Metal powder as feedstock for laser-based additive manufacturing: From production to powder modification

被引:16
作者
Mathias, Laura E. T. [1 ]
Pinotti, Vitor E. [1 ]
Batistao, Bruna F. [1 ]
Rojas-Arias, Nicolas [1 ]
Figueira, Gustavo [1 ]
Andreoli, Angelo F. [2 ]
Gargarella, Piter [1 ,2 ,3 ]
机构
[1] Univ Fed Sao Carlos, Grad Program Mat Sci & Engn, Rodovia Washington Luis,km 235 SP 310, BR-13565905 Sao Carlos, SP, Brazil
[2] Univ Fed Sao Carlos, Dept Mat Engn, Rodovia Washington Luis,km 235 SP 310, BR-13565905 Sao Carlos, SP, Brazil
[3] Univ Fed Sao Carlos, Ctr Characterizat & Dev Mat, Rodovia Washington Luis,km 235 SP 310, BR-13565905 Sao Carlos, SP, Brazil
基金
巴西圣保罗研究基金会;
关键词
Metal powder; Gas atomization; Powder characterization; Additive manufacturing; Laser powder bed fusion; Direct laser deposition; STAINLESS-STEEL; GAS ATOMIZATION; PARTICLE-SIZE; MECHANICAL-PROPERTIES; ALUMINUM-ALLOY; ALSI10MG ALLOY; MATRIX COMPOSITES; NANOCOMPOSITES; BEHAVIOR; DEPOSITION;
D O I
10.1557/s43578-023-01271-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Laser powder bed fusion (L-PBF) and direct laser deposition (DLD) are the two main processes currently used in the additive manufacturing (AM) of metals. For both methods, metal powders are used as feedstock, and they must present specific physical and chemical properties to ensure optimal processing and reliable and reproducible printing results. Particle morphology, size distribution, and flowability, among other factors, depend on the powder production process and directly influence the processing parameters and physical characteristics of the parts built by AM. This systematic review presents different concepts involving L-PBF and DLD manufacturing and the application of metal powders. The methods used to produce and characterize metal powders and the modification techniques to improve their processability by AM are detailed and discussed. Environmental and health risks are also presented, and safety measures that must be considered while handling metal powders. Some key topics requiring attention for further development are highlighted.
引用
收藏
页码:165 / 175
页数:11
相关论文
共 147 条
[91]  
Neikov OlegD., 2009, Handbook of non-ferrous metal powders: technologies and applications
[92]  
Nozar M., 2019, DAAAM Proceedings, V1, P0654, DOI DOI 10.2507/30TH.DAAAM.PROCEEDINGS.090
[93]   Jamming probability of granular flow in 3D hopper with shallow columns: DEM simulations [J].
Park, Su-San ;
Kim, Eung Soo .
GRANULAR MATTER, 2020, 22 (04)
[94]   Effects of atomizing media and post processing on mechanical properties of 17-4 PH stainless steel manufactured via selective laser melting [J].
Pasebani, Somayeh ;
Ghayoor, Milad ;
Badwe, Sunil ;
Irrinki, Harish ;
Atre, Sundar, V .
ADDITIVE MANUFACTURING, 2018, 22 :127-137
[95]  
Mendonça CD, 2018, MATER RES-IBERO-AM J, V21, DOI [10.1590/1980-5373-MR-2017-0717, 10.1590/1980-5373-mr-2017-0717]
[96]   Direct additive laser manufacturing using gas- and water-atomised H13 tool steel powders [J].
Pinkerton, AJ ;
Li, L .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2005, 25 (5-6) :471-479
[97]  
Popovich A., 2016, METAL POWDER ADDITIV, P227, DOI [10.1007/s11837-015-1321-z, DOI 10.1007/S11837-015-1321-Z]
[98]   Selective laser melting of Al7050 powder: Melting mode transition and comparison of the characteristics between the keyhole and conduction mode [J].
Qi, Ting ;
Zhu, Haihong ;
Zhang, Hu ;
Yin, Jie ;
Ke, Linda ;
Zeng, Xiaoyan .
MATERIALS & DESIGN, 2017, 135 :257-266
[99]   Laser alloyed Al-W coatings on aluminum for enhanced corrosion resistance [J].
Rajamure, Ravi Shanker ;
Vora, Hitesh D. ;
Srinivasan, S. G. ;
Dahotre, Narendra B. .
APPLIED SURFACE SCIENCE, 2015, 328 :205-214
[100]   Microstructural control of an Al-W aluminum matrix composite during direct laser metal deposition [J].
Ramakrishnan, A. ;
Dinda, G. P. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 813