Effect of Modified Nanographene Oxide on the Mechanical and Swelling Properties of Silicone Rubber Nanocomposites

被引:22
作者
Aravinth, V. [1 ]
Gurumoorthi, G. [1 ]
Vishvanathperumal, S. [2 ]
Navaneethakrishnan, V. [1 ]
机构
[1] EGS Pillay Engn Coll, Dept Mech Engn, Nagappattinam 611002, Tamilnadu, India
[2] SA Engn Coll, Dept Mech Engn, Chennai 600077, Tamilnadu, India
关键词
silicone rubber; nanographite oxide; 4; 4'-diphenylmethane diisocyanate; mechanical properties; swelling resistance; BUTADIENE RUBBER; GRAPHENE OXIDE; DYNAMIC PROPERTIES; GRAPHITE; CARBON; COMPRESSION; RESISTANCE; BEHAVIOR; SILANE;
D O I
10.7317/pk.2023.47.3.288
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Nanocomposites were created by using nanographene oxide (GO) as a reinforcing filler into silicone rubber and evaluating the materials' mechanical and abrasion resistance properties. GO was treated with 4,4'-diphenylmethane diisocyanate (MDI), then mixed with phenyl silicone rubber (PSR) at different concentrations (2-10 phr) and vulcanised. It was investigated the impact of MDI modified GO concentration on the morphology of PSR nanocomposites. The swell-ing properties of silicone rubber/MDI modified GO nanocomposites were also investigated in relation to penetrants (aro-matic, aliphatic, and chlorinated solvents) and nanofiller concentrations (0-10 phr). Due to greater dispersion and reinforcing impact, mechanical parameters (tensile strength and modulus), and swelling resistance of silicone nano -composites improve with MDI-GO concentration. The rate of rise is constant up to a concentration of 6 phr MDI-GO, after which it drops, confirming the formation of agglomeration. The MDI modification of GO improves the dispersion of MDI-GO in silicone rubber considerably, according to FESEM analysis. Because of its strong contact with the polymer matrix, GO serves as reinforcement. This research expands the range of applications for GO in the silicone rubber sector.
引用
收藏
页码:288 / 302
页数:15
相关论文
共 66 条
  • [1] Honeycomb Carbon: A Review of Graphene
    Allen, Matthew J.
    Tung, Vincent C.
    Kaner, Richard B.
    [J]. CHEMICAL REVIEWS, 2010, 110 (01) : 132 - 145
  • [2] Covalent modification of graphene oxide by 4,4′-methylenebis(phenyl isocyanate) to enhance corrosion resistance of polystyrene coating
    An, Kai
    Peng, Sunjuan
    Yang, Chuanning
    Qing, Yongquan
    Hu, Chuanbo
    Wang, Linshan
    Liu, Changsheng
    [J]. COLLOID AND POLYMER SCIENCE, 2019, 297 (06) : 839 - 848
  • [3] Properties of SBR/NR Blend: The Effects of Carbon Black/Silica (CB/SiO2) Hybrid Filler and Silane Coupling Agent
    Anand, G.
    Vishvanathperumal, S.
    [J]. SILICON, 2022, 14 (14) : 9051 - 9060
  • [4] [Anonymous], 1985, DEGRADATION MECH ACC
  • [5] Control of the cell structure of microcellular silicone rubber/nanographite foam for enhanced mechanical performance
    Bai, Jianwei
    Liao, Xia
    Huang, Erbo
    Luo, Yong
    Yang, Qi
    Li, Guangxian
    [J]. MATERIALS & DESIGN, 2017, 133 : 288 - 298
  • [6] Preparation and characterization of vulcanized silicone rubber/halloysite nanotube nanocomposites: Effect of matrix hardness and HNT content
    Berahman, Reyhaneh
    Raiati, Maryam
    Mazidi, Majid Mehrabi
    Paran, Seyed Mohamad Reza
    [J]. MATERIALS & DESIGN, 2016, 104 : 333 - 345
  • [7] On the cyclic deformation behavior, fracture properties and cytotoxicity of silicone-based elastomers for biomedical applications
    Bernardi, L.
    Hopf, R.
    Sibilio, D.
    Ferrari, A.
    Ehret, A. E.
    Mazza, E.
    [J]. POLYMER TESTING, 2017, 60 : 117 - 123
  • [8] Bin Othman A, 2001, POLYM TEST, V20, P159
  • [9] Blow C.M., 1981, Rubber Technology and Manufacture, V2
  • [10] Microhardness profiles on aged rubber compounds
    Brown, RP
    Soulagnet, G
    [J]. POLYMER TESTING, 2001, 20 (03) : 295 - 303