Nickel-aluminum bronze (NAB) alloy design under two-steps casting and submerged friction stir processing

被引:6
|
作者
Zangene, Danial [1 ]
Kayvandarian, Fuad [1 ]
Khodabakhshi, Farzad [1 ]
Malekan, Mehdi [1 ]
Hajovska, Zuzana [2 ]
机构
[1] Univ Tehran, Univ Coll Engn, Sch Met & Mat Engn, POB 11155-4563, Tehran, Iran
[2] Slovak Acad Sci, Inst Mat & Machine Mech, Dubravska Cesta 9-6319, Bratislava 84513, Slovakia
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 890卷
关键词
Nickel -aluminum bronze (NAB); Alloy design; Casting; Submerged friction -stir processing (FSP); Microstructure; Mechanical property; MECHANICAL-PROPERTIES; MICROSTRUCTURAL MODIFICATION; CORROSION BEHAVIOR; GRAIN-REFINEMENT; HOT DEFORMATION; NIAL BRONZE; MG ALLOY; PARAMETERS;
D O I
10.1016/j.msea.2023.145960
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This research aimed to investigate the impact of friction stir processing (FSP) as a modifying technique on the microstructure and mechanical properties of Cu-10Al, Cu-10Al-5Ni, and Cu-10Al-5Ni-5Fe nickel-aluminum bronze (NAB) alloys under two different conditions of ambient and underwater submerged conditions con-cerning the as-cast state of these materials. Adding nickel as an alloying element to the Cu-10Al composition resulted in the formation of NiAl intermetallic compound and a 3 % increase in the volume percentage of sec-ondary phases. Furthermore, incorporating iron into the Cu-10Al-5Ni composition prevented the formation of detrimental gamma 2 phase and instead created kappa intermetallic compounds within the structure, leading to an overall increase of approximately 14 % in the volume percentage of secondary phases compared to the Cu-10Al composition. The initial coarse, rough, and heterogeneous structure of the cast samples was transformed into a fine, equiaxed, and homogeneous structure through the friction stirring modification conducted in both air and underwater environments for all alloy compositions, primarily due to action of dynamic recrystallization (DRX). Notably, a finer structure was achieved when the FSP was performed underwater in the submerged state. Regarding developments in mechanical properties, FSP treatment performed in air demonstrated an average enhancement of 15 % in strength and hardness across all three compounds. In contrast, the flexibility of Cu-10Al, Cu-10Al-5Ni, and Cu-10Al-5Ni-5Fe alloys in terms of elongation to failure was reduced by 70 %, 80 %, and 20 %, respectively, in comparison to the cast samples. Conversely, the underwater submerged FSP led to a notable increase of 55 % in both strength and hardness for all three compounds. However, the ductility of the alloys was reduced by 80 % compared to the cast states.
引用
收藏
页数:15
相关论文
共 21 条
  • [1] Microstructural and Mechanical Properties of Friction Stir Welded Nickel-Aluminum Bronze (NAB) Alloy
    Kucukomeroglu, T.
    Senturk, E.
    Kara, L.
    Ipekoglu, G.
    Cam, G.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (01) : 320 - 326
  • [2] Corrosion properties of submerged friction stir modified as-cast nickel-aluminum bronze (NAB) compositions
    Kayvandarian, Fuad
    Zanganeh, Danial
    Khodabakhshi, Farzad
    Malekan, Mehdi
    ELECTROCHIMICA ACTA, 2024, 501
  • [3] Microstructural and Mechanical Properties of Friction Stir Welded Nickel-Aluminum Bronze (NAB) Alloy
    T. Küçükömeroğlu
    E. Şentürk
    L. Kara
    G. İpekoğlu
    G. Çam
    Journal of Materials Engineering and Performance, 2016, 25 : 320 - 326
  • [4] Effect of friction stir processing on erosion-corrosion behavior of nickel-aluminum bronze
    Lotfollahi, M.
    Shamanian, M.
    Saatchi, A.
    MATERIALS & DESIGN, 2014, 62 : 282 - 287
  • [5] Effect of seawater salinity on the fretting corrosion behavior of nickel-aluminum bronze (NAB) alloy
    Deng, Qing
    Zhang, Po
    Li, Xiaozhi
    Shen, Ziyao
    Mi, Xue
    Cai, Zhaobing
    Gu, Le
    TRIBOLOGY INTERNATIONAL, 2024, 193
  • [6] The grain refinement mechanisms of various phases in shot-peened Nickel-Aluminum bronze (NAB) alloy
    Zhao, Bingjie
    Lv, Yuting
    Ding, Yang
    Wang, Liqiang
    Lu, Weijie
    MATERIALS CHARACTERIZATION, 2018, 144 : 77 - 85
  • [7] Micro/Nano-Scale Selective Phase/Area Corrosion Behavior of Nickel Aluminum Bronze (NAB)/Zn Composite Prepared by Friction Stir Processing
    Liu, Yaojie
    Jiang, Di
    Wei, Guijiang
    Cao, Lianmin
    Liu, Wentao
    Lv, Yuting
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2023, 54 (09): : 3425 - 3430
  • [8] Ductility Improvement of an AZ61 Magnesium Alloy through Two-Pass Submerged Friction Stir Processing
    Luo, Xicai
    Cao, Genghua
    Zhang, Wen
    Qiu, Cheng
    Zhang, Datong
    MATERIALS, 2017, 10 (03):
  • [9] Corrosion performance of friction surfaced nickel aluminium bronze (NAB) alloy under erosion corrosion and salt fog environment
    Rajakumar, S.
    Balasubramanian, V.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2018, 53 : 21 - 26
  • [10] Effect of the length of the tool pin on the hardening of 2024 aluminum alloy under friction stir processing
    Valeeva, A. Kh
    Akhunova, A. Kh
    Kabirova, D. B.
    Imayev, M. F.
    Fazlyakhmetov, R. F.
    LETTERS ON MATERIALS, 2021, 11 (02): : 119 - 124