Study on the mechanical properties and fatigue failure mechanism of 7075-T6 aluminum alloy joints under different joining processes

被引:4
|
作者
Zhang, Yue [1 ,2 ]
Zhu, Linwei [2 ]
Peng, Ruitao [1 ,2 ]
Xu, Honghe [2 ]
Lu, Yan [2 ]
机构
[1] Xiangtan Univ, Postdoctoral Stn Mech, Xiangtan 411105, Hunan, Peoples R China
[2] Xiangtan Univ, Sch Mech Engn, Xiangtan, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
AA7075-T6; clinching; self-piercing riveting; resistance spot welding; fatigue; fretting wear; PIERCING RIVETED JOINTS; BEHAVIOR; MICROSTRUCTURE; TITANIUM; STRENGTH; TENSILE;
D O I
10.1177/09544089221136447
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
To obtain the theoretical basis and reference basis for the selection of low ductility aluminum alloy joining methods, three kinds of joints were obtained using 7075-T6 aluminum alloy sheets for clinching, self-piercing riveting (SPR), and resistance spot welding (RSW) joints, and the single-lap shear tests were performed on the three kinds of joints, and fatigue tests were conducted on the clinched joints and SPR joints. The fatigue fracture of the SPR joint was analyzed using scanning electron microscopy (SEM) and X-ray energy-dispersive spectroscopy (EDS). The results showed that the SPR joint demonstrated the best static performance, followed by the clinched joint and the RSW joint. In the case of the fatigue test, the SPR joint showed better fatigue performance than that of the clinched joint. The fatigue failure of the SPR joint and clinched joint is associated with fretting wear. Fretting wear of the SPR joint is more severe than that of the clinched joint. The debris produced by fretting led to microcracking phenomena in the plate. Under the action of alternating load, the microcracks continued to expand and generate macrocracks, and the joint was broken and finally failed. This fretting wear is the root cause of the failure of the SPR joint. Thus, the SPR joints exhibited the best mechanical properties.
引用
收藏
页码:2466 / 2474
页数:9
相关论文
共 50 条
  • [21] Fatigue Fracture Mechanism of Extruded Al Alloy 7075-T6 in High Humidity
    Kariya, K.
    Kawagoishi, N.
    Maeda, H.
    Chen, Q.
    Goto, M.
    Nu, Y.
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS X, 2012, 488-489 : 45 - +
  • [22] Study of mechanical joint strength of aluminum alloy 7075-T6 and dual phase steel 980 welded by friction bit joining and weld-bonding under corrosion medium
    Lim, Yong Chae
    Squires, Lile
    Pan, Tsung-Yu
    Miles, Michael
    Song, Guang-Ling
    Wang, Yanli
    Feng, Zhili
    MATERIALS & DESIGN, 2015, 69 : 37 - 43
  • [23] Ductile Fracture and S-N Curve Simulation of a 7075-T6 Aluminum Alloy under Static and Constant Low-Cycle Fatigue
    Abdellah, Mohammed Y.
    JOURNAL OF FAILURE ANALYSIS AND PREVENTION, 2021, 21 (04) : 1476 - 1488
  • [24] Investigation into Corrosion Pit-to-Fatigue Crack Transition in 7075-T6 Aluminum Alloy
    Sabelkin, V.
    Mall, S.
    Misak, H.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (06) : 2535 - 2541
  • [25] Effect of split sleeve cold expansion on microstructure and fatigue performance of 7075-T6 aluminum alloy holes
    Wang, Chenguang
    Zou, Fan
    Zhou, Entao
    Fan, Zhilei
    Ge, Ende
    An, Qinglong
    Ming, Weiwei
    Chen, Ming
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 167
  • [26] Artificial neural networks application for modeling of friction stir welding effects on mechanical properties of 7075-T6 aluminum alloy
    Maleki, E.
    4TH GLOBAL CONFERENCE ON MATERIALS SCIENCE AND ENGINEERING (CMSE 2015), 2015, 103
  • [27] Mechanical properties and deformation dependent microstructural aspects of laser shock peened 7075-T6 aluminum alloy without coating
    Dhakal, Binod
    Swaroop, S.
    MATERIALS CHARACTERIZATION, 2022, 183
  • [28] Experimental Investigation of Annealing Parameters Effects on Microstructure and Mechanical Properties of 7075-T6 Alloy
    Demirel, Mehmet Yasin
    Karaagac, Ibrahim
    JOURNAL OF POLYTECHNIC-POLITEKNIK DERGISI, 2020, 23 (02): : 283 - 289
  • [29] Crack growth behavior of Al alloy 7075-T6 under ultrasonic fatigue
    Faculty of Engineering, Kagoshima University, 1-21-40 Korimoto, Kagoshima-shi, Kagoshima, 890-0065, Japan
    Nihon Kikai Gakkai Ronbunshu A, 2006, 9 (1356-1363): : 1356 - 1363
  • [30] Zr-based metallic glass thin film coating for fatigue-properties improvement of 7075-T6 aluminum alloy
    Chang, Y. Z.
    Tsai, P. H.
    Li, J. B.
    Lin, H. C.
    Jang, J. S. C.
    Li, C.
    Chen, G. J.
    Chen, Y. C.
    Chu, J. P.
    Liaw, P. K.
    THIN SOLID FILMS, 2013, 544 : 331 - 334