frontier Technol Low Carbon Steelmaking, Shenyang 110819, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-killed steel; inclusions; calcium treatment; molten steel composition; liquid zone; NONMETALLIC INCLUSIONS; DEOXIDATION EQUILIBRIA; TRANSIENT EVOLUTION; SULFUR; SLAG; MECHANISM; MODEL; MG; THERMODYNAMICS; IMPROVEMENT;
D O I
10.2355/isijinternational.ISIJINT-2022-274
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The effects of oxygen, magnesium, and sulfur content in Al-killed tinplate steel on the "liquid zone" of inclusion modification by calcium treatment were clarified through industrial experiments and thermodynamic calculation, and the characteristics of inclusions modification were studied. The results show that the inclusions in molten steel before calcium treatment are mainly Al2O3 inclusions. The inclusions in molten steel are CaO center dot Al2O3 after calcium treatment with a holding time of 10 min, while the inclusions are mainly 3CaO center dot Al2O3 with a holding time of 30 min. And 12CaO center dot 7Al(2)O(3) inclusions are observed in molten steel when T.O content increases to 40 ppm after calcium treatment with a holding time of 30 min. As the increase of T.O content from 10 ppm to 40 ppm, the difference between the upper and lower limits of the critical calcium content corresponding to the "liquid zone" increases from 5 ppm to 17 ppm. The increase of T.O content in molten steel will enlarge the "liquid zone" range of inclusion modification by calcium treatment, and increase the critical calcium content. With the increase of magnesium content in molten steel, the liquid phase ratio of inclusions modification by calcium treatment decreases. To obtain the liquid phase ratio of inclusions at least 50% in molten steel, not only the calcium content in steel should be strictly controlled, but also the magnesium content in steel should not be larger than 15 ppm. With the increase of sulfur content in molten steel, the "liquid zone" range of inclusion modification by calcium treatment becomes narrow.
引用
收藏
页码:303 / 312
页数:10
相关论文
共 50 条
  • [21] Effect of Ce on inclusion, microstructure and mechanical properties of Al-killed high-strength steel
    Huang, Fei
    Li, Jing
    Zang, Ruoyu
    IRONMAKING & STEELMAKING, 2023, 50 (07) : 744 - 756
  • [22] Dissolution Behavior of Mg from Magnesia-Chromite Refractory into Al-killed Molten Steel
    Liu, Chunyang
    Yagi, Motoki
    Gao, Xu
    Kim, Sun-Joong
    Huang, Fuxiang
    Ueda, Shigeru
    Kitamura, Shin-Ya
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2018, 49 (05): : 2298 - 2307
  • [23] Modification of MgO·Al2O3 spinel inclusions in Al-killed steel by Ca-treatment
    Shu-feng Yang
    Jing-she Li
    Zai-fei Wang
    Jiao Li
    Lin Lin
    International Journal of Minerals, Metallurgy, and Materials, 2011, 18 : 18 - 23
  • [25] Dissolution Behavior of Mg from MgO-C Refractory in Al-killed Molten Steel
    Liu, Chunyang
    Gao, Xu
    Kim, Sun-joong
    Ueda, Shigeru
    Kitamura, Shin-ya
    ISIJ INTERNATIONAL, 2018, 58 (03) : 488 - 495
  • [26] Inclusion Evolution after Calcium Addition in Low Carbon Al-Killed Steel with Ultra Low Sulfur Content
    Yang, Guangwei
    Wang, Xinhua
    ISIJ INTERNATIONAL, 2015, 55 (01) : 126 - 133
  • [27] Effect of Refining-Slag Basicity on Precipitation Behavior of Spinel Inclusions in Al-Killed Steel
    Yan, Xinbo
    Yu, Yue
    Li, Jianli
    JOM, 2024, 76 (07) : 3302 - 3310
  • [28] Effect of Ce on inclusion evolution and HAZ mechanical properties of Al-killed high-strength steel
    Geng, Ruming
    Li, Jing
    Shi, Chengbin
    IRONMAKING & STEELMAKING, 2021, 48 (07) : 796 - 802
  • [29] Influence of Mg/Ti complex addition on evolution and thermodynamics of the inclusion in Al-killed steel
    Zhang, Tongsheng
    Li, Yandong
    Mu, Haoyuan
    Liu, Chengjun
    Jiang, Maofa
    METALLURGICAL RESEARCH & TECHNOLOGY, 2017, 114 (03)
  • [30] Transformation of inclusions in Al-killed steels with different calcium contents during the heat treatment
    Wang, Weijian
    Zhang, Lifeng
    Luo, Yan
    Ren, Ying
    Sun, Xiaohui
    IRONMAKING & STEELMAKING, 2022, 49 (05) : 472 - 483